material

CdSnSb2

ID:

mp-10063

DOI:

10.17188/1185094


Tags: Cadmium tin diantimonide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.135 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.44 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.078 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.001 44.1
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.005 309.0
InSb (mp-20012) <1 0 0> <0 0 1> 0.005 44.1
Ni (mp-23) <1 0 0> <0 0 1> 0.006 220.7
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.007 123.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.008 220.7
CdTe (mp-406) <1 0 0> <0 0 1> 0.009 44.1
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.017 353.2
Cu (mp-30) <1 0 0> <0 0 1> 0.024 220.7
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.033 220.7
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.038 309.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.038 309.0
CdTe (mp-406) <1 1 0> <1 1 0> 0.040 123.4
TiO2 (mp-2657) <1 1 1> <1 0 1> 0.043 293.4
InSb (mp-20012) <1 1 0> <1 1 0> 0.048 123.4
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.053 97.8
PbSe (mp-2201) <1 0 0> <0 0 1> 0.064 353.2
SiC (mp-8062) <1 0 0> <1 0 0> 0.073 174.6
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.078 309.0
SiC (mp-7631) <1 1 0> <1 1 0> 0.085 246.9
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.086 123.4
SiC (mp-8062) <1 1 0> <1 1 0> 0.089 246.9
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.090 353.2
GaSb (mp-1156) <1 0 0> <0 0 1> 0.094 353.2
Au (mp-81) <1 0 0> <0 0 1> 0.098 88.3
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.098 220.7
TePb (mp-19717) <1 1 0> <1 1 0> 0.100 123.4
C (mp-66) <1 0 0> <0 0 1> 0.115 220.7
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.121 220.7
CdSe (mp-2691) <1 0 0> <0 0 1> 0.122 353.2
InP (mp-20351) <1 0 0> <1 0 0> 0.138 174.6
Te2W (mp-22693) <0 0 1> <1 1 0> 0.139 246.9
LiF (mp-1138) <1 0 0> <0 0 1> 0.147 220.7
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.160 220.7
Mg (mp-153) <0 0 1> <1 1 1> 0.167 131.1
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.176 44.1
Ag (mp-124) <1 0 0> <0 0 1> 0.177 88.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.189 353.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.190 309.0
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.203 264.9
C (mp-48) <0 0 1> <0 0 1> 0.204 220.7
GaP (mp-2490) <1 1 1> <0 0 1> 0.222 264.9
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.226 262.2
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.241 353.2
TePb (mp-19717) <1 0 0> <0 0 1> 0.248 44.1
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.276 261.9
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.289 353.2
TiO2 (mp-390) <0 0 1> <0 0 1> 0.296 353.2
GdScO3 (mp-5690) <1 1 1> <1 0 1> 0.301 293.4
MgO (mp-1265) <1 0 0> <0 0 1> 0.309 88.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
52 29 28 0 0 0
29 52 28 0 0 0
28 28 51 0 0 0
0 0 0 24 0 0
0 0 0 0 24 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
31.6 -11.1 -11.4 0 0 0
-11.1 31.6 -11.4 0 0 0
-11.4 -11.4 32.2 0 0 0
0 0 0 42.2 0 0
0 0 0 0 42.2 0
0 0 0 0 0 42.8
Shear Modulus GV
19 GPa
Bulk Modulus KV
36 GPa
Shear Modulus GR
17 GPa
Bulk Modulus KR
36 GPa
Shear Modulus GVRH
18 GPa
Bulk Modulus KVRH
36 GPa
Elastic Anisotropy
0.63
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnGeAs2 (mp-4008) 0.0131 0.000 3
MgSnP2 (mp-1009083) 0.0114 0.010 3
ZnGeP2 (mp-4524) 0.0179 0.000 3
AlCuSe2 (mp-8016) 0.0032 0.000 3
GaCuS2 (mp-5238) 0.0104 0.000 3
FeCu2GeS4 (mp-917359) 0.0176 0.037 4
CoCu2GeS4 (mp-6498) 0.0286 0.055 4
CoCu2GeS4 (mp-560428) 0.0364 0.055 4
FeCu2GeS4 (mp-22053) 0.0091 0.037 4
FeCu2GeSe4 (mp-1087471) 0.0723 0.037 4
ZrO (mp-33088) 0.0250 0.424 2
CoO (mp-557513) 0.0250 0.000 2
ZnNi (mp-567903) 0.0250 1.083 2
CuS (mp-760381) 0.0230 0.013 2
CoO (mp-24864) 0.0250 0.000 2
Si (mp-149) 0.0250 0.000 1
Sn (mp-117) 0.0250 0.000 1
C (mp-66) 0.0250 0.136 1
Ge (mp-32) 0.0250 0.000 1
Se (mp-12771) 0.0250 0.514 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd Sn_d Sb
Final Energy/Atom
-3.3371 eV
Corrected Energy
-27.4645 eV
Uncorrected energy = -26.6965 eV Composition-based energy adjustment (-0.192 eV/atom x 4.0 atoms) = -0.7680 eV Corrected energy = -27.4645 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 44259
Submitted by
User remarks:
  • Cadmium tin diantimonide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)