material

Nb4CoSi

ID:

mp-10003

DOI:

10.17188/1184816


Tags: Niobium cobalt silicon (4/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.353 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.013 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.82 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
NbCoSi + Nb
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mcc [124]
Hall
-P 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 43233 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.000 154.9
PbSe (mp-2201) <1 0 0> <0 0 1> 0.001 38.7
GaSb (mp-1156) <1 1 0> <1 0 0> 0.001 218.8
GaSb (mp-1156) <1 0 0> <0 0 1> 0.003 38.7
CdSe (mp-2691) <1 1 0> <1 0 0> 0.005 218.8
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.007 281.3
PbSe (mp-2201) <1 1 0> <1 0 0> 0.009 218.8
GaN (mp-804) <1 0 1> <1 0 0> 0.009 343.8
CdSe (mp-2691) <1 0 0> <0 0 1> 0.014 38.7
Ag (mp-124) <1 0 0> <0 0 1> 0.035 154.9
AlN (mp-661) <1 0 0> <1 0 0> 0.041 31.3
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.052 116.2
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.058 312.5
MgF2 (mp-1249) <0 0 1> <1 1 1> 0.068 176.3
InSb (mp-20012) <1 0 0> <1 1 1> 0.071 176.3
GaSe (mp-1943) <0 0 1> <1 1 0> 0.073 88.4
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.073 44.2
ZnTe (mp-2176) <1 1 1> <1 1 0> 0.073 132.6
Au (mp-81) <1 1 0> <1 0 0> 0.074 343.8
C (mp-66) <1 1 1> <1 1 0> 0.076 44.2
InAs (mp-20305) <1 1 1> <1 1 0> 0.076 132.6
Ag (mp-124) <1 1 0> <1 0 0> 0.077 343.8
CdTe (mp-406) <1 0 0> <1 1 1> 0.077 176.3
CeO2 (mp-20194) <1 1 1> <1 1 0> 0.094 309.4
SiC (mp-7631) <1 0 0> <1 0 0> 0.098 93.8
Si (mp-149) <1 1 1> <1 1 0> 0.099 309.4
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.102 248.9
SiC (mp-8062) <1 0 0> <0 0 1> 0.107 38.7
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.113 343.8
BN (mp-984) <1 0 0> <1 0 0> 0.128 156.3
Au (mp-81) <1 0 0> <0 0 1> 0.132 154.9
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.135 218.8
SiC (mp-11714) <0 0 1> <1 1 0> 0.153 353.6
BaTiO3 (mp-5986) <1 1 1> <1 0 1> 0.155 199.1
BN (mp-984) <1 0 1> <1 0 1> 0.157 99.5
CdSe (mp-2691) <1 1 1> <1 1 0> 0.158 132.6
InAs (mp-20305) <1 1 0> <1 0 0> 0.163 218.8
SiC (mp-7631) <0 0 1> <1 1 0> 0.165 353.6
AlN (mp-661) <0 0 1> <1 1 0> 0.166 265.2
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.179 38.7
NaCl (mp-22862) <1 1 1> <1 0 0> 0.191 281.3
BN (mp-984) <0 0 1> <1 1 0> 0.199 44.2
GaSb (mp-1156) <1 1 1> <1 1 0> 0.203 132.6
ZnO (mp-2133) <0 0 1> <1 1 0> 0.205 132.6
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.207 218.8
InAs (mp-20305) <1 0 0> <0 0 1> 0.211 38.7
GaN (mp-804) <1 0 0> <1 0 0> 0.220 187.5
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.223 99.5
SiC (mp-7631) <1 0 1> <0 0 1> 0.244 193.7
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.245 312.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
332 124 124 0 0 0
124 307 140 0 0 0
124 140 307 0 0 0
0 0 0 103 0 0
0 0 0 0 99 0
0 0 0 0 0 99
Compliance Tensor Sij (10-12Pa-1)
3.8 -1.1 -1.1 0 0 0
-1.1 4.4 -1.6 0 0 0
-1.1 -1.6 4.4 0 0 0
0 0 0 9.7 0 0
0 0 0 0 10.1 0
0 0 0 0 0 10.1
Shear Modulus GV
97 GPa
Bulk Modulus KV
191 GPa
Shear Modulus GR
97 GPa
Bulk Modulus KR
191 GPa
Shear Modulus GVRH
97 GPa
Bulk Modulus KVRH
191 GPa
Elastic Anisotropy
0.03
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb4CoP (mp-21447) 0.1855 0.044 3
Nb4SiNi (mp-22396) 0.1611 0.009 3
Ta4FeP (mp-22444) 0.1851 0.055 3
Nb4FeSi (mp-22312) 0.1084 0.048 3
Zr4CuP (mp-581733) 0.1569 0.063 3
Ta2Be (mp-11278) 0.2735 0.000 2
Mg2Cu (mp-865014) 0.2614 0.017 2
Mn2B (mp-20318) 0.2718 0.000 2
Ta2Co (mp-574) 0.2736 0.000 2
Th2Au (mp-1629) 0.2745 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv Co Si
Final Energy/Atom
-9.1758 eV
Corrected Energy
-109.9680 eV
Uncorrected energy = -110.1100 eV Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV Corrected energy = -109.9680 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43233
Submitted by
User remarks:
  • Niobium cobalt silicon (4/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)