Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.547 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.669 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWC |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 110.9 |
C (mp-48) | <1 0 0> | <1 0 0> | 332.6 |
C (mp-48) | <1 0 1> | <1 1 0> | 156.8 |
C (mp-48) | <1 1 1> | <1 1 0> | 344.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 125.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 125.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 125.4 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 125.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 288.2 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 230.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 250.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 110.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 288.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 153.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 268.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 94.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 199.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 344.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 268.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 153.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 250.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 177.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 243.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 199.5 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 268.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 192.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 344.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 94.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 266.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 199.5 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 268.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 268.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 94.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 192.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 94.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 115.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 177.4 |
Te2W (mp-22693) | <1 1 1> | <1 1 0> | 219.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 0> | 313.6 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 156.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 44.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 62.7 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 221.7 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 219.5 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 219.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 110.9 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 188.1 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 153.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 153.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoSi(CuS2)2 (mp-11769) | 0.0805 | 0.074 | 4 |
MnAg2GeTe4 (mp-1025568) | 0.1211 | 0.007 | 4 |
FeSi(CuSe2)2 (mp-1025510) | 0.0826 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.0166 | 0.041 | 4 |
CoCu2GeS4 (mp-6498) | 0.0349 | 0.061 | 4 |
RbSb (mp-1009650) | 0.0000 | 0.918 | 2 |
RuN (mp-1009770) | 0.0000 | 0.073 | 2 |
YC (mp-998894) | 0.0000 | 0.809 | 2 |
ZrN (mp-1009885) | 0.0000 | 0.320 | 2 |
SiSn (mp-1009813) | 0.0000 | 0.150 | 2 |
AlCuSe2 (mvc-16085) | 0.0155 | 0.000 | 3 |
CdSnSb2 (mp-10063) | 0.0155 | 0.000 | 3 |
AlCuSe2 (mp-8016) | 0.0154 | 0.000 | 3 |
ZnGeAs2 (mp-4008) | 0.0114 | 0.000 | 3 |
GaCuS2 (mp-5238) | 0.0123 | 0.000 | 3 |
Ge (mp-32) | 0.0000 | 0.000 | 1 |
C (mp-66) | 0.0000 | 0.136 | 1 |
Si (mp-149) | 0.0000 | 0.000 | 1 |
Sn (mp-117) | 0.0000 | 0.000 | 1 |
Se (mp-12771) | 0.0000 | 0.509 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points60 |
U Values-- |
PseudopotentialsVASP PAW: W_pv C |
Final Energy/Atom-10.5455 eV |
Corrected Energy-21.0909 eV
-21.0909 eV = -21.0909 eV (uncorrected energy)
|