Final Magnetic Moment1.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.870 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.193 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrO2 |
Band Gap0.269 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 118.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 113.7 |
GaSe (mp-1943) | <1 1 1> | <1 1 1> | 118.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 113.7 |
BN (mp-984) | <1 0 0> | <1 1 0> | 353.7 |
BN (mp-984) | <1 0 1> | <1 1 0> | 353.7 |
C (mp-48) | <0 0 1> | <1 0 0> | 181.9 |
C (mp-48) | <1 0 0> | <1 1 0> | 321.5 |
C (mp-48) | <1 0 1> | <1 1 0> | 160.8 |
BN (mp-984) | <1 1 0> | <1 1 1> | 275.7 |
BN (mp-984) | <1 1 1> | <1 1 0> | 353.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 295.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 181.9 |
Al (mp-134) | <1 0 0> | <1 1 1> | 196.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 96.5 |
Al (mp-134) | <1 1 1> | <1 1 1> | 118.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 257.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 289.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 321.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 1> | 315.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 128.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 128.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 128.6 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 128.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 341.0 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 275.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 353.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 113.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 113.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.6 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 157.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 196.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 96.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 45.5 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 64.3 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 227.4 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 196.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 289.4 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 295.6 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 157.5 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 257.2 |
SiC (mp-7631) | <1 1 1> | <1 1 0> | 257.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 157.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 289.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 204.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 353.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 275.7 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 157.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 257.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 289.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrBeCd (mp-631509) | 0.0000 | 0.945 | 3 |
KTaPt (mp-631314) | 0.0000 | 1.530 | 3 |
CrFeTe (mp-1009592) | 0.0000 | 0.246 | 3 |
LiCdAs (mp-1018135) | 0.0000 | 0.000 | 3 |
GdBiPd (mp-1076916) | 0.0000 | 0.000 | 3 |
Be2Si (mp-1009829) | 0.0000 | 0.235 | 2 |
Mn2Ge (mp-1008920) | 0.0000 | 0.245 | 2 |
MgH2 (mp-1008901) | 0.0000 | 0.109 | 2 |
Ca2Ge (mp-1009755) | 0.0000 | 0.016 | 2 |
Ti2Ga (mp-1008726) | 0.0000 | 0.827 | 2 |
Explore more synthesis descriptions for materials of composition CrO2.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv O |
Final Energy/Atom-7.2469 eV |
Corrected Energy-25.1584 eV
-25.1584 eV = -21.7408 eV (uncorrected energy) - 2.0130 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)