material

Ir

ID:

mp-101

DOI:

10.17188/1186086


Tags: Iridium

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
21.93 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 53813 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaF3 (mp-905) <0 0 1> <1 1 1> 0.003 182.1
Ni (mp-23) <1 1 0> <1 1 0> 0.003 191.2
BN (mp-984) <0 0 1> <1 1 1> 0.008 104.1
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.008 297.4
Si (mp-149) <1 0 0> <1 0 0> 0.037 30.0
Si (mp-149) <1 1 0> <1 1 0> 0.039 42.5
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.045 30.0
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.048 42.5
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.048 315.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.063 233.7
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.065 255.4
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.067 191.2
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.080 225.3
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.086 318.6
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.090 285.4
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.096 42.5
SiC (mp-7631) <1 0 1> <1 0 0> 0.105 240.3
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.133 63.7
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.145 182.1
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.146 127.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.156 30.0
GaP (mp-2490) <1 1 0> <1 1 0> 0.163 42.5
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.164 165.2
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.188 225.3
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.190 255.4
WS2 (mp-224) <1 1 0> <1 1 0> 0.196 233.7
Te2W (mp-22693) <0 0 1> <1 0 0> 0.216 330.5
WS2 (mp-224) <1 0 1> <1 1 0> 0.220 276.2
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.226 63.7
DyScO3 (mp-31120) <1 1 1> <1 0 0> 0.236 285.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.251 135.2
Mg (mp-153) <1 0 0> <1 1 0> 0.256 148.7
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.258 150.2
MoS2 (mp-1434) <1 1 1> <1 1 0> 0.277 233.7
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.280 135.2
Mg (mp-153) <0 0 1> <1 1 1> 0.291 26.0
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.294 191.2
InP (mp-20351) <1 1 1> <1 1 1> 0.298 182.1
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.300 30.0
WS2 (mp-224) <1 1 1> <1 1 1> 0.301 78.1
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.315 42.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.324 135.2
MgO (mp-1265) <1 1 0> <1 1 0> 0.333 233.7
LiF (mp-1138) <1 1 0> <1 1 0> 0.340 191.2
BN (mp-984) <1 1 0> <1 1 0> 0.345 169.9
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.356 254.9
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.380 225.3
Te2W (mp-22693) <0 1 0> <1 0 0> 0.402 270.4
BaF2 (mp-1029) <1 1 0> <1 1 0> 0.403 169.9
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.443 52.0
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
2.53 J/m2 (0.16 eV/Å2)
Weighted work function Φ
5.31 eV
Shape factor η
5.12
Surface energy anisotropy αγ
0.066
Miller Indices
(hkl)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(111) 2.36, 0.15 5.42 0.36
(332) 2.50, 0.16 5.22 0.19
(322) 2.56, 0.16 5.24 0.16
(221) 2.59, 0.16 5.18 0.10
(331) 2.71, 0.17 4.87 0.00
(211) 2.71, 0.17 5.21 0.05
(110) * 2.77, 0.17 5.01 0.00
(110) 2.83, 0.18 4.77 0.00
(311) 2.85, 0.18 5.14 0.06
(321) 2.86, 0.18 5.00 0.00
(100) 2.88, 0.18 5.54 0.08
(320) 2.95, 0.18 4.75 0.00
(310) 3.02, 0.19 5.04 0.00
(210) 3.04, 0.19 4.94 0.00

* indicates reconstructed surface.

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
3 twist [111] 60.00 (111) 0.35 4.22
3 tilt [110] 109.47 (112) 1.62 3.80
3 tilt [111] 180.00 (110) 1.86 3.69
5 twist [100] 36.87 (100) 1.30 4.34
5 tilt [100] 53.13 (013) 1.73 4.31
5 tilt [100] 36.87 (021) 2.19 3.89
7 twist [111] 38.21 (111) 0.86 3.71
7 tilt [111] 38.21 (321) 1.87 3.85
9 tilt [110] 38.94 (221) 1.58 3.59
9 twist [110] 38.94 (110) 2.25 3.30

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
576 231 231 0 0 0
231 576 231 0 0 0
231 231 576 0 0 0
0 0 0 252 0 0
0 0 0 0 252 0
0 0 0 0 0 252
Compliance Tensor Sij (10-12Pa-1)
2.3 -0.6 -0.6 0 0 0
-0.6 2.3 -0.6 0 0 0
-0.6 -0.6 2.3 0 0 0
0 0 0 4 0 0
0 0 0 0 4 0
0 0 0 0 0 4
Shear Modulus GV
220 GPa
Bulk Modulus KV
346 GPa
Shear Modulus GR
213 GPa
Bulk Modulus KR
346 GPa
Shear Modulus GVRH
217 GPa
Bulk Modulus KVRH
346 GPa
Elastic Anisotropy
0.17
Poisson's Ratio
0.24

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -8.853 14.582 19.043 8.183
pack_evans_james -8.853 14.583 2.106 4.063
vinet -8.856 14.567 19.520 6.271
tait -8.854 14.570 2.131 6.238
birch_euler -8.854 14.576 2.399 1.108
pourier_tarantola -8.862 14.559 0.376 3.153
birch_lagrange -8.882 14.569 1.424 6.661
murnaghan -8.849 14.603 2.050 3.883
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1125 0.005 3
CrCoPt2 (mp-570863) 0.0492 0.034 3
LiCa6Ge (mp-12609) 0.0000 0.183 3
GaFeNi2 (mp-1065359) 0.0412 0.065 3
GaCo2Ni (mp-1018060) 0.0157 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2155 0.028 4
CrFeCoNi (mp-1012640) 0.3608 0.065 4
CrFeCoNi (mp-1096923) 0.4019 0.193 4
CuPt7 (mp-12608) 0.0000 0.000 2
SbPt7 (mp-1030) 0.0000 0.034 2
Tm3P (mp-971958) 0.0000 0.489 2
LiPt7 (mp-30765) 0.0000 0.000 2
Ca7Ge (mp-10008) 0.0000 0.224 2
Ru (mp-8639) 0.0000 0.107 1
Cr (mp-8633) 0.0000 0.403 1
Pt (mp-126) 0.0000 0.000 1
Os (mp-8643) 0.0000 0.133 1
Co (mp-102) 0.0000 0.016 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ir
Final Energy/Atom
-8.8384 eV
Corrected Energy
-8.8384 eV
Uncorrected energy = -8.8384 eV Corrected energy = -8.8384 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 64992
  • 659854
  • 53813
  • 640730
  • 640729
  • 41524
  • 426948
Submitted by
User remarks:
  • Iridium

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)