Final Magnetic Moment3.042 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.424 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.827 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi2Ga |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 271.8 |
C (mp-48) | <1 0 1> | <1 0 0> | 310.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 271.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 349.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 349.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 155.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 164.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 201.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 310.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 38.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 54.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 67.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 67.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 271.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 38.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 54.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 67.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 329.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 310.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 38.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 67.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 310.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 201.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 310.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 109.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 269.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 194.1 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 194.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 269.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 349.4 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 274.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 349.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 194.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 269.0 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 269.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 194.1 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 194.1 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 194.1 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 271.8 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 194.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 67.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 201.7 |
BN (mp-984) | <0 0 1> | <1 1 1> | 201.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 310.6 |
BN (mp-984) | <1 1 0> | <1 1 1> | 67.2 |
BN (mp-984) | <1 1 1> | <1 0 0> | 271.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 201.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 310.6 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 271.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
34 | 57 | 57 | 0 | 0 | 0 |
57 | 34 | 57 | 0 | 0 | 0 |
57 | 57 | 34 | 0 | 0 | 0 |
0 | 0 | 0 | -13 | 0 | 0 |
0 | 0 | 0 | 0 | -13 | 0 |
0 | 0 | 0 | 0 | 0 | -13 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-25.8 | 16.2 | 16.2 | 0 | 0 | 0 |
16.2 | -25.8 | 16.2 | 0 | 0 | 0 |
16.2 | 16.2 | -25.8 | 0 | 0 | 0 |
0 | 0 | 0 | -78.2 | 0 | 0 |
0 | 0 | 0 | 0 | -78.2 | 0 |
0 | 0 | 0 | 0 | 0 | -78.2 |
Shear Modulus GV-12 GPa |
Bulk Modulus KV50 GPa |
Shear Modulus GR-12 GPa |
Bulk Modulus KR50 GPa |
Shear Modulus GVRH-12 GPa |
Bulk Modulus KVRH50 GPa |
Elastic Anisotropy0.01 |
Poisson's Ratio0.64 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SnRuW (mp-631387) | 0.0000 | 0.714 | 3 |
KTaPt (mp-631314) | 0.0000 | 1.530 | 3 |
CrFeTe (mp-1009592) | 0.0000 | 0.246 | 3 |
LiCdAs (mp-1018135) | 0.0000 | 0.000 | 3 |
GdBiPd (mp-1076916) | 0.0000 | 0.000 | 3 |
Be2Si (mp-1009829) | 0.0000 | 0.238 | 2 |
CrO2 (mp-1009555) | 0.0000 | 0.193 | 2 |
Mn2Ge (mp-1008920) | 0.0000 | 0.245 | 2 |
MgH2 (mp-1008901) | 0.0000 | 0.109 | 2 |
Ca2Ge (mp-1009755) | 0.0000 | 0.016 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Ga_d |
Final Energy/Atom-5.8484 eV |
Corrected Energy-17.5453 eV
-17.5453 eV = -17.5453 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)