Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.413 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSc6Sn5 + ScSn2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 313.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 253.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 179.1 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 189.9 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 232.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 77.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 126.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 316.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 253.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 126.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 189.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 232.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 253.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 316.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 189.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 268.6 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 316.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 1 1> | 310.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 44.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 63.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 223.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 253.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 189.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 232.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 189.9 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 316.5 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 77.5 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 77.5 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 189.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 223.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 310.2 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 316.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 253.2 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 189.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 189.9 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 268.6 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 223.8 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 223.8 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 1> | 155.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 1 1> | 155.1 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 223.8 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 189.9 |
Si (mp-149) | <1 1 1> | <1 1 0> | 253.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 89.5 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 223.8 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 189.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 189.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 253.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 310.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 44.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
4 | 67 | 67 | 0 | 0 | 0 |
67 | 4 | 67 | 0 | 0 | 0 |
67 | 67 | 4 | 0 | 0 | 0 |
0 | 0 | 0 | -29 | 0 | 0 |
0 | 0 | 0 | 0 | -29 | 0 |
0 | 0 | 0 | 0 | 0 | -29 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-8.3 | 7.8 | 7.8 | 0 | 0 | 0 |
7.8 | -8.3 | 7.8 | 0 | 0 | 0 |
7.8 | 7.8 | -8.3 | 0 | 0 | 0 |
0 | 0 | 0 | -35 | 0 | 0 |
0 | 0 | 0 | 0 | -35 | 0 |
0 | 0 | 0 | 0 | 0 | -35 |
Shear Modulus GV-30 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR-30 GPa |
Bulk Modulus KR46 GPa |
Shear Modulus GVRH-30 GPa |
Bulk Modulus KVRH46 GPa |
Elastic Anisotropy0.01 |
Poisson's Ratio0.91 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn3CrS4 (mp-1080726) | 0.0175 | 0.129 | 3 |
Zn3CrSe4 (mp-1095028) | 0.0124 | 0.287 | 3 |
Zn3CrTe4 (mp-1087545) | 0.0105 | 0.114 | 3 |
CdSnSb2 (mp-10063) | 0.0250 | 0.000 | 3 |
GaCuS2 (mp-5238) | 0.0192 | 0.000 | 3 |
FeCu2GeS4 (mp-917359) | 0.0383 | 0.185 | 4 |
CoCu2GeS4 (mp-6498) | 0.0382 | 0.055 | 4 |
CoCu2GeS4 (mp-560428) | 0.0476 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.0260 | 0.185 | 4 |
FeCu2GeSe4 (mp-1087471) | 0.0871 | 0.036 | 4 |
TcB (mp-1002184) | 0.0000 | 1.106 | 2 |
RhC (mp-1009696) | 0.0000 | 0.560 | 2 |
IrC (mp-1001789) | 0.0000 | 0.531 | 2 |
ZnN (mp-999485) | 0.0000 | 0.460 | 2 |
PtC (mp-1018164) | 0.0000 | 0.910 | 2 |
O2 (mp-1057818) | 0.0000 | 1.881 | 1 |
Si (mp-149) | 0.0000 | 0.000 | 1 |
Sn (mp-117) | 0.0000 | 0.000 | 1 |
C (mp-66) | 0.0000 | 0.136 | 1 |
Se (mp-12771) | 0.0000 | 0.514 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv Sn_d |
Final Energy/Atom-4.7583 eV |
Corrected Energy-9.5165 eV
-9.5165 eV = -9.5165 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)