Material ID Formula Crystal System Space Group Formation Energy
(eV/atom)
E Above Hull
(eV/atom)
# Sites Volume (Å3) Density (g/cm3)
mp-1001571 CaFeO3 cubic Pm3m -2.282 0.052 5 56.5 4.232
mp-1016852 BaMnO3 cubic Pm3m -2.368 0.126 5 65.6 6.081
mp-1040469 KMoO3 cubic Pm3m -2.122 0.106 5 64.2 4.732
mp-1040471 NaMoO3 cubic Pm3m -2.096 0.095 5 61.6 4.501
mp-1040472 KWO3 cubic Pm3m -2.130 0.070 5 64.8 6.940
mp-1075901 Sr6Ca2Co5(CuO8)3 monoclinic P2 -1.826 0.154 40 462.0 5.302
mp-1075902 EuCuO3 cubic Pm3m -1.986 0.079 5 56.0 7.813
mp-1075904 EuFeO3 cubic Pm3m -2.463 0.093 5 57.7 7.356
mp-1075911 RbNbO3 cubic Pm3m -2.765 0.083 5 68.9 5.459
mp-1075921 LaNiO3 cubic Pm3m -2.370 0.035 5 57.4 7.108
mp-1075922 Sr7CaTi8O24 cubic Pm3m -3.553 0.009 40 488.4 4.829
mp-1075928 SrCa(CoO3)2 tetragonal P4/mmm -1.958 0.099 40 449.2 5.050
mp-1075930 LaSm(CoO3)2 tetragonal P4/mmm -2.551 0.094 40 434.1 7.698
mp-1075933 SmAgO3 cubic Pm3m -1.706 0.423 5 67.4 7.548
mp-1075935 BaSr7Fe7CoO24 trigonal R3m -2.269 0.032 40 485.3 5.422
mp-1075937 Rb2W2O5 orthorhombic Ima2 -1.516 0.573 18 297.7 6.902
mp-1075943 Ba3Sr5Ti8O24 tetragonal P4/mmm -3.531 0.008 40 503.9 5.329
mp-1075948 Sr7CaTi5Mn3O24 monoclinic Cm -3.153 0.020 40 480.0 4.987
mp-1075952 Na2Ta2O5 orthorhombic Ima2 -2.676 0.176 18 251.1 6.452
mp-1075953 K5Na3Ta5Nb3O24 triclinic P1 -2.987 0.014 40 519.6 5.855
mp-1075954 La5Sm3Cr7FeO24 monoclinic Cm -2.889 0.273 40 482.8 6.705
mp-1075955 Sr5Ca3Fe7CoO24 monoclinic Cm -2.271 0.026 40 466.6 4.955
mp-1075956 K2Mo2O5 orthorhombic Ima2 -1.785 0.333 18 277.8 4.186
mp-1075961 La7SmCo5(CuO8)3 monoclinic Cm -2.500 0.074 40 452.9 7.304
mp-1075962 Sr5Ca3Ti3Mn5O24 triclinic P1 -2.869 0.052 40 467.9 4.829
mp-1075966 Sr2Ca2Fe3CoO12 monoclinic Pm -2.223 0.041 40 461.0 4.855
mp-1075968 Sr3Ca5Mn4(FeO6)4 monoclinic Cm -2.371 0.069 40 461.2 4.646
mp-1075969 Sr6Ca2MnFe7O24 orthorhombic Cmm2 -2.336 0.021 40 473.4 5.036
mp-1075973 SmMnO3 cubic Pm3m -2.786 0.572 5 59.1 7.118
mp-1075974 Ba3Sr5Ti7MnO24 monoclinic Cm -3.397 0.016 40 502.0 5.372
mp-1075975 EuCoO3 cubic Pm3m -2.172 0.095 5 53.6 8.022
mp-1075976 Sr5Ca3TiMn7O24 monoclinic Cm -2.592 0.067 40 460.3 4.960
mp-1075982 BaSr7Co5(CuO8)3 monoclinic Cm -1.855 0.103 40 474.6 5.668
mp-1075984 La7SmMn3Fe5O24 monoclinic Cm -2.841 0.196 40 492.6 6.575
mp-1075987 La7SmTiV7O24 trigonal R3m -3.201 0.138 40 498.3 6.369
mp-1075988 BaSr7Ti6Mn2O24 orthorhombic Amm2 -3.226 0.071 40 490.6 5.184
mp-1075989 Ba3Sr5Co4(CuO6)4 monoclinic Cm -1.777 0.152 40 492.2 5.817
mp-1075997 Sr4Ca4FeCo7O24 monoclinic Cm -2.042 0.050 40 456.7 4.956
mp-1076000 LaAgO3 cubic Pm3m -1.897 0.238 5 69.3 7.058
mp-1076014 Ca2Mn2O5 orthorhombic Ima2 -2.582 0.069 18 230.4 3.893
mp-1076020 SrCa3Mn4O12 tetragonal P4/mmm -2.437 0.103 20 222.9 4.616
mp-1076037 Eu2Ti2O5 orthorhombic Ima2 -3.276 0.067 18 241.3 6.602
mp-1076048 Na2V2O5 orthorhombic Ima2 -2.326 0.071 18 220.3 3.436
mp-1076053 La2Cu2O5 orthorhombic Ima2 -2.491 0.093 18 240.8 6.688
mp-1076054 BaSr7Co4(CuO6)4 trigonal R3m -1.863 0.060 40 472.7 5.707
mp-1076055 Sm2V2O5 orthorhombic Ima2 -2.757 0.223 18 248.8 6.441
mp-1076058 Sr4Ca4Mn5(FeO8)3 triclinic P1 -2.395 0.067 40 461.6 4.810
mp-1076062 Sr7CaFe5(CoO8)3 monoclinic Cm -2.207 0.019 40 468.3 5.295
mp-1076063 Sm2Co2O5 orthorhombic Ima2 -2.634 0.455 18 238.1 6.955
mp-1076070 LaCuO3 cubic Pm3m -2.409 0.024 5 58.0 7.166
mp-1076074 SrCa3TiMn3O12 orthorhombic Amm2 -2.721 0.081 40 450.9 4.511
mp-1076076 La7SmCo6(CuO12)2 orthorhombic Cmm2 -2.504 0.099 40 450.6 7.324
mp-1076079 Sr5Ca3MnFe7O24 monoclinic Cm -2.331 0.027 40 469.9 4.905
mp-1076080 Sr5Ca3Mn7FeO24 monoclinic Cm -2.434 0.071 40 461.9 4.971
mp-1076088 Mg2Co2O5 orthorhombic Ima2 -2.002 0.174 18 184.3 4.441
mp-1076090 BaSr7(Fe2O5)4 triclinic P1 -2.470 0.006 144 2056.8 4.900
mp-1076092 Sr7CaMn2(Fe3O10)2 triclinic P1 -2.491 0.031 144 2008.6 4.690
mp-1076095 K5Na3Ta4Nb4O24 monoclinic Cm -2.957 0.017 40 520.9 5.559
mp-1076096 SrCa3(CoO3)4 tetragonal P4/mmm -1.953 0.108 20 220.2 4.794
mp-1076107 Sr5Ca3FeCo7O24 monoclinic Cm -2.058 0.032 40 457.1 5.125
mp-1076118 Sr6Ca2Co7CuO20 triclinic P1 -1.946 0.224 144 1908.8 4.878
mp-1076119 La2Ag2O5 orthorhombic Ima2 -2.220 0.139 18 286.8 6.641
mp-1076121 La2Ni2O5 orthorhombic Ima2 -2.528 0.091 18 246.5 6.404
mp-1076123 Eu2Co2O5 orthorhombic Ima2 -2.351 0.042 18 233.4 7.139
mp-1076128 Ca7Mg(CoO3)8 cubic Pm3m -1.905 0.144 40 430.0 4.481
mp-1076131 La7SmV8O24 cubic Pm3m -3.150 0.125 40 493.8 6.437
mp-1076132 Ca7MgCo7CuO24 trigonal R3m -1.780 0.245 40 430.9 4.489
mp-1076134 Sr3Ca5Ti3Mn5O20 triclinic P1 -2.971 0.061 144 1944.1 4.105
mp-1076137 Ba3Sr5Co2(CuO4)6 monoclinic Pm -1.748 0.097 40 486.2 5.919
mp-1076138 Sr3CaTi2Mn2O12 orthorhombic Cmm2 -2.847 0.201 40 472.6 4.923
mp-1076139 Ca7MgFeCo7O24 trigonal R3m -1.953 0.131 40 431.9 4.449
mp-1076141 Sr5Ca3Mn4(FeO5)4 triclinic P1 -2.499 0.067 144 1967.0 4.462
mp-1076147 Sr2Ca2Fe3CoO10 triclinic P1 -2.419 0.039 144 1917.7 4.446
mp-1076151 Ca2Ti2O5 orthorhombic Ima2 -3.249 0.117 18 237.5 3.578
mp-1076157 Mg2Fe2O5 orthorhombic Ima2 -2.240 0.630 18 198.3 4.025
mp-1076159 Sr7CaFe4(CoO5)4 triclinic P1 -2.320 0.035 144 1970.1 4.830
mp-1076163 Sr4Ca4Mn7FeO20 triclinic P1 -2.548 0.057 144 1940.8 4.351
mp-1076165 Sr8Fe7CoO20 triclinic P1 -1.719 0.730 144 2020.5 4.835
mp-1076170 Sr3CaTi3MnO10 triclinic P1 -3.186 0.150 144 2015.0 4.361
mp-1076171 La5Sm3Co7CuO24 monoclinic Cm -2.524 0.100 40 447.7 7.439
mp-1076172 La7SmMn4(FeO5)4 triclinic P1 -2.893 0.134 144 2087.9 5.999
mp-1076175 Sr4Ca4Co7CuO20 triclinic P1 -1.987 0.223 144 1875.9 4.627
mp-1076176 La7Sm(Fe2O5)4 triclinic P1 -2.822 0.102 144 2072.3 6.056
mp-1076177 Sr6Ca2Mn3(FeO4)5 triclinic P1 -2.496 0.048 144 1990.1 4.572
mp-1076179 La6Sm2V3Cr5O20 triclinic P1 -2.863 0.263 144 2015.8 6.152
mp-1076181 BaSr7Mn2(Fe3O10)2 triclinic P1 -2.473 0.032 144 2067.6 4.869
mp-1076182 Sr6Ca2Mn5Fe3O20 triclinic P1 -2.515 0.052 144 1985.9 4.576
mp-1076183 Sr7CaTi3Mn5O20 triclinic P1 -2.955 0.045 144 2025.4 4.564
mp-1076184 SrCa3Mn4O10 triclinic P1 -2.566 0.067 144 1895.1 4.119
mp-1076189 Ba3Sr(Cu2O5)2 triclinic P1 -1.842 0.103 144 2129.3 5.701
mp-1076190 Sr4Ca4Mn5Fe3O20 triclinic P1 -2.518 0.067 144 1948.4 4.340
mp-1076191 La3SmV3CrO10 triclinic P1 -2.887 0.268 144 2033.2 6.089
mp-1076192 Sr5Ca3TiMn7O20 triclinic P1 -2.692 0.052 144 1962.9 4.435
mp-1076194 La3SmCr2(FeO5)2 triclinic P1 -2.853 0.198 144 2086.2 6.003
mp-1076195 KNaMoWO5 triclinic P1 -1.836 0.265 144 2102.9 5.330
mp-1076196 BaSr7Ti6Mn2O20 triclinic P1 -3.177 0.142 144 2058.1 4.737
mp-1076197 Sr2Ca2Mn3FeO10 triclinic P1 -2.532 0.063 144 1940.2 4.355
mp-1076198 Sr2Ca6Fe3(CoO4)5 triclinic P1 -2.312 0.052 144 1840.8 4.322
mp-1076199 Sr5Ca3MnFe7O20 triclinic P1 -2.500 0.031 144 1966.7 4.472
mp-1076202 Sr7CaTi5Mn3O20 triclinic P1 -3.150 0.085 144 2039.1 4.487
mp-1076203 La5Sm3Cr6(FeO10)2 triclinic P1 -2.843 0.249 144 2029.8 6.182
mp-1076204 La7SmCr2(Fe3O10)2 triclinic P1 -2.841 0.148 144 2077.6 6.016
mp-1076205 K4Na4Mo3(WO4)5 triclinic P1 -1.835 0.264 144 2121.8 5.558
mp-1076206 K2Na2NbW3O10 triclinic P1 -2.012 0.263 144 2117.9 5.824
mp-1076207 Ca7MgTiMn7O20 triclinic P1 -2.678 0.087 144 1826.4 3.845
mp-1076208 K5Na3Nb4(WO5)4 triclinic P1 -2.221 0.245 144 2136.8 5.258
mp-1076213 SrCaMn2O6 tetragonal P4/mmm -2.431 0.101 40 456.9 4.849
mp-1076214 Ca7MgMn7FeO24 trigonal R3m -2.344 0.165 40 441.7 4.245
mp-1076215 K2Nb2O5 orthorhombic Ima2 -2.502 0.152 18 276.8 4.127
mp-1076217 Sr3Ca5TiMn7O24 monoclinic Cm -2.584 0.083 40 454.3 4.678
mp-1076218 La3SmV2Cr2O12 orthorhombic Pmm2 -3.093 0.144 20 243.0 6.594
mp-1076219 La4Sm4Co7CuO24 monoclinic Cm -2.494 0.125 40 448.4 7.470
mp-1076222 KNa7V7MoO24 trigonal R3m -2.236 0.136 40 441.0 3.903
mp-1076223 Eu2Ni2O5 orthorhombic Ima2 -1.826 0.401 18 230.2 7.232
mp-1076224 KNa(WO3)2 tetragonal P4/mmm -2.095 0.088 10 127.8 6.833
mp-1076247 Ba6Sr2CoCu7O24 orthorhombic Amm2 -1.709 0.092 40 508.4 6.163
mp-1076249 La5Sm3Ni7AgO24 monoclinic Cm -2.248 0.119 40 462.5 7.354
mp-1076253 La6Sm2V5Cr3O24 monoclinic Pm -3.112 0.132 40 492.4 6.505
mp-1076260 Sr5Ca3Fe2(CoO4)6 monoclinic Pm -1.896 0.228 40 458.7 5.096
mp-1076261 Na2W2O5 orthorhombic Ima2 -1.788 0.275 18 248.2 6.606
mp-1076264 Ba2Sr6Co3Cu5O24 monoclinic P2 -1.777 0.108 40 484.8 5.750
mp-1076268 Sr2Ca6Mn5(FeO8)3 orthorhombic Amm2 -2.387 0.080 40 456.1 4.522
mp-1076273 Sr2Ca2Co3CuO10 triclinic P1 -1.984 0.203 144 1854.4 4.698
mp-1076275 La7SmCo6(AgO12)2 orthorhombic Cmm2 -2.376 0.153 40 478.1 7.210
mp-1076286 Eu2Cr2O5 orthorhombic Ima2 -1.272 1.441 18 242.7 6.676
mp-1076287 La6Sm2Co7AgO24 orthorhombic Amm2 -2.454 0.137 40 451.8 7.493
mp-1076289 Sm2Mn2O5 orthorhombic Ima2 -2.886 0.376 18 255.6 6.375
mp-1076296 Ba6Sr2CoCu7O20 triclinic P1 -1.863 0.129 144 2112.8 5.731
mp-1076317 MgCuO3 cubic Pm3m -1.171 0.497 5 51.9 4.343
mp-1076319 Ca2Fe2O5 orthorhombic Ima2 -2.524 0.510 18 231.9 3.893
mp-1076323 Rb2Nb2O5 orthorhombic Ima2 -2.447 0.191 18 293.1 4.949
mp-1076325 LaSm(NiO3)2 tetragonal P4/mmm -2.309 0.088 40 448.0 7.453
mp-1076335 K5Na3Nb8O24 tetragonal P4/mmm -2.838 0.024 40 527.5 4.381
mp-1076337 Ba2Sr6Ti7MnO24 orthorhombic Cmm2 -3.406 0.015 40 495.4 5.277
mp-1076338 La3SmV3CrO12 orthorhombic Pma2 -3.016 0.234 40 490.5 6.527
mp-1076342 Ba7SrCoCu7O24 trigonal R3m -1.688 0.110 40 510.4 6.300
mp-1076351 KNa7V6(MoO12)2 orthorhombic Amm2 -2.220 0.129 40 450.1 3.990
mp-1076354 Rb2V2O5 orthorhombic Ima2 -2.148 0.235 18 297.9 3.933
mp-1076359 Sr4Ca4Mn7FeO24 monoclinic Cm -2.428 0.081 40 458.1 4.840
mp-1076360 RbCrO3 cubic Pm3m -1.570 0.508 5 61.5 5.009
mp-1076363 K5Na3TaNb7O24 monoclinic Cm -2.868 0.022 40 527.0 4.663
mp-1076368 MgFeO3 cubic Pm3m -1.727 0.463 5 53.4 3.984
mp-1076372 Sr7CaFe6(CoO12)2 orthorhombic Amm2 -2.236 0.024 40 473.5 5.227
mp-1076377 BaSr7Ti7MnO24 trigonal R3m -3.418 0.010 40 491.6 5.150
mp-1076382 La7Sm(FeO3)8 cubic Pm3m -2.808 0.144 40 493.5 6.573
mp-1076384 SrCaTiMnO6 monoclinic Cm -2.866 0.189 40 465.6 4.657
mp-1076391 K2W2O5 orthorhombic Ima2 -1.586 0.515 18 282.1 6.190
mp-1076393 Sm2Cu2O5 orthorhombic Ima2 -2.439 0.134 18 229.0 7.363
mp-1076399 Sr6Ca2Fe7CoO24 orthorhombic Cmm2 -2.277 0.019 40 469.4 5.093
mp-1076401 Rb2Cr2O5 orthorhombic Ima2 -1.686 0.425 18 310.1 3.801
mp-1076408 BaSr7Mn2(FeO4)6 orthorhombic Amm2 -2.350 0.021 40 484.6 5.413
mp-1076409 Sr8MnFe7O20 monoclinic Cm -2.486 0.012 144 2036.7 4.784
mp-1076410 Sr2Ca2Mn(FeO4)3 monoclinic Pm -2.338 0.047 40 464.6 4.788
mp-1076412 K5Na3Nb6(WO12)2 orthorhombic Amm2 -2.665 0.031 40 524.7 4.980
mp-1076413 K5Na3Ta7NbO24 monoclinic Cm -3.047 0.009 40 516.6 6.454
mp-1076418 La7SmMn2(Fe3O10)2 triclinic P1 -2.859 0.117 144 2084.8 6.014
mp-1076424 Sr3Ca(FeO3)4 tetragonal P4/mmm -2.315 0.015 20 236.3 5.048
mp-1076428 Sr5Ca3Fe4(CoO5)4 triclinic P1 -2.332 0.045 144 1922.2 4.621
mp-1076429 Ba2Sr6Co5(CuO8)3 monoclinic P2 -1.791 0.175 40 484.4 5.724
mp-1076431 La7SmCr2(FeO4)6 orthorhombic Cmm2 -2.894 0.121 40 489.3 6.603
mp-1076438 La2Co2O5 orthorhombic Ima2 -2.692 0.286 18 251.5 6.281
mp-1076439 Ba2Co2O5 orthorhombic Ima2 -2.097 0.318 18 280.6 5.592
mp-1076444 Sr2Ca2MnFe3O10 triclinic P1 -2.502 0.051 144 1942.7 4.362
mp-1076445 Sr8MnFe7O24 cubic Pm3m -2.348 0.002 40 478.8 5.309
mp-1076449 SrCa7Mn7FeO20 triclinic P1 -2.558 0.075 144 1866.6 4.016
mp-1076450 Sr3Ca5Mn4(FeO5)4 triclinic P1 -2.501 0.083 144 1920.8 4.241
mp-1076454 Sr2Ti2O5 orthorhombic Ima2 -3.261 0.079 18 254.0 4.588
mp-1076455 La7SmMn3(FeO4)5 triclinic P1 -2.875 0.126 144 2079.4 6.027
mp-1076457 Sr6Ca2Fe5(CoO8)3 monoclinic P2 -2.202 0.025 40 465.8 5.154
mp-1076459 La7SmCrFe7O20 triclinic P1 -2.830 0.126 144 2073.6 6.040
mp-977412 EuNiO3 cubic Pm3m -1.936 0.071 5 54.5 7.874
mp-1076463 Sm2Fe2O5 orthorhombic Ima2 -2.804 0.115 18 246.6 6.632
mp-1076470 Sr2Ca6Co7CuO20 triclinic P1 -2.006 0.219 144 1819.1 4.425
mp-1076473 BaSr7MnFe7O20 triclinic P1 -2.470 0.021 144 2066.3 4.875
mp-1076479 Sr3Ca5FeCo7O20 triclinic P1 -2.242 0.037 144 1860.9 4.467
mp-1076481 K5Na3Nb5(WO8)3 triclinic P1 -2.593 0.019 40 523.0 5.285
mp-1076482 Sr3Ca5Mn3(FeO4)5 triclinic P1 -2.503 0.072 144 1922.6 4.240
mp-1076483 La4Sm4Co7CuO20 triclinic P1 -2.642 0.114 144 1946.1 6.666
mp-1076484 K3Na5V2(MoO4)6 monoclinic Pm -2.170 0.088 40 490.6 4.379
mp-1076485 Ca7MgMn8O24 cubic Pm3m -2.156 0.380 40 435.6 4.302
mp-1076487 Sr7CaMnFe7O20 triclinic P1 -2.490 0.019 144 2010.3 4.689
mp-1076488 Sr6Ca2Fe3(CoO4)5 triclinic P1 -2.293 0.037 144 1945.2 4.740
mp-1076491 Ba4Sr4Co3Cu5O24 triclinic P1 -1.760 0.129 40 496.3 5.950
mp-1076492 La6Sm2Co7AgO20 triclinic P1 -2.644 0.103 144 1978.3 6.630
mp-1076493 BaSr7Ti5Mn3O20 triclinic P1 -3.135 0.088 144 2083.9 4.701
mp-1076496 SrCaMn2O5 triclinic P1 -2.562 0.053 144 1939.5 4.350
mp-1076502 Sr4Ca4Fe3(CoO4)5 triclinic P1 -2.303 0.046 144 1896.3 4.529
mp-1076505 Sr3CaTiMn3O10 triclinic P1 -2.820 0.051 144 2002.6 4.482
mp-1076508 La2Cr2O5 orthorhombic Ima2 -2.877 0.207 18 254.1 6.035
mp-1076509 K4Na4VMo7O20 triclinic P1 -1.974 0.186 144 2066.0 4.150
mp-1076510 K5Na3Ta8O24 tetragonal P4/mmm -3.078 0.006 40 517.9 6.721
mp-1076512 K5Na3Ta3Nb5O24 triclinic P1 -2.927 0.019 40 522.2 5.265
mp-1076513 La7SmMn7CuO20 triclinic P1 -2.896 0.149 144 2111.8 5.947
mp-1076516 Sr5Ca3Fe7CoO20 triclinic P1 -2.457 0.026 144 1945.1 4.536
mp-1076521 Ba2Ti2O5 orthorhombic Imma -3.203 0.096 18 272.9 5.481
mp-1076526 Ca7Mg(Co2O5)4 triclinic P1 -2.176 0.080 144 1744.5 4.174
mp-1076527 Mg2Cu2O5 orthorhombic Ima2 -1.680 0.174 18 187.5 4.530
mp-1076528 BaSr3Co2(CuO6)2 orthorhombic Cmm2 -1.832 0.094 40 482.6 5.761
mp-1076529 La6Sm2Cr3Fe5O24 monoclinic Pm -2.910 0.132 40 488.3 6.642
mp-1076534 RbTaO3 cubic Pm3m -2.987 0.057 5 67.5 7.737
mp-1076540 K3Na5VMo7O20 triclinic P1 -1.999 0.156 144 2029.6 4.172
mp-1076543 Ca7MgTiMn7O24 trigonal R3m -2.502 0.161 40 441.6 4.216
mp-1076545 K2Na6V5Mo3O20 triclinic P1 -2.221 0.089 144 1923.8 3.724
mp-1076546 K4Na4Mo7WO24 tetragonal P4mm -2.131 0.079 40 511.1 4.834
mp-1076548 Ca2Cu2O5 orthorhombic Ima2 -1.942 0.138 18 221.1 4.315
mp-1076557 Sr5Ca3Ti5Mn3O20 triclinic P1 -3.160 0.088 144 1995.1 4.270
mp-1076561 Sr4Ca4TiMn7O24 monoclinic Cm -2.587 0.076 40 456.9 4.824
mp-1076570 Sr7CaTi7MnO24 trigonal R3m -3.422 0.013 40 482.2 4.916
mp-1076580 La5Sm3Cr6(FeO12)2 orthorhombic Amm2 -2.982 0.148 40 482.0 6.730
mp-1076581 La7SmTi3V5O24 monoclinic Cm -3.324 0.131 40 496.2 6.376
mp-1076584 La6Sm2V3Cr5O24 monoclinic Pm -3.100 0.127 40 487.3 6.579
mp-1076592 BaSr7MnFe7O24 trigonal R3m -2.336 0.013 40 484.6 5.415
mp-1076595 La7SmTi2V6O20 triclinic P1 -3.037 0.256 144 1993.0 6.146
mp-1076597 Sr7CaMn2(FeO4)6 orthorhombic Amm2 -2.258 0.121 40 476.2 5.169
mp-1076598 La7SmMn2(FeO4)6 orthorhombic Cmm2 -2.623 0.386 40 487.0 6.654
mp-1076600 Ba3Sr5Co3Cu5O24 triclinic P1 -1.772 0.116 40 489.4 5.865
mp-1076601 Sr5Ca3Mn6(FeO10)2 triclinic P1 -2.532 0.054 144 1963.4 4.464
mp-1076602 Sr3Ca5Fe4(CoO6)4 monoclinic Cm -2.146 0.051 40 452.6 4.793
mp-1076603 La5Sm3Cr8O24 tetragonal P4/mmm -3.062 0.132 40 482.2 6.701
mp-1076606 KNaMo2O5 triclinic P1 -1.927 0.192 144 2087.1 4.251
mp-1076610 La7SmMnFe7O24 trigonal R3m -2.812 0.169 40 490.9 6.604
mp-1076611 La3SmCr2(FeO6)2 orthorhombic Pmm2 -2.948 0.125 20 243.2 6.655
mp-1076614 Sr3Ca5Fe5Co3O20 triclinic P1 -2.380 0.054 144 1883.0 4.371
mp-1076626 Sr2Ca6FeCo7O24 orthorhombic Amm2 -2.037 0.058 40 444.1 4.741
mp-1076627 Sr2TiMnO5 orthorhombic Ima2 -3.089 0.039 36 511.6 4.648
mp-1076628 Sr3Ca5Ti3Mn5O24 triclinic P1 -2.859 0.069 40 460.4 4.564
mp-1076630 KNa7V8O20 monoclinic Cc -2.222 0.180 72 899.5 3.424
mp-1076631 Sr7CaFe6(CoO10)2 triclinic P1 -2.407 0.019 144 1988.9 4.763
mp-1076633 KVO3 cubic Pm3m -2.200 0.217 5 57.2 4.007
mp-1076637 K3Na5V2(Mo3O10)2 triclinic P1 -2.043 0.153 144 2011.4 4.061
mp-1076638 RbVO3 cubic Pm3m -2.058 0.357 5 60.0 5.102
mp-1076642 NaCrO3 cubic Pm3m -1.726 0.296 5 52.7 3.879
mp-1076651 Sr7CaMn3Fe5O24 monoclinic Cm -2.377 0.025 40 475.5 5.173
mp-1076652 Mg2Ti2O5 orthorhombic Ima2 -2.950 0.257 18 203.5 3.660
mp-1076656 La5Sm3Ni7AgO20 triclinic P1 -2.445 0.138 144 1985.7 6.637
mp-1076659 KNaMoWO6 tetragonal P4mm -2.190 0.019 40 514.1 5.657
mp-1076664 La7SmTiV7O20 triclinic P1 -2.973 0.250 144 2048.1 5.990
mp-1076665 KNa7V7CrO24 trigonal R3m -2.167 0.184 40 435.9 3.782
mp-1076669 La7SmMn6(FeO12)2 orthorhombic Amm2 -2.710 0.406 40 490.4 6.596
mp-1076671 La7SmMn4(FeO6)4 tetragonal P4mm -2.863 0.201 40 492.0 6.581
mp-1076674 Sr4Ca4Fe3Co5O24 triclinic P1 -2.125 0.036 40 460.9 4.889
mp-1076675 SrCa3(Co2O5)2 triclinic P1 -2.215 0.033 144 1829.4 4.383
mp-1076678 Sr6Ca2Co5Cu3O20 triclinic P1 -1.996 0.150 144 1885.8 4.970
mp-1076679 La7SmV7CrO24 trigonal R3m -3.137 0.131 40 496.3 6.409
mp-1076680 Sr2Ca2TiMn3O10 triclinic P1 -2.828 0.062 144 1951.2 4.276
mp-1076681 BaSr7Co6(CuO12)2 orthorhombic Amm2 -1.853 0.140 40 469.6 5.712
mp-1076683 Ba3Sr5Co4(CuO5)4 triclinic P1 -1.999 0.097 144 2035.9 5.416
mp-1076685 K4Na4MoW7O24 tetragonal P4mm -2.178 0.013 40 516.7 6.476
mp-1076688 Sr3CaCo3CuO12 orthorhombic Pma2 -1.834 0.171 40 460.8 5.300
mp-1076695 Sr7CaTi8O20 triclinic P1 -3.275 0.071 144 1986.9 4.534
mp-1076696 K2Cr2O5 orthorhombic Ima2 -1.668 0.482 18 262.6 3.316
mp-1076706 SmCuO3 cubic Pm3m -2.297 0.124 5 55.3 7.869
mp-1076711 SrCuO3 cubic Pm3m -1.747 0.010 5 58.6 5.642
mp-1076718 Sr2Mn2O5 orthorhombic Ima2 -2.559 0.018 18 250.6 4.838
mp-1076723 La7SmNi6(AgO12)2 orthorhombic Amm2 -2.173 0.164 40 478.1 7.206
mp-1076724 La4Sm4Co7AgO20 triclinic P1 -2.628 0.118 144 1950.1 6.803
mp-1076732 KCrO3 cubic Pm3m -1.688 0.390 5 57.7 4.001
mp-1076737 Rb2Ta2O5 orthorhombic Imma -2.569 0.268 18 278.1 7.319
mp-1076741 Sr6Ca2Co7CuO24 orthorhombic Cmm2 -1.853 0.176 40 456.7 5.330
mp-1076747 Sr7CaFe4(CoO6)4 trigonal R3m -2.156 0.034 40 465.0 5.344
mp-1076750 Sr3Ca5Mn7FeO20 triclinic P1 -2.550 0.064 144 1916.5 4.241
mp-1076751 K4Na4NbW7O24 tetragonal P4mm -2.258 0.013 40 515.2 6.485
mp-1076754 K4Na4Mo7WO20 triclinic P1 -1.904 0.197 144 2089.2 4.527
mp-1076755 K4Na4Nb3(WO4)5 triclinic P1 -2.114 0.256 144 2113.9 5.550
mp-1076758 Sr7CaFe5Co3O20 triclinic P1 -2.360 0.030 144 1972.1 4.814
mp-1076759 LaSmCo2O5 triclinic P1 -2.667 0.114 144 1941.9 6.665
mp-1076761 Sr3Ca(Fe2O5)2 triclinic P1 -2.493 0.016 144 1996.7 4.566
mp-1076765 La4Sm4Ni7AgO20 triclinic P1 -2.440 0.143 144 1969.2 6.732
mp-1076766 La5Sm3VCr7O20 triclinic P1 -2.851 0.251 144 2018.0 6.189
mp-1076769 Sr6Ca2Fe5Co3O20 triclinic P1 -2.367 0.034 144 1949.2 4.709
mp-1076776 SrCa3TiMn3O10 triclinic P1 -2.837 0.068 144 1906.9 4.044
mp-1076782 BaCoO3 cubic Pm3m -1.886 0.222 5 63.1 6.426
mp-1076792 La7SmMn7FeO24 trigonal R3m -2.903 0.236 40 489.5 6.605
mp-1076796 Sr5Ca3Mn4(FeO6)4 monoclinic Cm -2.168 0.266 40 468.2 4.914
mp-1076797 La7SmMn6(FeO10)2 triclinic P1 -2.915 0.130 144 2130.0 5.875
mp-1076800 BaCuO3 cubic Pm3m -1.672 0.079 5 64.2 6.439
mp-1076802 Sr3Ca5Fe5(CoO8)3 triclinic P1 -2.187 0.044 40 455.0 4.756
mp-1076805 Sr6Ca2Fe3Co5O24 monoclinic P2 -2.129 0.028 40 462.0 5.219
mp-1076810 LaSmNi2O5 triclinic P1 -2.447 0.168 144 1913.5 6.757
mp-1076812 K2Na2Nb(WO4)3 orthorhombic Pmm2 -2.327 0.031 20 257.3 6.199
mp-1076820 MgCoO3 cubic Pm3m -1.409 0.550 5 50.6 4.311
mp-1076821 KNa7V7CrO20 triclinic P1 -2.282 0.110 144 1780.7 3.464
mp-1076827 Sr7CaTi3Mn5O24 monoclinic Cm -2.878 0.034 40 474.0 5.099
mp-1076829 SrCa7Fe2(CoO4)6 orthorhombic Amm2 -1.866 0.265 40 441.7 4.577
mp-1076831 KNa(MoO3)2 tetragonal P4/mmm -2.101 0.108 10 125.7 4.624
mp-1076836 K2Na2Mo3WO12 tetragonal P4/mmm -2.160 0.051 40 509.3 5.137
mp-1076848 Sm2Ag2O5 orthorhombic Ima2 -2.173 0.179 18 274.8 7.208
mp-1076854 Sr3Ca5Mn3Fe5O24 triclinic P1 -2.356 0.057 40 461.2 4.649
mp-1076858 Sr7CaFe7CoO24 trigonal R3m -2.283 0.013 40 474.2 5.208
mp-1076861 SrCa7FeCo7O24 trigonal R3m -2.026 0.070 40 437.1 4.637
mp-1076862 Sr2Ca6Mn5Fe3O20 triclinic P1 -2.511 0.093 144 1900.0 4.118
mp-1076863 Ba2Fe2O5 orthorhombic Ima2 -2.378 0.036 18 281.6 5.499
mp-1076866 La7SmCo6(AgO10)2 triclinic P1 -2.602 0.111 144 2007.8 6.656
mp-1076871 La7SmCo6(CuO10)2 triclinic P1 -2.359 0.376 144 1987.4 6.428
mp-1076874 La5Sm3Co7CuO20 triclinic P1 -2.392 0.365 144 1978.3 6.519
mp-1076875 Sr3CaTi2Mn2O10 triclinic P1 -3.095 0.051 144 1998.9 4.443
mp-1076877 Sr2Ca6TiMn7O20 triclinic P1 -2.703 0.068 144 1892.4 4.100
mp-1076878 La7SmV8O20 triclinic P1 -2.914 0.238 144 2082.8 5.900
mp-1076879 La5Sm3V2Cr6O20 triclinic P1 -2.865 0.248 144 2007.3 6.219
mp-1076880 La7SmCo5Cu3O20 triclinic P1 -2.402 0.307 144 1981.2 6.464
mp-1076881 Ba3Sr5Co3(CuO4)5 triclinic P1 -1.878 0.187 144 2037.9 5.425
mp-1076884 Sr6Ca2Fe7CoO20 triclinic P1 -2.450 0.022 144 1972.9 4.632
mp-1076885 La7SmTi3V5O20 triclinic P1 -3.089 0.274 144 2002.6 6.106
mp-1076886 K5Na3Nb5W3O20 triclinic P1 -2.303 0.251 144 2144.0 4.958
mp-1076888 K3Na5V3(MoO4)5 triclinic P1 -2.096 0.141 144 1991.9 3.951
mp-1076889 La7SmV7CrO20 triclinic P1 -2.902 0.252 144 2047.9 6.004
mp-1076890 K4Na4Mo5W3O20 triclinic P1 -1.858 0.243 144 2101.5 5.056
mp-1076891 K2Na2Mo3WO10 triclinic P1 -1.880 0.221 144 2093.3 4.797
mp-1076892 BaSr7Fe7CoO20 triclinic P1 -1.691 0.753 144 2057.3 4.909
mp-1076893 Ba2Sr6Co5Cu3O20 triclinic P1 -2.010 0.113 144 2005.7 5.317
mp-1076894 K5Na3Nb7WO20 triclinic P1 -2.457 0.237 144 2141.9 4.399
mp-1076896 Ba4Sr4Co3(CuO4)5 triclinic P1 -1.891 0.176 144 2027.1 5.617
mp-1076897 Ca7MgMn8O20 triclinic P1 -2.542 0.096 144 1820.5 3.883
mp-1076898 BaSr3Co2(CuO5)2 triclinic P1 -2.010 0.083 144 1989.9 5.375
mp-1077617 Eu2Fe2O5 orthorhombic Ima2 -0.949 1.592 18 244.9 6.721
mp-1077622 EuAgO3 cubic Pm3m -1.517 0.266 5 68.4 7.475
mp-1077659 Sr5Ca3Ti5Mn3O24 triclinic P1 -3.142 0.040 40 472.9 4.728
mp-1077660 Sr8Fe7CoO24 cubic Pm3m -2.277 0.015 40 477.9 5.333
mp-1077663 SrCa7TiMn7O24 trigonal R3m -2.576 0.099 40 447.2 4.399
mp-1077667 SrCa7Mn6(FeO12)2 orthorhombic Amm2 -2.392 0.103 40 449.8 4.406
mp-1077669 Sr2Ca2TiMn3O12 monoclinic Pm -2.528 0.266 40 461.4 4.751
mp-1077670 Sr6Ca2Mn3Fe5O24 monoclinic P2 -2.371 0.036 40 470.8 5.058
mp-1077671 Sr6Ca2Mn5(FeO8)3 monoclinic P2 -2.405 0.049 40 469.0 5.070
mp-1077688 SrCa7TiMn7O20 triclinic P1 -2.707 0.071 144 1874.8 3.970
mp-1077691 SrCa7Mn6(FeO10)2 triclinic P1 -2.541 0.081 144 1872.0 4.008
mp-1077695 Sr3Ca5TiMn7O20 triclinic P1 -2.697 0.065 144 1921.3 4.203
mp-1097775 Ba2Cu2O5 orthorhombic Ima2 -1.834 0.101 18 273.9 5.842
mp-1097890 Eu2Ni2O5 monoclinic Cm -2.039 0.189 18 236.2 7.049
mp-1099583 SmTiO3 cubic Pm3m -3.453 0.196 5 60.0 6.820
mp-1099588 SmFeO3 cubic Pm3m -2.686 0.222 5 59.7 7.066
mp-1099591 NaVO3 cubic Pm3m -2.246 0.142 5 53.7 3.767
mp-542899 Sr2Co2O5 orthorhombic Ima2 -2.027 0.175 18 244.9 5.060
mp-1099600 Sr2Ca6Co7CuO24 orthorhombic Amm2 -1.868 0.169 40 442.9 4.783
mp-1099601 K4Na4Mo3W5O24 orthorhombic Pmm2 -2.192 0.011 40 515.5 5.925
mp-1099602 Ba3Sr(CuO3)4 tetragonal P4/mmm -1.686 0.071 20 257.4 6.102
mp-1099603 Sr5Ca3Mn6(FeO12)2 monoclinic Pm -2.310 0.172 40 462.7 4.965
mp-1099605 Sr2Ca2Fe(CoO4)3 monoclinic Pm -1.893 0.233 40 456.0 4.953
mp-1099606 K3Na5V3Mo5O24 triclinic P1 -2.182 0.103 40 486.9 4.259
mp-1099611 Sr4Ca4Co7CuO24 monoclinic Cm -1.879 0.154 40 445.4 5.111
mp-1099619 EuMnO3 cubic Pm3m -2.614 0.050 5 58.3 7.263
mp-1099622 K5Na3Nb7WO24 monoclinic Cm -2.761 0.018 40 525.5 4.685
mp-1099624 BaSr7Ti5Mn3O24 monoclinic Cm -3.147 0.020 40 486.7 5.250
mp-1099625 Sm2Ni2O5 orthorhombic Ima2 -2.427 0.185 18 233.3 7.092
mp-1099626 La2Fe2O5 orthorhombic Ima2 -2.854 0.072 18 259.8 6.002
mp-1099627 La2Mn2O5 orthorhombic Ima2 -2.951 0.095 18 269.5 5.763
mp-1099629 K2Na6V5(MoO8)3 monoclinic P2 -2.209 0.124 40 465.1 4.080
mp-1099653 Sr2Ca6FeCo7O20 triclinic P1 -2.244 0.043 144 1838.3 4.351
mp-1099661 Sr7CaMn3(FeO4)5 triclinic P1 -2.491 0.042 144 2011.6 4.680
mp-1099664 KNa7V8O24 cubic Pm3m -2.238 0.156 40 431.5 3.815
mp-1099665 Sr2Ca2FeCo3O10 triclinic P1 -2.272 0.038 144 1894.9 4.543
mp-1099668 SmNiO3 cubic Pm3m -2.265 0.122 5 54.6 7.816
mp-1099669 KNa7V7MoO20 triclinic P1 -2.290 0.083 144 1825.6 3.538
mp-1099672 Sr5Ca3Mn7FeO20 triclinic P1 -2.546 0.050 144 1955.5 4.479
mp-1099674 Sr2Ca2Mn3FeO12 monoclinic Pm -2.404 0.082 40 460.0 4.823
mp-1099675 La5Sm3V2Cr6O24 orthorhombic Amm2 -2.874 0.338 40 481.3 6.705
mp-1099676 Ba4Sr4CoCu7O24 monoclinic Cm -1.713 0.089 40 496.4 5.979
mp-1099678 Sr3CaCo3CuO10 triclinic P1 -1.994 0.178 144 1886.6 4.952
mp-1099682 BaSr7Ti8O20 triclinic P1 -3.265 0.069 144 2022.3 4.774
mp-1099683 Na2Cr2O5 orthorhombic Ima2 -1.966 0.187 18 211.4 3.612
mp-1099685 BaSr7(FeO3)8 cubic Pm3m -2.315 0.004 40 486.4 5.399
mp-1099687 K4Na4Nb3W5O24 orthorhombic Pmm2 -2.422 0.020 40 518.9 5.858
mp-1099692 Sr7CaMn4(FeO5)4 triclinic P1 -2.495 0.051 144 2013.9 4.672
mp-1099694 SrCaCo2O5 triclinic P1 -2.204 0.029 144 1863.2 4.642
mp-1099696 SrCa7Mn7FeO24 trigonal R3m -2.418 0.103 40 447.3 4.428
mp-1099698 La4Sm4Co7AgO24 monoclinic Cm -2.418 0.165 40 451.7 7.579
mp-1099701 Sr7CaMnFe7O24 trigonal R3m -2.342 0.014 40 476.2 5.172
mp-1099702 Sr2Ca6TiMn7O24 orthorhombic Amm2 -2.580 0.091 40 449.4 4.553
mp-1099703 Sr3CaTi3MnO12 orthorhombic Pma2 -3.281 0.028 40 479.6 4.802
mp-1099704 La7SmMn7FeO20 triclinic P1 -2.927 0.118 144 2131.5 5.868
mp-1099708 Sr3Ca5Fe4(CoO5)4 triclinic P1 -2.341 0.054 144 1873.7 4.404
mp-1099712 K5Na3Ta2Nb6O24 orthorhombic Amm2 -2.897 0.021 40 523.5 4.973
mp-1099713 Sr7CaMn4(FeO6)4 trigonal R3m -2.392 0.032 40 475.0 5.176
mp-1099722 K2Na2MoW3O10 triclinic P1 -1.815 0.282 144 2111.9 5.860
mp-1099724 La5Sm3VCr7O24 monoclinic Cm -3.069 0.134 40 479.6 6.733
mp-1099727 K4Na4Mo5(WO8)3 orthorhombic Pmm2 -2.175 0.035 40 514.3 5.371
mp-1099742 Ba2Sr6Co3(CuO4)5 triclinic P1 -1.906 0.155 144 1994.3 5.379
mp-1099745 SrCa7Fe2(Co3O10)2 triclinic P1 -2.287 0.046 144 1811.9 4.228
mp-1099746 La7SmTi2V6O24 orthorhombic Amm2 -3.268 0.130 40 497.2 6.372
mp-1099747 Eu2Mn2O5 orthorhombic Ima2 -1.044 1.615 18 247.1 6.638
mp-1099750 Eu2V2O5 orthorhombic Ima2 -2.825 0.022 18 250.7 6.436
mp-1099757 Sm2Ti2O5 orthorhombic Imma -3.245 0.201 18 234.0 6.763
mp-1099761 Sr2Cu2O5 orthorhombic Ima2 -1.916 0.036 18 242.7 5.233
mp-1099762 Sr5Ca3Ti3Mn5O20 triclinic P1 -2.963 0.055 144 1978.3 4.353
mp-1099763 Ba2Sr2Co(CuO4)3 monoclinic Pm -1.738 0.108 40 498.2 5.942
mp-1099764 K2Ta2O5 orthorhombic Ima2 -2.670 0.188 18 265.8 6.499
mp-1099765 Eu2Cu2O5 orthorhombic Ima2 -2.115 0.111 18 230.9 7.352
mp-1099778 BaSr7Ti8O24 cubic Pm3m -3.550 0.004 40 496.1 5.080
mp-1099786 Ca2Co2O5 orthorhombic Ima2 -2.016 0.248 18 224.7 4.109
mp-1099788 Sr2Ca6Mn7FeO24 orthorhombic Amm2 -2.422 0.096 40 451.9 4.557
mp-1099795 Ba7Sr(Cu2O5)4 triclinic P1 -1.834 0.105 144 2187.1 5.701
mp-1099798 Sr5Ca3Fe2(Co3O10)2 triclinic P1 -2.267 0.036 144 1920.1 4.648
mp-1099799 Sr4Ca4TiMn7O20 triclinic P1 -2.693 0.060 144 1947.8 4.308
mp-1099805 Mg2Mn2O5 orthorhombic Ima2 -2.354 0.157 18 197.1 4.019
mp-1099808 La7SmCrFe7O24 trigonal R3m -2.850 0.133 40 490.4 6.602
mp-1099810 Sr2Ca6Mn7FeO20 triclinic P1 -2.553 0.070 144 1890.7 4.132
mp-1099812 Ba2Sr2CoCu3O10 triclinic P1 -1.905 0.131 144 2047.3 5.577
mp-1099816 Sr5Ca3FeCo7O20 triclinic P1 -2.236 0.029 144 1903.3 4.700
mp-1099821 K2Na2Mo(WO4)3 orthorhombic Pmm2 -2.170 0.027 20 257.5 6.215
mp-1099822 Rb2Mo2O5 orthorhombic Ima2 -1.723 0.388 18 294.8 4.988
mp-1099824 Ba7Sr(CuO3)8 cubic Pm3m -1.676 0.078 40 511.2 6.306
mp-1099827 Sr3Ca5FeCo7O24 monoclinic Cm -2.028 0.066 40 444.9 4.910
mp-1099831 Ca7MgMn7FeO20 triclinic P1 -2.518 0.109 144 1814.3 3.900
mp-1099832 La7SmMn7CuO24 trigonal R3m -2.836 0.300 40 485.0 6.693
mp-1099837 K2V2O5 orthorhombic Ima2 -2.117 0.306 18 269.5 3.205
mp-1099844 Sr2Ca2Co3CuO12 monoclinic Pm -1.841 0.169 40 455.4 5.016
mp-1099847 SrCa7FeCo7O20 triclinic P1 -2.254 0.040 144 1805.9 4.254
mp-1099855 Sr3CaTiMn3O12 orthorhombic Pma2 -2.726 0.060 40 467.3 5.029
mp-1099860 K5Na3Ta6Nb2O24 monoclinic Pm -3.017 0.012 40 521.4 6.114
mp-1099861 La7SmMn5Fe3O20 triclinic P1 -2.904 0.141 144 2105.1 5.947
mp-1099862 BaSr7Fe6(CoO10)2 triclinic P1 -2.388 0.024 144 2043.5 4.952
mp-1099865 La7SmMn8O20 triclinic P1 -2.940 0.105 144 2146.7 5.824
mp-1099867 KNa3V2(MoO6)2 orthorhombic Cmm2 -2.214 0.092 40 476.9 4.135
mp-1099868 KNa3V2(MoO5)2 triclinic P1 -2.183 0.090 144 1944.4 3.838
mp-1099871 La7SmNi6(AgO10)2 triclinic P1 -2.108 0.445 144 2083.9 6.408
mp-1099873 CaCuO3 cubic Pm3m -1.707 0.165 5 55.0 4.575
mp-1099875 Na2Mo2O5 orthorhombic Ima2 -1.967 0.142 18 243.5 4.336
mp-1099877 SrCaTiMnO5 triclinic P1 -3.106 0.053 144 1969.3 4.189
mp-1099881 Sr2TiMnO6 cubic Pm3m -2.943 0.096 40 480.6 5.170
mp-1099885 La3SmV2Cr2O10 triclinic P1 -2.876 0.261 144 1981.4 6.255
mp-1099886 Ba3SrCo(CuO4)3 orthorhombic Amm2 -1.720 0.126 20 253.2 6.173
mp-1099887 La7SmMn5(FeO8)3 monoclinic Cm -2.859 0.231 40 480.7 6.732
mp-1099889 Sr7CaTi7MnO20 triclinic P1 -3.229 0.117 144 2014.6 4.495
mp-1099890 Sr2Ca6Fe3Co5O24 orthorhombic Amm2 -2.111 0.053 40 450.5 4.652
mp-1099892 La6Sm2Cr3(FeO4)5 triclinic P1 -2.851 0.169 144 2077.7 6.040
mp-1099896 La6Sm2Cr5(FeO8)3 monoclinic Pm -2.882 0.222 40 482.3 6.699
mp-1099902 La7SmMnFe7O20 triclinic P1 -2.842 0.108 144 2070.7 6.058
mp-1099904 Ba2Mn2O5 orthorhombic Ima2 -2.466 0.020 18 280.8 5.494
mp-1099905 La2Ti2O5 orthorhombic Ima2 -3.326 0.136 18 245.1 6.145
mp-1099907 Ca7MgFeCo7O20 triclinic P1 -2.223 0.072 144 1759.8 4.126
mp-1099912 KNa7V6Cr2O20 triclinic P1 -2.226 0.155 144 1771.4 3.486
mp-1099913 K5Na3Nb6(WO10)2 triclinic P1 -2.381 0.261 144 2133.7 4.699
mp-1099923 La7SmMn8O24 cubic Pm3m -2.920 0.221 40 488.3 6.619
mp-1099927 Eu2Ag2O5 orthorhombic Ima2 -1.795 0.173 18 271.4 7.338
mp-1099931 La6Sm2V5Cr3O20 triclinic P1 -2.881 0.266 144 1999.2 6.196
mp-1099932 KNa7V6Cr2O24 orthorhombic Amm2 -2.109 0.198 40 432.9 3.812
mp-1099934 CaCoO3 cubic Pm3m -1.944 0.118 5 53.3 4.580
mp-1099936 BaSr7Fe6(CoO12)2 orthorhombic Amm2 -2.237 0.033 40 482.3 5.467
mp-1099938 K3Na5VMo7O24 monoclinic Cm -2.154 0.077 40 499.2 4.454
mp-1099943 K5Na3Nb4(WO6)4 monoclinic Cm -2.490 0.039 40 520.0 5.606
mp-1099945 KNaW2O5 triclinic P1 -1.795 0.290 144 2124.6 6.375
mp-1099946 Sr7CaFe7CoO20 triclinic P1 -1.756 0.705 144 1994.6 4.740
mp-1099948 K4Na4NbW7O20 triclinic P1 -1.907 0.274 144 2122.4 6.097
mp-1099951 Sm2Cr2O5 orthorhombic Ima2 -2.828 0.205 18 244.3 6.590
mp-1099952 Ca7MgCo7CuO20 triclinic P1 -2.146 0.087 144 1733.6 4.218
mp-1099956 KNa7V6(MoO10)2 triclinic P1 -2.210 0.131 144 1858.7 3.636
mp-1099972 K4Na4MoW7O20 triclinic P1 -1.815 0.277 144 2123.0 6.105
mp-1099974 Sr6Ca2MnFe7O20 triclinic P1 -2.495 0.025 144 1988.2 4.583
mp-1099978 La6Sm2Cr5Fe3O20 triclinic P1 -2.856 0.227 144 2066.3 6.049
mp-1099990 BaSr7Co4(CuO5)4 triclinic P1 -2.016 0.075 144 1973.2 5.253
mp-1100009 Sr4Ca4FeCo7O20 triclinic P1 -2.240 0.032 144 1877.6 4.596
mp-1100028 La5Sm3Cr8O20 triclinic P1 -2.855 0.237 144 2016.6 6.197
mp-1100047 La5Sm3Cr7FeO20 triclinic P1 -2.850 0.241 144 2011.5 6.226
mp-1100068 BaSr7Co5Cu3O20 triclinic P1 -1.905 0.215 144 1974.4 5.234
mp-1100141 K5Na3Ta7NbO20 triclinic P1 -2.666 0.192 144 2075.9 6.220
mp-19025 LaMnO3 cubic Pm3m -2.940 0.201 5 61.4 6.544
mp-19035 BaFeO3 cubic Pm3m -2.248 0 5 65.6 6.105
mp-2998 BaTiO3 cubic Pm3m -3.487 0.015 5 65.7 5.892
mp-4170 NaTaO3 cubic Pm3m -3.065 0.015 5 63.2 6.620
mp-4651 SrTiO3 tetragonal I4/mcm -3.562 0 10 122.6 4.972
mp-5229 SrTiO3 cubic Pm3m -3.561 0.001 5 61.4 4.962
mp-556076 Sr2Co2O5 triclinic P1 -2.193 0.252 18 244.0 5.078
mp-5827 CaTiO3 cubic Pm3m -3.502 0.064 5 58.8 3.836
mp-755018 RbTaO3 trigonal R3m -2.991 0.053 5 68.5 7.622
mp-756315 EuVO3 cubic Pm3m -2.935 0 5 59.1 7.047
mp-754941 EuCrO3 cubic Pm3m -2.729 0.078 5 58.4 7.165
mp-975138 RbWO3 cubic Pm3m -2.033 0.156 5 66.8 7.883
mp-975292 RbMoO3 cubic Pm3m -2.028 0.192 5 66.6 5.722