Final Magnetic Moment6.846 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.242 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGdB6 + B |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 282.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 293.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 239.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 293.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 282.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 159.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 319.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 159.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 239.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 282.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 159.8 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 319.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 282.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 226.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 226.0 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 293.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 226.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 282.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 282.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 226.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 239.7 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 226.0 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 226.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 113.0 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 169.5 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 293.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 226.0 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 113.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 282.5 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 159.8 |
PbS (mp-21276) | <1 1 1> | <1 1 0> | 319.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 169.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 239.7 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 293.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 169.5 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 159.8 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 0> | 239.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 239.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 226.0 |
Si (mp-149) | <1 0 0> | <1 1 0> | 239.7 |
Si (mp-149) | <1 1 0> | <1 0 0> | 169.5 |
Au (mp-81) | <1 0 0> | <1 0 0> | 226.0 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 159.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 113.0 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 339.0 |
Cu (mp-30) | <1 0 0> | <1 1 1> | 195.7 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 319.6 |
Cu (mp-30) | <1 1 1> | <1 1 1> | 293.6 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 79.9 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 79.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YB12 (mp-7817) | 0.0067 | 0.000 | 2 |
ThB12 (mp-12570) | 0.0017 | 0.010 | 2 |
NdB12 (mp-1004756) | 0.0107 | 0.050 | 2 |
SmB12 (mp-1004525) | 0.0017 | 0.017 | 2 |
EuB12 (mp-1096955) | 0.0076 | 0.102 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Gd B |
Final Energy/Atom-7.4899 eV |
Corrected Energy-97.3688 eV
-97.3688 eV = -97.3688 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)