Final Magnetic Moment1.600 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.158 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.214 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCeCu2 + Ce |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 1 0> | <1 1 0> | 267.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 267.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 237.9 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 182.1 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 89.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 168.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 327.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 89.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 189.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 327.2 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 255.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 89.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 84.1 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 255.0 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 208.2 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 1> | 291.4 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 0> | 297.4 |
CdWO4 (mp-19387) | <1 1 0> | <1 1 1> | 291.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 42.1 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 267.7 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 145.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 105.2 |
Bi2Te3 (mp-34202) | <1 0 0> | <1 0 0> | 147.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 63.1 |
BN (mp-984) | <1 1 0> | <1 1 1> | 291.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 109.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 273.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 84.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 89.2 |
Al (mp-134) | <1 1 1> | <1 1 1> | 109.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 168.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 273.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 59.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 255.0 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 327.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 119.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 126.2 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 59.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 147.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 237.9 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 105.2 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 182.1 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 273.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 315.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 189.3 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 327.2 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 255.0 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 145.7 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 255.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 36.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.4343 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.5955 | 0.057 | 4 |
TmNp3 (mp-1005727) | 0.0000 | 0.696 | 2 |
PmTl3 (mp-862970) | 0.0000 | 0.000 | 2 |
Mn3S (mp-975439) | 0.0000 | 0.477 | 2 |
Ho3Zr (mp-981545) | 0.0000 | 0.083 | 2 |
Mg3Mo (mp-978287) | 0.0000 | 0.305 | 2 |
LiCa6Ge (mp-12609) | 0.0000 | 0.184 | 3 |
ZnCu2Ni (mp-30593) | 0.4436 | 0.002 | 3 |
Cr22Ni50Mo3 (mp-767825) | 0.4406 | 0.000 | 3 |
GaCo2Ni (mp-1018060) | 0.1699 | 0.080 | 3 |
CrCoPt2 (mp-570863) | 0.2277 | 0.035 | 3 |
Na (mp-974558) | 0.0000 | 0.003 | 1 |
U (mp-1008669) | 0.0000 | 0.379 | 1 |
H2 (mp-634659) | 0.0000 | 0.000 | 1 |
Sn (mp-1022725) | 0.0000 | 0.061 | 1 |
Br (mp-998861) | 0.0000 | 0.658 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Ce Cu_pv |
Final Energy/Atom-5.3224 eV |
Corrected Energy-21.2895 eV
-21.2895 eV = -21.2895 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)