mp-1001 BaN2 monoclinic C2/c -0.768 0 6 115.3 4.761
mp-1203253 S7N orthorhombic Pnma -0.393 0 32 973.7 1.627
mp-743 RbN3 tetragonal I4/mcm -0.430 0 8 160.7 2.634
mp-22003 NaN3 trigonal R3m -0.391 0 4 60.0 1.798
mp-2599 NdN cubic Fm3m -1.544 0 2 34.5 7.627
mp-1865 UN cubic Fm3m -1.502 0 2 28.9 14.470
mp-8282 Ti2N tetragonal P42/mnm -1.446 0 6 74.7 4.882
mp-749 SmN cubic Fm3m -1.669 0 2 32.7 8.356
mp-804 GaN hexagonal P63mc -0.668 0 4 46.9 5.924
mp-2114 YN cubic Fm3m -1.879 0 2 29.8 5.743
mp-1017987 Tc3N hexagonal P6m2 -0.214 0 4 48.9 10.457
mp-567290 LaN hexagonal P63mc -1.513 0 4 88.2 5.760
mp-866056 AcN hexagonal P63mc -1.274 0 4 101.1 7.918
mp-1008833 NpN2 cubic Fm3m -1.209 0 3 35.6 12.348
mp-32742 U16N25 trigonal R3 -1.636 0 41 605.0 11.413
mp-1183691 CrN hexagonal P6m2 -0.703 0 2 16.2 6.763
mp-2596 NpN cubic Fm3m -1.306 0 2 28.9 14.447
mp-504769 N2O5 hexagonal P63/mmc -0.729 0 14 178.4 2.011
mp-2131 SrN6 orthorhombic Fddd -0.518 0 14 218.0 2.616
mp-22205 InN hexagonal P63mc -0.090 0 4 64.4 6.642
mp-510557 CsN3 tetragonal I4/mcm -0.435 0 8 182.8 3.178
mp-672289 Ge3N4 trigonal P31c -0.263 0 28 355.5 5.118
mp-8780 Cr2N trigonal P31m -0.514 0 9 87.4 6.724
mp-1009657 CaN2 tetragonal I4/mmm -0.760 0 3 39.2 2.888
mp-1018027 VN hexagonal P6m2 -1.354 0 2 17.3 6.239
mp-567907 P3N5 monoclinic C2/c -0.538 0 16 200.9 2.694
mp-1279 TaN hexagonal P62m -1.364 0 6 69.4 13.996
mp-1019319 TcN cubic Pm3m -0.184 0 6 66.6 8.372
mp-29973 SrN monoclinic C2/m -0.716 0 8 175.1 3.855
mp-1221446 N2O cubic P213 -0.449 0 12 216.6 1.349
mp-1019052 ReN cubic Pm3m -0.146 0 6 67.6 14.757
mp-1975 TmN cubic Fm3m -2.014 0 2 27.9 10.903
mp-974435 Re3N hexagonal P6m2 -0.128 0 4 50.2 18.950
mp-2634 NbN hexagonal P6m2 -1.260 0 2 22.2 7.984
mp-1892 Ba2N trigonal R3m -0.533 0 3 108.8 4.404
mp-2033 Ni3N hexagonal P6322 -0.066 0 8 78.7 8.019
mp-1102 LuN cubic Fm3m -2.070 0 2 26.9 11.663
mp-1014265 Zr2N tetragonal P42/mnm -1.343 0 6 98.2 6.645
mp-2828 HfN cubic Fm3m -1.939 0 2 23.4 13.684
mp-1216242 W2N3 monoclinic Cm -0.661 0 10 111.5 12.205
mp-1079585 Nb2N trigonal P31m -1.004 0 9 124.1 8.023
mp-343 PrN cubic Fm3m -1.473 0 2 35.6 7.230
mp-1776 UN2 cubic Fm3m -1.612 0 3 36.8 12.016
mp-7234 Nb5N6 hexagonal P63/mcm -1.220 0 22 251.0 7.257
mp-16031 Sn3N4 cubic Fd3m -0.007 0 14 191.0 7.165
mp-1019316 Tc2N hexagonal P63/mmc -0.234 0 6 68.5 10.180
mp-1224388 Hf3N2 trigonal R3m -1.624 0 5 69.9 13.387
mp-492 TiN cubic Fm3m -1.908 0 2 19.2 5.340
mp-2493 CeN cubic Fm3m -1.690 0 2 32.2 7.942
mp-277 Zr3N4 orthorhombic Pnma -1.693 0 28 356.5 6.143
mp-1707 BaN6 monoclinic P21/m -0.514 0 14 237.8 3.092
mp-2686 Ca2N trigonal R3m -0.888 0 3 72.3 2.162
mp-10564 SrN2 tetragonal I4/mmm -0.749 0 3 47.0 4.090
mp-1410 DyN cubic Fm3m -1.890 0 2 29.6 9.888
mp-2659 LiN3 monoclinic C2/m -0.419 0 4 45.4 1.790
mp-1188283 V8N tetragonal P42/mnm -0.374 0 18 226.2 6.189
mp-10736 Ba3N hexagonal P63/mcm -0.407 0 8 368.0 3.844
mp-2811 MoN hexagonal P63mc -0.559 0 16 163.8 8.914
mp-1188721 IN4 orthorhombic Pna21 -0.206 0 20 511.4 2.376
mp-1079438 Ta2N trigonal P31m -1.044 0 9 121.7 15.393
mp-1018160 PmN cubic Fm3m -1.623 0 2 33.4 7.894
mp-776470 Hf3N4 orthorhombic Pnma -1.883 0 28 341.2 11.514
mp-2251 Li3N hexagonal P6/mmm -0.463 0 4 44.9 1.289
mp-33090 V2N trigonal P31m -1.099 0 9 94.7 6.096
mp-1009130 MnN cubic F43m -0.490 0 2 19.3 5.922
mp-448 CoN cubic F43m -0.085 0 2 19.3 6.282
mp-2789 NO2 cubic Im3 -0.824 0 18 275.8 1.662
mp-834 ThN cubic Fm3m -1.764 0 2 34.7 11.786
mp-27488 Ta3N5 orthorhombic Cmcm -1.286 0 16 208.8 9.746
mp-2117 TbN cubic Fm3m -1.847 0 2 30.3 9.486
mp-530081 Mo15N16 monoclinic Cc -0.551 0 62 644.9 8.565
mp-2857 ScN cubic Fm3m -2.104 0 2 23.1 4.246
mp-1352 ZrN cubic Fm3m -1.870 0 2 24.6 7.099
mp-9981 Mn2N orthorhombic Pbcn -0.412 0 12 117.8 6.988
mp-1009545 PaN cubic Fm3m -1.821 0 2 30.4 13.374
mp-1804 Fe3N hexagonal P6322 -0.165 0 8 81.2 7.421
mp-19830 ErN cubic Fm3m -1.969 0 2 28.5 10.566
mp-1719 PuN cubic Fm3m -1.478 0 2 30.2 14.203
mp-864757 YbN2 tetragonal P42/mnm -0.899 0 6 80.2 8.325
mp-1559 Mg3N2 cubic Ia3 -0.907 0 40 503.7 2.662
mp-1245 Sr2N trigonal R3m -0.674 0 3 90.0 3.493
mp-864647 Hf2N tetragonal P42/mnm -1.371 0 6 93.1 13.237
mp-984 BN hexagonal P63/mmc -1.473 0 4 42.1 1.956
mp-940 GdN cubic Fm3m -1.770 0 2 31.0 9.165
mp-1180208 NF2 triclinic P1 -0.318 0 12 217.9 1.585
mp-6988 FeN cubic F43m -0.321 0 2 18.9 6.127
mp-1642 Ta5N6 hexagonal P63/mcm -1.339 0 22 246.7 13.312
mp-844 Ca3N2 cubic Ia3 -0.946 0 40 755.6 2.606
mp-988 Si3N4 hexagonal P63/m -1.314 0 14 148.6 3.134
mp-676 CaN6 orthorhombic Fddd -0.483 0 14 192.3 2.144
mp-22631 Co2N orthorhombic Pnnm -0.061 0 6 55.3 7.919
mp-32590 U4N7 tetragonal I4cm -1.659 0 44 600.3 11.621
mp-883 HoN cubic Fm3m -1.930 0 2 29.0 10.233
mp-20340 EuN cubic Fm3m -1.002 0 2 32.8 8.414
mp-540572 NCl3 orthorhombic Pnma -0.052 0 48 1463.4 1.639
mp-827 KN3 tetragonal I4/mcm -0.435 0 8 141.2 1.908
mp-505622 Mn4N cubic Pm3m -0.251 0 5 53.0 7.329
mp-864675 Yb3N2 trigonal R3c -1.101 0 10 176.4 10.301
mp-661 AlN hexagonal P63mc -1.596 0 4 42.5 3.201
mp-685209 Sc39N34 trigonal P3m1 -1.965 0 73 910.5 4.066
mp-9460 Zn3N2 cubic Ia3 -0.041 0 40 479.2 6.216
mp-29145 H3N cubic P213 -0.543 0 16 133.9 0.845
mp-1203025 Np2N3 cubic Ia3 -1.393 0 40 593.2 11.556
mp-467 Th3N4 trigonal R3m -1.828 0 7 119.5 10.448
mp-1212961 Eu2N cubic Fd3m -0.834 0 12 298.2 7.081
mp-18337 Be3N2 cubic Ia3 -1.227 0 40 270.6 2.703
mp-570538 NaN3 monoclinic C2/m -0.391 0.000 4 60.2 1.793
mp-2245 Si3N4 trigonal P31c -1.313 0.000 28 298.9 3.117
mp-7991 BN hexagonal P63/mmc -1.473 0.000 4 45.2 1.825
mp-1771 NO2 monoclinic P21/c -0.824 0.001 12 185.0 1.652
mp-13852 Ge3N4 hexagonal P63/m -0.262 0.002 14 177.6 5.123
mp-13150 BN trigonal R3m -1.471 0.002 2 20.0 2.060
mp-1066400 NaN3 trigonal R3m -0.389 0.002 4 62.0 1.741
mp-1064952 NaN3 monoclinic Cm -0.389 0.002 4 60.7 1.777
mp-555 Fe8N tetragonal I4/mmm -0.070 0.003 9 101.1 7.569
mp-629015 BN hexagonal P63/mmc -1.469 0.004 4 39.8 2.071
mp-27953 Mo2N tetragonal I41/amd -0.368 0.004 6 73.5 9.306
mp-604884 BN hexagonal P6m2 -1.469 0.004 4 38.7 2.128
mp-830 GaN cubic F43m -0.663 0.005 2 23.5 5.921
mp-22387 U2N3 cubic Ia3 -1.618 0.006 40 606.3 11.352
mp-1216851 V32N3 monoclinic P2/m -0.282 0.006 35 449.6 6.176
mp-685145 BN orthorhombic Fmm2 -1.466 0.007 2 19.1 2.155
mp-20411 InN cubic F43m -0.081 0.010 2 32.3 6.628
mp-1078389 MoN hexagonal P63/mmc -0.548 0.010 8 81.8 8.923
mp-754553 Zn3N2 orthorhombic Pnma -0.031 0.010 20 241.5 6.167
mp-2341 Li3N hexagonal P63/mmc -0.451 0.011 8 69.9 1.656
mp-973 U2N3 trigonal P3m1 -1.611 0.013 5 68.1 12.626
mp-1047 Ca3N2 trigonal R3c -0.933 0.014 10 184.6 2.667
mp-1065394 MoN hexagonal P63/mmc -0.545 0.014 4 40.7 8.967
mp-256 LaN cubic Fm3m -1.499 0.014 2 37.4 6.787
mp-581833 RbN3 tetragonal P4/mmm -0.415 0.014 4 85.7 2.471
mp-866083 Zr3N2 trigonal R3c -1.539 0.015 10 147.0 6.814
mp-7790 Ti2N tetragonal I41/amd -1.431 0.015 6 76.5 4.763
mp-755988 Hf3N4 cubic Fd3m -1.868 0.016 14 186.7 10.521
mp-1187591 Ti3N2 trigonal R3c -1.614 0.016 10 112.8 5.052
mp-643432 H3N orthorhombic P212121 -0.526 0.017 16 113.2 0.999
mp-673174 Fe8N3 monoclinic C2 -0.162 0.017 33 327.3 7.440
mp-754556 Nb3N5 orthorhombic Cmcm -0.989 0.018 16 212.3 5.455
mp-1217048 Ti8N5 tetragonal P4m2 -1.570 0.018 13 151.9 4.952
mp-1188869 Nb2N3 orthorhombic Pnma -1.055 0.019 20 205.8 7.354
mp-557865 NO2 cubic Im3 -0.805 0.020 18 324.3 1.413
mp-1700 AlN cubic F43m -1.575 0.021 2 21.3 3.193
mp-779689 H3N cubic P213 -0.521 0.022 16 152.1 0.744
mp-1205986 Co3N hexagonal P6322 -0.023 0.023 8 77.7 8.160
mp-1077354 ReN2 monoclinic C2/m -0.072 0.025 6 55.7 12.768
mp-1221525 Mo2N trigonal R3m -0.347 0.026 3 36.6 9.341
mp-1204579 NO3 monoclinic P21/c -0.611 0.027 64 1049.4 1.570
mp-999549 WN2 hexagonal P6m2 -0.524 0.027 3 29.2 12.066
mp-1077232 WN2 hexagonal P63/mmc -0.524 0.027 6 58.2 12.092
mp-1459 TaN hexagonal P6m2 -1.336 0.028 2 21.9 14.764
mp-7927 Nb4N5 tetragonal I4/m -1.164 0.029 9 104.0 7.053
mp-6977 Be3N2 hexagonal P63/mmc -1.198 0.029 10 68.6 2.665
mp-1096994 HfN hexagonal P63/mmc -1.908 0.031 4 46.8 13.648
mp-1018157 CrN cubic F43m -0.672 0.031 2 21.3 5.146
mp-8046 Ta4N5 tetragonal I4/m -1.302 0.031 9 102.2 12.900
mp-986716 Sr3N2 cubic Ia3 -0.660 0.031 40 942.4 4.100
mp-1096882 Cr3N2 trigonal R3c -0.557 0.032 10 91.9 6.648
mp-568293 Ca3N2 orthorhombic Pbcn -0.914 0.032 20 354.7 2.776
mp-23922 HN orthorhombic Pmna -0.329 0.033 32 298.4 1.337
mp-754381 Zr3N4 cubic Fd3m -1.659 0.035 14 195.4 5.604
mp-1224391 Hf4N3 trigonal R3m -1.678 0.036 7 93.5 13.430
mp-2701 NbN hexagonal P63/mmc -1.219 0.040 4 43.8 8.114
mp-870 TlN3 tetragonal I4/mcm 0.041 0.041 8 150.2 5.449
mp-32994 Hf4N3 tetragonal I4/mmm -1.672 0.041 7 93.6 13.406
mp-1206425 Co4N cubic Pm3m 0.005 0.042 5 51.7 8.025
mp-1018948 Re2N hexagonal P63/mmc -0.091 0.043 6 70.3 18.259
mp-1208406 Ta2N3 orthorhombic Pnma -1.259 0.043 20 202.7 13.234
mp-1093992 ZrN hexagonal P63/mmc -1.825 0.045 4 49.2 7.105
mp-11661 Zr3N4 cubic I43d -1.648 0.045 14 158.0 6.929
mp-973935 OsN2 hexagonal P6/mmm 0.046 0.046 3 34.3 10.568
mp-1019077 ReN2 monoclinic P21/m -0.050 0.047 6 57.6 12.350
mp-1014160 ZrN trigonal P3m1 -1.823 0.048 4 49.2 7.103
mp-2132 CrN cubic Fm3m -0.655 0.048 8 71.3 6.146
mp-568172 Ca3N2 monoclinic C2/m -0.898 0.048 15 262.9 2.809
mp-1070456 Be3N2 trigonal R3m -1.178 0.049 5 34.3 2.669
mp-754353 Zr3N4 trigonal R3m -1.642 0.051 7 88.3 6.199
mp-21476 Fe2N orthorhombic Pbcn -0.162 0.055 12 112.8 7.399
mp-248 Fe2N trigonal P31m -0.158 0.059 9 84.5 7.410
mp-1211954 IrN3 cubic Im3 0.063 0.063 16 161.9 9.610
mp-571281 Ge3N4 cubic I43d -0.200 0.063 14 162.4 5.604
mp-1096898 Cr3N2 monoclinic C2/m -0.525 0.065 15 135.9 6.747
mp-1184048 Eu2N tetragonal P42/mnm -0.767 0.067 6 143.8 7.343
mp-1094090 Ni4N cubic Pm3m 0.014 0.067 5 51.3 8.056
mp-1019080 ReN2 monoclinic Pc -0.030 0.067 6 68.1 10.453
mp-11660 Hf3N4 cubic I43d -1.814 0.069 14 151.4 12.975
mp-569167 Nb4N3 tetragonal I4/mmm -1.081 0.069 7 85.5 8.038
mp-535 Fe4N cubic Pm3m -0.062 0.070 5 49.6 7.951
mp-1221793 Mn2N trigonal P3m1 -0.341 0.070 3 30.4 6.765
mp-1009770 RuN cubic F43m 0.071 0.071 2 23.8 8.039
mp-1097011 IN2 tetragonal I4/mcm -0.099 0.073 6 149.2 3.448
mp-33046 TiN trigonal R3m -1.834 0.073 44 480.7 4.703
mp-754434 Hf3N4 trigonal R3m -1.810 0.074 7 84.7 11.601
mp-1195863 ZnN6 trigonal P3221 0.065 0.075 42 627.0 2.375
mp-971684 C3N4 orthorhombic Cmcm 0.075 0.075 28 314.6 1.944
mp-1639 BN cubic F43m -1.396 0.077 2 11.9 3.458
mp-1193580 C3N4 hexagonal P6m2 0.078 0.078 28 310.3 1.970
mp-1019239 PdN2 orthorhombic Immm 0.080 0.080 3 55.8 4.001
mp-1014345 Cr3N4 hexagonal P63/m -0.523 0.080 14 139.1 5.063
mp-1101173 WN2 tetragonal I42d -0.464 0.087 6 146.0 4.818
mp-6913 YN hexagonal P63/mmc -1.792 0.087 4 69.7 4.905