Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.045 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHf |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6/mmm [191] |
Hall-P 6 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 65.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 86.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 21.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 77.2 |
BN (mp-984) | <1 0 1> | <1 0 1> | 79.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.0 |
BN (mp-984) | <1 1 1> | <1 1 0> | 133.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.1 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 275.5 |
Al (mp-134) | <1 0 0> | <1 0 1> | 133.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 169.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 86.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 108.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 159.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 43.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 240.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 319.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 195.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 281.9 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 347.8 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 239.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 262.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 214.1 |
TeO2 (mp-2125) | <1 1 1> | <1 1 1> | 103.3 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 133.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 46.3 |
SiC (mp-7631) | <1 0 1> | <1 1 0> | 187.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 213.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 292.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 216.8 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 107.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 92.7 |
MgO (mp-1265) | <1 1 0> | <1 1 1> | 103.3 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 160.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 278.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 139.0 |
TiO2 (mp-2657) | <1 0 1> | <1 1 1> | 275.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 173.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 195.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 231.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 1> | 159.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 195.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 154.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 319.5 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 169.9 |
C (mp-48) | <0 0 1> | <1 0 0> | 108.1 |
C (mp-48) | <1 0 0> | <1 0 0> | 77.2 |
C (mp-48) | <1 0 1> | <1 0 1> | 79.9 |
C (mp-48) | <1 1 0> | <1 1 0> | 133.8 |
C (mp-48) | <1 1 1> | <1 1 0> | 133.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrCoGe (mp-10394) | 0.0635 | 0.065 | 3 |
CoNiSn (mp-20237) | 0.0517 | 0.161 | 3 |
FeCoGe (mp-1025047) | 0.0235 | 0.050 | 3 |
FeNiGe (mp-1024972) | 0.0602 | 0.154 | 3 |
UGaCu (mp-1077802) | 0.0825 | 0.080 | 3 |
AlFe2 (mp-985579) | 0.0043 | 0.100 | 2 |
GaNi2 (mp-570904) | 0.0447 | 0.020 | 2 |
UAu2 (mp-12072) | 0.0100 | 0.000 | 2 |
Mg2Sn (mp-1018795) | 0.0367 | 0.083 | 2 |
UAu2 (mp-569022) | 0.0064 | 0.000 | 2 |
Ti (mp-72) | 0.0114 | 0.000 | 1 |
Li (mp-1063005) | 0.2980 | 0.019 | 1 |
Hg (mp-10861) | 0.2723 | 0.003 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv |
Final Energy/Atom-9.9120 eV |
Corrected Energy-29.7361 eV
-29.7361 eV = -29.7361 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)