material

TiAs

ID:

mp-10052

DOI:

10.17188/1185084


Tags: Titanium arsenide (1/1) - HT Titanium arsenide (1/1)

Material Details

Final Magnetic Moment
0.109 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.906 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.014 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiAs
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 44074 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaSe (mp-1943) <0 0 1> <0 0 1> 0.001 151.7
NaCl (mp-22862) <1 0 0> <1 1 1> 0.003 162.1
PbS (mp-21276) <1 1 1> <0 0 1> 0.006 186.7
Te2W (mp-22693) <0 0 1> <1 1 0> 0.007 155.3
Mg (mp-153) <0 0 1> <0 0 1> 0.007 35.0
WS2 (mp-224) <1 1 1> <0 0 1> 0.011 315.0
Mg (mp-153) <1 0 1> <0 0 1> 0.027 151.7
YVO4 (mp-19133) <1 1 0> <1 1 0> 0.032 194.1
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.033 151.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.037 35.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.037 35.0
WS2 (mp-224) <1 1 0> <0 0 1> 0.039 315.0
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.043 175.0
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.047 46.7
C (mp-48) <1 0 1> <1 0 0> 0.048 179.3
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.049 315.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.054 268.9
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.058 105.0
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.068 291.4
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.068 315.0
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.069 175.0
TePb (mp-19717) <1 1 1> <0 0 1> 0.073 221.7
BN (mp-984) <0 0 1> <0 0 1> 0.076 105.0
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.076 245.0
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.086 221.7
Te2W (mp-22693) <1 0 1> <1 1 1> 0.087 202.7
GaP (mp-2490) <1 0 0> <0 0 1> 0.093 245.0
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.098 175.0
InP (mp-20351) <1 1 1> <0 0 1> 0.098 186.7
NaCl (mp-22862) <1 1 1> <0 0 1> 0.101 221.7
Te2W (mp-22693) <1 0 0> <1 1 0> 0.102 194.1
LaF3 (mp-905) <1 0 0> <1 0 0> 0.107 268.9
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.116 175.0
KCl (mp-23193) <1 1 0> <1 1 0> 0.117 116.5
Ni (mp-23) <1 1 0> <1 1 0> 0.124 155.3
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.126 303.2
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.135 175.0
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.137 268.3
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.142 315.0
CdS (mp-672) <0 0 1> <0 0 1> 0.143 46.7
Ni (mp-23) <1 0 0> <1 1 1> 0.149 162.1
WSe2 (mp-1821) <1 0 1> <0 0 1> 0.158 256.7
Mg (mp-153) <1 1 1> <0 0 1> 0.161 245.0
SiC (mp-8062) <1 1 0> <1 0 0> 0.164 134.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.164 77.6
Cu (mp-30) <1 1 0> <0 0 1> 0.164 93.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.165 186.7
Au (mp-81) <1 1 0> <1 0 0> 0.172 224.1
C (mp-48) <0 0 1> <0 0 1> 0.180 46.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.184 44.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
165 67 101 0 0 0
67 165 101 0 0 0
101 101 196 0 0 0
0 0 0 112 0 0
0 0 0 0 112 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
9 -1.2 -4 0 0 0
-1.2 9 -4 0 0 0
-4 -4 9.3 0 0 0
0 0 0 8.9 0 0
0 0 0 0 8.9 0
0 0 0 0 0 20.4
Shear Modulus GV
72 GPa
Bulk Modulus KV
118 GPa
Shear Modulus GR
57 GPa
Bulk Modulus KR
114 GPa
Shear Modulus GVRH
65 GPa
Bulk Modulus KVRH
116 GPa
Elastic Anisotropy
1.28
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiTiTe2 (mp-10189) 0.2162 0.014 3
ScAgSe2 (mp-12908) 0.1861 0.002 3
TmAgTe2 (mp-12953) 0.2194 0.016 3
LiSnS2 (mp-27683) 0.2029 0.098 3
GdAgSe2 (mp-1097028) 0.1440 0.012 3
Li8Cr(FeO4)3 (mp-767681) 0.5527 1.033 4
Li8TiMn3O12 (mp-767679) 0.5697 0.088 4
Li8Mn(FeO4)3 (mp-766973) 0.5674 0.073 4
Li8MnCr3O12 (mp-766919) 0.6116 0.112 4
Li8Mn3CrO12 (mp-765119) 0.5643 0.107 4
ScTe (mp-10026) 0.0384 0.000 2
CrS (mp-523) 0.0412 0.125 2
IrN (mp-1066162) 0.0425 1.001 2
FeS (mp-849066) 0.0617 0.316 2
MnBi (mp-22878) 0.0452 0.449 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.6853 0.005 5
Na (mp-999501) 0.5954 0.124 1
Sb (mp-632286) 0.7467 0.059 1
Bi (mp-567379) 0.5597 0.062 1
Te (mp-570459) 0.6591 0.044 1
Bi (mp-1096851) 0.7211 0.099 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv As
Final Energy/Atom
-7.1835 eV
Corrected Energy
-28.7339 eV
-28.7339 eV = -28.7339 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 44074
  • 611502
Submitted by
User remarks:
  • Titanium arsenide (1/1) - HT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)