material

KCu4Se3

ID:

mp-10092

DOI:

10.17188/1186025


Tags: Potassium copper selenide (1/4/3) Potassium copper tricopper(I) selenide

Material Details

Final Magnetic Moment
0.022 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.360 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.014 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.55 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
K(CuSe)2 + Cu3Se2 + Cu
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mmm [123]
Hall
-P 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 280072 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.000 208.8
MgO (mp-1265) <1 0 0> <0 0 1> 0.002 144.6
PbS (mp-21276) <1 0 0> <0 0 1> 0.002 144.6
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.002 16.1
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.003 64.3
C (mp-66) <1 0 0> <0 0 1> 0.009 64.3
C (mp-48) <0 0 1> <1 1 0> 0.010 167.8
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.013 55.9
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.013 335.6
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.015 144.6
NaCl (mp-22862) <1 0 0> <0 0 1> 0.019 32.1
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.021 160.6
ZnO (mp-2133) <1 0 0> <1 0 0> 0.021 158.2
CdS (mp-672) <1 0 0> <0 0 1> 0.025 257.0
CdS (mp-672) <1 1 1> <0 0 1> 0.025 208.8
Al (mp-134) <1 1 1> <1 1 0> 0.031 55.9
CdS (mp-672) <1 0 1> <1 0 0> 0.032 197.7
Te2W (mp-22693) <1 0 0> <1 0 0> 0.035 197.7
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.035 240.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.036 16.1
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.037 64.3
Ni (mp-23) <1 1 0> <1 1 1> 0.039 174.6
TiO2 (mp-390) <1 0 0> <1 1 0> 0.041 111.9
LiGaO2 (mp-5854) <0 1 1> <1 1 1> 0.042 174.6
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.043 85.4
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.046 32.1
TiO2 (mp-390) <1 1 0> <1 0 0> 0.046 158.2
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.047 279.6
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.050 279.6
Au (mp-81) <1 1 0> <0 0 1> 0.050 273.1
TiO2 (mp-390) <0 0 1> <0 0 1> 0.058 128.5
ZnSe (mp-1190) <1 1 1> <1 0 1> 0.061 170.7
C (mp-66) <1 1 1> <1 1 1> 0.062 291.0
MoS2 (mp-1434) <1 0 1> <1 0 0> 0.063 276.8
Al (mp-134) <1 0 0> <0 0 1> 0.066 16.1
GaSe (mp-1943) <0 0 1> <1 1 0> 0.066 111.9
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.068 208.8
CaCO3 (mp-3953) <0 0 1> <1 1 1> 0.069 291.0
Cu (mp-30) <1 1 1> <1 1 1> 0.071 291.0
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.072 64.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.072 224.9
GaAs (mp-2534) <1 1 1> <1 0 1> 0.073 170.7
Ni (mp-23) <1 1 1> <1 1 0> 0.073 167.8
TbScO3 (mp-31119) <1 0 1> <1 1 0> 0.073 55.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.074 224.9
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.074 279.6
BN (mp-984) <1 0 0> <0 0 1> 0.074 96.4
DyScO3 (mp-31120) <1 0 1> <1 1 0> 0.076 55.9
C (mp-66) <1 1 0> <1 0 1> 0.077 213.4
LaAlO3 (mp-2920) <1 0 1> <1 0 1> 0.077 298.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
73 16 33 0 0 0
16 73 33 0 0 0
33 33 51 0 0 0
0 0 0 14 0 0
0 0 0 0 14 0
0 0 0 0 0 11
Compliance Tensor Sij (10-12Pa-1)
19.7 2.1 -14.1 0 0 0
2.1 19.7 -14.1 0 0 0
-14.1 -14.1 37.9 0 0 0
0 0 0 70.7 0 0
0 0 0 0 70.7 0
0 0 0 0 0 94.7
Shear Modulus GV
15 GPa
Bulk Modulus KV
40 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
40 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
40 GPa
Elastic Anisotropy
0.76
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TlCu4S3 (mp-8159) 0.1680 0.001 3
RbCu4S3 (mp-1025519) 0.2483 0.000 3
CsCd4As3 (mp-1079080) 0.1531 0.000 3
KCu4S3 (mp-27677) 0.2573 0.000 3
RbZn4As3 (mp-975144) 0.2006 0.000 3
TmBi2ClO4 (mp-546082) 0.4539 0.000 4
HoBi2ClO4 (mp-549127) 0.4623 0.000 4
ErBi2ClO4 (mp-549709) 0.4614 0.000 4
EuBi2ClO4 (mp-550566) 0.4653 0.000 4
LuBi2ClO4 (mp-550805) 0.4550 0.000 4
YCu2Bi2(SeO2)2 (mp-550306) 0.5730 0.000 5
YFe2Bi2(SeO2)2 (mp-1022730) 0.5623 0.180 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv Cu_pv Se
Final Energy/Atom
-3.8591 eV
Corrected Energy
-32.2889 eV
Uncorrected energy = -30.8729 eV Composition-based energy adjustment (-0.472 eV/atom x 3.0 atoms) = -1.4160 eV Corrected energy = -32.2889 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 628205
  • 280072
Submitted by
User remarks:
  • Potassium copper selenide (1/4/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)