material

Cs

ID:

mp-1

DOI:

10.17188/1184811


Tags: Cesium - LT Cesium

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.039 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
1.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cs
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Im3m [229]
Hall
-I 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 44754 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.000 65.5
Cu (mp-30) <1 0 0> <1 0 0> 0.000 340.1
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.000 189.0
GaN (mp-804) <1 1 0> <1 1 0> 0.000 320.7
ZnO (mp-2133) <0 0 1> <1 1 1> 0.000 65.5
BN (mp-984) <0 0 1> <1 1 1> 0.000 65.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.000 151.2
SiC (mp-11714) <0 0 1> <1 0 0> 0.001 264.5
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 1 0> 0.001 160.3
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.001 196.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.001 189.0
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.001 196.4
SiC (mp-7631) <0 0 1> <1 0 0> 0.001 264.5
Mg (mp-153) <1 1 1> <1 0 0> 0.001 151.2
AlN (mp-661) <0 0 1> <1 1 1> 0.001 261.8
AlN (mp-661) <1 0 0> <1 0 0> 0.001 189.0
MgO (mp-1265) <1 1 1> <1 0 0> 0.001 189.0
SiC (mp-8062) <1 1 1> <1 0 0> 0.001 264.5
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.002 264.5
LaF3 (mp-905) <0 0 1> <1 0 0> 0.002 226.8
SiC (mp-11714) <1 0 0> <1 0 0> 0.002 189.0
SiC (mp-7631) <1 0 0> <1 0 0> 0.002 189.0
BN (mp-984) <1 0 1> <1 0 0> 0.002 302.3
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.003 151.2
SiO2 (mp-6930) <1 1 1> <1 0 0> 0.003 264.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.003 151.2
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.003 261.8
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.004 151.2
Te2Mo (mp-602) <1 1 1> <1 0 0> 0.004 189.0
LiF (mp-1138) <1 1 0> <1 1 0> 0.004 213.8
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.004 196.4
Al (mp-134) <1 1 1> <1 1 1> 0.004 196.4
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.004 261.8
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.005 226.8
ZrO2 (mp-2858) <0 1 1> <1 1 1> 0.005 196.4
WSe2 (mp-1821) <1 1 1> <1 1 1> 0.005 261.8
Mg (mp-153) <1 1 0> <1 1 0> 0.006 320.7
C (mp-66) <1 0 0> <1 1 0> 0.006 267.2
SiC (mp-7631) <1 0 1> <1 0 0> 0.006 189.0
CaCO3 (mp-3953) <1 0 0> <1 1 1> 0.007 261.8
GaN (mp-804) <1 0 1> <1 1 0> 0.007 267.2
Si (mp-149) <1 0 0> <1 0 0> 0.007 151.2
InAs (mp-20305) <1 0 0> <1 0 0> 0.008 37.8
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.008 151.2
Ge (mp-32) <1 0 0> <1 0 0> 0.008 302.3
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.009 213.8
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.009 302.3
InAs (mp-20305) <1 1 0> <1 1 0> 0.009 53.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.009 37.8
InAs (mp-20305) <1 1 1> <1 1 1> 0.010 65.5
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
0.06 J/m2 (0.00 eV/Å2)
Weighted work function Φ
2.03 eV
Shape factor η
5.20
Surface energy anisotropy αγ
0.054
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(110) 0.06, 0.00 2.04 0.89
(320) 0.07, 0.00 1.97 0.00
(211) 0.07, 0.00 1.86 0.00
(310) 0.07, 0.00 1.97 0.10
(210) 0.07, 0.00 1.77 0.00
(100) 0.07, 0.00 1.97 0.01
(321) 0.07, 0.00 1.83 0.00
(221) 0.08, 0.00 1.94 0.00
(111) 0.08, 0.00 1.59 0.00
(332) 0.08, 0.00 1.65 0.00
(322) 0.08, 0.00 1.72 0.00
(311) 0.08, 0.01 1.65 0.00

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
3 tilt [111] 180.00 (110) -0.00 0.12
3 tilt [110] 109.47 (112) -0.00 0.14
3 twist [111] 60.00 (111) 0.01 0.14
5 tilt [100] 36.87 (012) 0.01 0.13
5 tilt [100] 53.13 (013) 0.02 0.12
5 twist [100] 36.87 (100) 0.02 0.12
7 twist [111] 38.21 (111) 0.01 0.15
7 tilt [111] 38.21 (132) 0.01 0.14
9 twist [110] 38.94 (110) -0.00 0.12
9 tilt [110] 38.94 (221) 0.02 0.13

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
2 2 2 0 0 0
2 2 2 0 0 0
2 2 2 0 0 0
0 0 0 1 0 0
0 0 0 0 1 0
0 0 0 0 0 1
Compliance Tensor Sij (10-12Pa-1)
21424.8 -10615 -10615 0 0 0
-10615 21424.8 -10615 0 0 0
-10615 -10615 21424.8 0 0 0
0 0 0 718.6 0 0
0 0 0 0 718.6 0
0 0 0 0 0 718.6
Shear Modulus GV
1 GPa
Bulk Modulus KV
2 GPa
Shear Modulus GR
0 GPa
Bulk Modulus KR
2 GPa
Shear Modulus GVRH
0 GPa
Bulk Modulus KVRH
2 GPa
Elastic Anisotropy
104.62
Poisson's Ratio
0.38

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -0.853 116.981 0.108 3.076
pack_evans_james -0.853 116.982 0.012 2.363
vinet -0.853 116.952 0.109 3.579
tait -0.853 116.921 0.012 4.454
birch_euler -0.853 116.959 0.014 -0.614
pourier_tarantola -0.853 116.950 0.002 1.382
birch_lagrange -0.853 116.959 0.007 5.198
murnaghan -0.853 117.050 0.012 2.290
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li3Ag2Ge3 (mp-29166) 0.0854 0.072 3
Li3Si3Ag2 (mp-29165) 0.0455 0.117 3
PuCdAu2 (mp-862859) 0.0870 0.377 3
EuAg2Sn (mp-865192) 0.0472 0.014 3
UAl2Cu (mp-19872) 0.0854 0.474 3
VFeCoGe (mp-1063914) 0.1393 0.000 4
TiFeCoAs (mp-998974) 0.1393 0.134 4
TiGaFeCo (mp-998964) 0.1393 0.000 4
TiFeCoSb (mp-998973) 0.1393 0.186 4
TiFeCoSi (mp-998971) 0.1393 0.029 4
Yb3W (mp-979939) 0.0161 0.756 2
NaNb3 (mp-977182) 0.0455 0.740 2
Ge3F (mp-976783) 0.0360 0.425 2
LaV (mp-973891) 0.0420 0.550 2
H3Pb (mp-973786) 0.0360 0.778 2
Be (mp-20) 0.0287 0.096 1
Cu (mp-998890) 0.1393 0.037 1
Kr (mp-974400) 0.1393 0.002 1
H2 (mp-632250) 0.1393 2.271 1
Ge (mp-998883) 0.1393 0.339 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv
Final Energy/Atom
-0.8566 eV
Corrected Energy
-0.8566 eV
Uncorrected energy = -0.8566 eV Corrected energy = -0.8566 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 626969
  • 44754
  • 76941
  • 626975
  • 426937
Submitted by
User remarks:
  • Cesium

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)