material

InBi

ID:

mp-1001833

DOI:

10.17188/1273049


Tags: Indium bismuthide

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.025 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.026 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
InBi
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
F43m [216]
Hall
F 4 2 3
Point Group
43m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <1 0 0> 0.000 188.2
Cu (mp-30) <1 0 0> <1 0 0> 0.000 235.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.001 235.2
CdS (mp-672) <1 1 0> <1 1 0> 0.002 199.6
CdS (mp-672) <0 0 1> <1 1 1> 0.004 244.4
C (mp-66) <1 1 0> <1 1 0> 0.007 199.6
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.008 244.4
InP (mp-20351) <1 1 0> <1 1 0> 0.015 199.6
InP (mp-20351) <1 1 1> <1 1 1> 0.015 244.4
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.024 282.2
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.028 133.1
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.037 163.0
SiC (mp-11714) <0 0 1> <1 0 0> 0.042 329.3
SiC (mp-7631) <0 0 1> <1 0 0> 0.045 329.3
GaN (mp-804) <1 1 0> <1 1 0> 0.075 266.1
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.082 332.6
Au (mp-81) <1 1 0> <1 1 0> 0.085 199.6
CaF2 (mp-2741) <1 1 1> <1 1 0> 0.087 266.1
InAs (mp-20305) <1 0 0> <1 0 0> 0.100 188.2
CsI (mp-614603) <1 1 0> <1 1 0> 0.105 266.1
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.115 188.2
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.119 235.2
GaP (mp-2490) <1 1 1> <1 1 0> 0.119 266.1
Si (mp-149) <1 0 0> <1 0 0> 0.125 235.2
BN (mp-984) <1 0 0> <1 0 0> 0.150 235.2
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.157 81.5
SiC (mp-8062) <1 0 0> <1 0 0> 0.158 94.1
Ag (mp-124) <1 1 0> <1 1 0> 0.159 199.6
TiO2 (mp-390) <1 1 0> <1 1 0> 0.164 266.1
Cu (mp-30) <1 1 0> <1 1 0> 0.171 199.6
NaCl (mp-22862) <1 1 1> <1 0 0> 0.174 282.2
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.177 163.0
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.182 332.6
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.184 188.2
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.192 332.6
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.204 332.6
C (mp-66) <1 0 0> <1 0 0> 0.207 235.2
PbS (mp-21276) <1 1 0> <1 1 0> 0.209 199.6
PbS (mp-21276) <1 1 1> <1 1 1> 0.214 244.4
Mg (mp-153) <1 1 0> <1 1 0> 0.214 266.1
TiO2 (mp-390) <1 0 0> <1 0 0> 0.217 188.2
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.233 282.2
CdS (mp-672) <1 0 0> <1 0 0> 0.240 141.1
GdScO3 (mp-5690) <0 1 1> <1 1 1> 0.243 163.0
AlN (mp-661) <1 0 1> <1 1 0> 0.245 332.6
ZnO (mp-2133) <1 1 0> <1 1 0> 0.259 266.1
Te2W (mp-22693) <0 1 1> <1 0 0> 0.261 235.2
GaAs (mp-2534) <1 1 1> <1 0 0> 0.266 282.2
CdSe (mp-2691) <1 0 0> <1 0 0> 0.279 188.2
ZnO (mp-2133) <1 0 1> <1 1 0> 0.285 199.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
42 25 25 0 0 0
25 42 25 0 0 0
25 25 42 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 18
Compliance Tensor Sij (10-12Pa-1)
41.6 -15.4 -15.4 0 0 0
-15.4 41.6 -15.4 0 0 0
-15.4 -15.4 41.6 0 0 0
0 0 0 54.9 0 0
0 0 0 0 54.9 0
0 0 0 0 0 54.9
Shear Modulus GV
14 GPa
Bulk Modulus KV
31 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
31 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
31 GPa
Elastic Anisotropy
0.67
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zn3CrS4 (mp-1080726) 0.0175 0.129 3
Zn3CrSe4 (mp-1095028) 0.0124 0.122 3
Zn3CrTe4 (mp-1087545) 0.0105 0.114 3
CdSnSb2 (mp-10063) 0.0250 0.000 3
GaCuS2 (mp-5238) 0.0192 0.000 3
FeCu2GeS4 (mp-917359) 0.0383 0.037 4
CoCu2GeS4 (mp-6498) 0.0382 0.055 4
CoCu2GeS4 (mp-560428) 0.0476 0.055 4
FeCu2GeS4 (mp-22053) 0.0260 0.037 4
FeCu2GeSe4 (mp-1087471) 0.0871 0.037 4
TiN (mp-998908) 0.0000 0.302 2
VN (mp-1001826) 0.0000 0.325 2
TaN (mp-1009833) 0.0000 0.492 2
CuN (mp-13117) 0.0000 0.796 2
HfC (mp-1002124) 0.0000 0.641 2
O2 (mp-1057818) 0.0000 1.881 1
Si (mp-149) 0.0000 0.000 1
Sn (mp-117) 0.0000 0.000 1
C (mp-66) 0.0000 0.136 1
Se (mp-12771) 0.0000 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d Bi
Final Energy/Atom
-3.2961 eV
Corrected Energy
-6.5922 eV
Uncorrected energy = -6.5922 eV Corrected energy = -6.5922 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 184573
Submitted by
User remarks:
  • Indium bismuthide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)