Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.356 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.117 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPrN |
Band Gap1.777 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <1 1 0> | 175.4 |
C (mp-48) | <1 1 1> | <1 1 0> | 306.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 155.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 350.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 219.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 217.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 341.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 31.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 43.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 53.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 279.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 175.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 214.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 248.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 175.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 131.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 310.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 155.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 217.0 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 214.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 175.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 279.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 279.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 155.0 |
BN (mp-984) | <0 0 1> | <1 1 1> | 214.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 93.0 |
BN (mp-984) | <1 1 0> | <1 1 0> | 175.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 248.0 |
Al (mp-134) | <1 0 0> | <1 1 1> | 161.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 155.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 131.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 131.5 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 310.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 161.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 155.0 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 131.5 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 306.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 248.0 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 306.9 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 87.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 306.9 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 306.9 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 263.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 131.5 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 43.8 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 310.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 161.1 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 131.5 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 43.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 217.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
111 | 84 | 84 | 0 | 0 | 0 |
84 | 111 | 84 | 0 | 0 | 0 |
84 | 84 | 111 | 0 | 0 | 0 |
0 | 0 | 0 | 36 | 0 | 0 |
0 | 0 | 0 | 0 | 36 | 0 |
0 | 0 | 0 | 0 | 0 | 36 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
26 | -11.2 | -11.2 | 0 | 0 | 0 |
-11.2 | 26 | -11.2 | 0 | 0 | 0 |
-11.2 | -11.2 | 26 | 0 | 0 | 0 |
0 | 0 | 0 | 27.5 | 0 | 0 |
0 | 0 | 0 | 0 | 27.5 | 0 |
0 | 0 | 0 | 0 | 0 | 27.5 |
Shear Modulus GV27 GPa |
Bulk Modulus KV93 GPa |
Shear Modulus GR22 GPa |
Bulk Modulus KR93 GPa |
Shear Modulus GVRH24 GPa |
Bulk Modulus KVRH93 GPa |
Elastic Anisotropy1.29 |
Poisson's Ratio0.38 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.16946 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.16946 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.16946 |
Piezoelectric Modulus ‖eij‖max0.16946 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.09 | 0.00 | 0.00 |
0.00 | 8.09 | 0.00 |
0.00 | 0.00 | 8.09 |
Dielectric Tensor εij (total) |
||
---|---|---|
14.95 | 0.00 | 0.00 |
0.00 | 14.95 | 0.00 |
0.00 | 0.00 | 14.95 |
Polycrystalline dielectric constant
εpoly∞
8.09
|
Polycrystalline dielectric constant
εpoly
14.95
|
Refractive Index n2.85 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn3CrS4 (mp-1080726) | 0.0175 | 0.324 | 3 |
Zn3CrSe4 (mp-1095028) | 0.0124 | 0.123 | 3 |
Zn3CrTe4 (mp-1087545) | 0.0105 | 0.115 | 3 |
CdSnSb2 (mp-10063) | 0.0250 | 0.000 | 3 |
GaCuS2 (mp-5238) | 0.0192 | 0.000 | 3 |
FeCu2GeS4 (mp-917359) | 0.0383 | 0.185 | 4 |
CoCu2GeS4 (mp-6498) | 0.0382 | 0.055 | 4 |
CoCu2GeS4 (mp-560428) | 0.0476 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.0260 | 0.185 | 4 |
FeCu2GeSe4 (mp-1087471) | 0.0871 | 0.035 | 4 |
HfN (mp-1001916) | 0.0000 | 0.271 | 2 |
WN (mp-1001828) | 0.0000 | 0.558 | 2 |
BiB (mp-1006880) | 0.0000 | 0.824 | 2 |
RbTe (mp-1009491) | 0.0000 | 0.600 | 2 |
ReN (mp-1002209) | 0.0000 | 0.450 | 2 |
O2 (mp-1057818) | 0.0000 | 1.882 | 1 |
Si (mp-149) | 0.0000 | 0.000 | 1 |
Sn (mp-117) | 0.0000 | 0.000 | 1 |
C (mp-66) | 0.0000 | 0.136 | 1 |
Se (mp-12771) | 0.0000 | 0.514 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 N |
Final Energy/Atom-7.7231 eV |
Corrected Energy-15.4463 eV
-15.4463 eV = -15.4463 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)