Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom1.401 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.401 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2 + Pd |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 1 0> | 105.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 272.3 |
C (mp-48) | <1 0 1> | <1 1 0> | 245.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 171.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 198.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 123.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 272.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 105.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 123.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 321.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 140.0 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 171.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 198.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 173.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 140.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 272.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 105.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 198.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 300.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 280.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 280.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 123.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 198.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 105.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 321.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 140.0 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 171.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 123.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 140.0 |
InP (mp-20351) | <1 0 0> | <1 1 1> | 214.3 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 105.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 173.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 214.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 297.0 |
Te2W (mp-22693) | <1 1 1> | <1 0 0> | 222.8 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 0> | 148.5 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 321.8 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 0> | 280.0 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 128.6 |
CdWO4 (mp-19387) | <1 1 0> | <1 1 0> | 280.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 222.8 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 300.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 173.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 105.0 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 214.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 24.8 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 35.0 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 173.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 321.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ThH2 (mp-1008734) | 0.0000 | 0.010 | 2 |
CrN2 (mp-1014264) | 0.0000 | 0.891 | 2 |
PdO2 (mp-752735) | 0.0000 | 0.231 | 2 |
Ti2Ga (mp-1008726) | 0.0000 | 0.827 | 2 |
TiO2 (mp-1008677) | 0.0000 | 0.301 | 2 |
KBePt (mp-631464) | 0.0000 | 0.766 | 3 |
BeInBi (mp-631497) | 0.0000 | 0.703 | 3 |
MgAgSb (mp-1008903) | 0.0000 | 0.000 | 3 |
AlAgB (mp-631568) | 0.0000 | 0.913 | 3 |
MnCoTe (mp-1008874) | 0.0000 | 0.016 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points60 |
U Values-- |
PseudopotentialsVASP PAW: Pd N |
Final Energy/Atom-5.6245 eV |
Corrected Energy-16.8736 eV
-16.8736 eV = -16.8736 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)