Final Magnetic Moment0.776 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.000 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3Mo |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 1 1> | 67.3 |
C (mp-48) | <1 0 0> | <1 0 0> | 168.4 |
C (mp-48) | <1 1 1> | <1 1 0> | 293.1 |
C (mp-48) | <1 0 1> | <1 0 0> | 181.3 |
C (mp-48) | <1 1 0> | <1 1 0> | 201.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 155.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 54.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 146.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 54.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 67.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 54.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 246.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 157.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 291.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 77.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 194.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 116.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 116.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 164.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 157.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 64.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 293.1 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 201.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 54.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 67.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 284.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 129.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 323.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 67.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 22.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 329.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 168.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 323.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 64.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 64.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 146.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 293.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 201.9 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 112.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 64.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 201.5 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 168.4 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 146.5 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 310.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 54.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 181.3 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 89.7 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 238.1 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 129.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
392 | 208 | 208 | 0 | 0 | 0 |
208 | 391 | 208 | 0 | 0 | 0 |
208 | 208 | 391 | 0 | 0 | 0 |
0 | 0 | 0 | 180 | 0 | 0 |
0 | 0 | 0 | 0 | 180 | 0 |
0 | 0 | 0 | 0 | 0 | 180 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.1 | -1.4 | -1.4 | 0 | 0 | 0 |
-1.4 | 4.1 | -1.4 | 0 | 0 | 0 |
-1.4 | -1.4 | 4.1 | 0 | 0 | 0 |
0 | 0 | 0 | 5.5 | 0 | 0 |
0 | 0 | 0 | 0 | 5.5 | 0 |
0 | 0 | 0 | 0 | 0 | 5.5 |
Shear Modulus GV145 GPa |
Bulk Modulus KV269 GPa |
Shear Modulus GR130 GPa |
Bulk Modulus KR269 GPa |
Shear Modulus GVRH137 GPa |
Bulk Modulus KVRH269 GPa |
Elastic Anisotropy0.57 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Be3Tc (mp-977552) | 0.0000 | 0.000 | 2 |
AlC3 (mp-1065540) | 0.0000 | 2.748 | 2 |
TiOs3 (mp-980203) | 0.0000 | 0.222 | 2 |
DyPt3 (mp-2465) | 0.0000 | 0.000 | 2 |
MgCd3 (mp-1094839) | 0.0000 | 0.015 | 2 |
H2 (mp-634659) | 0.0000 | 0.000 | 1 |
Sr (mp-76) | 0.0000 | 0.006 | 1 |
Ni (mp-1056486) | 0.0000 | 0.000 | 1 |
Cd (mp-1096861) | 0.0000 | 0.001 | 1 |
Pd (mp-1056438) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Co Mo_pv |
Final Energy/Atom-8.0431 eV |
Corrected Energy-32.1725 eV
-32.1725 eV = -32.1725 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)