Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom1.157 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.157 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCd + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 1 1> | 15.5 |
C (mp-48) | <1 1 1> | <1 0 0> | 98.1 |
C (mp-48) | <1 0 0> | <1 1 0> | 176.6 |
C (mp-48) | <1 0 1> | <1 0 0> | 205.2 |
C (mp-48) | <1 1 0> | <1 1 0> | 100.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 239.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 185.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 142.7 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 185.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 116.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 239.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 200.9 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 61.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 88.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 116.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 160.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 80.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 113.5 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 200.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 138.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 61.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 113.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 100.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 154.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 80.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 113.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 142.7 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 200.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 169.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 277.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 276.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 133.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 277.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 277.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 258.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 80.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 113.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 160.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 138.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 80.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 108.2 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 61.8 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 113.5 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 231.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 138.8 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 35.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 50.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 151.7 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 176.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 89.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlVFeCo (mp-1008530) | 0.0000 | 0.028 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.198 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.025 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.009 | 4 |
CeAg (mp-2756) | 0.0000 | 0.028 | 2 |
GdIn (mp-21005) | 0.0000 | 0.000 | 2 |
CaPd (mp-213) | 0.0000 | 0.000 | 2 |
BeCu (mp-2323) | 0.0000 | 0.012 | 2 |
PuBi (mp-1002230) | 0.0000 | 0.015 | 2 |
LiMnPd2 (mp-861629) | 0.0000 | 0.000 | 3 |
DyMgTl2 (mp-866007) | 0.0000 | 0.000 | 3 |
V2CuBr (mp-631442) | 0.0000 | 0.981 | 3 |
MgZnPd2 (mp-864923) | 0.0000 | 0.000 | 3 |
YDyRh2 (mp-979917) | 0.0000 | 0.009 | 3 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
Ge (mp-998883) | 0.0000 | 0.346 | 1 |
Ni (mp-1008728) | 0.0000 | 0.097 | 1 |
Si (mp-1014212) | 0.0000 | 0.541 | 1 |
Cu (mp-998890) | 0.0000 | 0.034 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points20 |
U Values-- |
PseudopotentialsVASP PAW: Cd N |
Final Energy/Atom-3.2762 eV |
Corrected Energy-6.5524 eV
-6.5524 eV = -6.5524 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)