Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.241 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.266 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density16.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRe2C + C |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 295.8 |
GaTe (mp-542812) | <0 0 1> | <1 0 1> | 217.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 50.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 223.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 93.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 93.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 137.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 93.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.6 |
C (mp-48) | <1 0 1> | <1 1 1> | 79.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 203.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 194.8 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 111.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 21.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 194.8 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 113.0 |
SiC (mp-7631) | <1 1 1> | <1 0 1> | 163.3 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 301.7 |
CaCO3 (mp-3953) | <1 1 1> | <0 0 1> | 151.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 113.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 106.0 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 137.1 |
CaCO3 (mp-3953) | <1 0 1> | <0 0 1> | 267.0 |
ZrO2 (mp-2858) | <1 1 1> | <1 0 1> | 206.9 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 138.6 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 285.4 |
GaTe (mp-542812) | <1 1 0> | <1 0 1> | 196.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 106.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 155.3 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 228.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 269.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 228.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 70.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 32.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 151.5 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 108.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 21.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 122.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 187.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 180.4 |
Al (mp-134) | <1 0 0> | <1 1 0> | 113.0 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 163.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 187.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 223.7 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 1> | 250.4 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 138.6 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 211.8 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 203.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 220.1 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 163.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
749 | 230 | 193 | 0 | 0 | 0 |
230 | 749 | 193 | 0 | 0 | 0 |
193 | 193 | 993 | 0 | 0 | 0 |
0 | 0 | 0 | 167 | 0 | 0 |
0 | 0 | 0 | 0 | 167 | 0 |
0 | 0 | 0 | 0 | 0 | 260 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
1.5 | -0.4 | -0.2 | 0 | 0 | 0 |
-0.4 | 1.5 | -0.2 | 0 | 0 | 0 |
-0.2 | -0.2 | 1.1 | 0 | 0 | 0 |
0 | 0 | 0 | 6 | 0 | 0 |
0 | 0 | 0 | 0 | 6 | 0 |
0 | 0 | 0 | 0 | 0 | 3.9 |
Shear Modulus GV244 GPa |
Bulk Modulus KV413 GPa |
Shear Modulus GR223 GPa |
Bulk Modulus KR409 GPa |
Shear Modulus GVRH234 GPa |
Bulk Modulus KVRH411 GPa |
Elastic Anisotropy0.48 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RhN (mp-1009732) | 0.0142 | 0.890 | 2 |
TaN (mp-1459) | 0.0116 | 0.027 | 2 |
NbN (mp-2634) | 0.0127 | 0.000 | 2 |
TiS (mp-1018028) | 0.0150 | 0.000 | 2 |
WC (mp-1894) | 0.0140 | 0.000 | 2 |
LiNbS2 (mp-7936) | 0.5597 | 0.000 | 3 |
FeWN2 (mp-29076) | 0.5075 | 0.000 | 3 |
Ca3SiBr2 (mp-567974) | 0.5868 | 0.254 | 3 |
LiNbSe2 (mp-1025496) | 0.5276 | 0.000 | 3 |
NaNbS2 (mp-7937) | 0.6170 | 0.000 | 3 |
Xe (mp-979286) | 0.7347 | 0.006 | 1 |
Na (mp-999501) | 0.7292 | 0.129 | 1 |
Li (mp-604313) | 0.4741 | 0.282 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points105 |
U Values-- |
PseudopotentialsVASP PAW: Re_pv C |
Final Energy/Atom-10.5935 eV |
Corrected Energy-21.1871 eV
-21.1871 eV = -21.1871 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)