Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.050 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.476 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToDyAs |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 64.0 |
C (mp-48) | <1 0 0> | <1 1 1> | 155.1 |
C (mp-48) | <1 0 1> | <1 1 0> | 162.8 |
C (mp-48) | <1 1 0> | <1 1 0> | 199.0 |
C (mp-48) | <1 1 1> | <1 1 0> | 271.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 288.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 166.3 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 108.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 191.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 54.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 115.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 115.1 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 162.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 155.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 64.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 144.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 289.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 166.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 54.3 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 66.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 22.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 54.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 243.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 191.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 155.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 166.3 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 288.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 281.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 127.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 230.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 319.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 64.0 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 271.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.3 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 66.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 64.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 144.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 289.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 64.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 72.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 88.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 319.8 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 144.7 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 307.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 89.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 54.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 179.1 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 108.5 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 1> | 88.6 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 1> | 288.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
DyYHg2 (mp-971799) | 0.0000 | 0.007 | 3 |
Si2HgTe (mp-631331) | 0.0000 | 0.720 | 3 |
NpSnRh2 (mp-864834) | 0.0000 | 0.127 | 3 |
TmCdPd2 (mp-865982) | 0.0000 | 0.000 | 3 |
ErSnRu2 (mp-866285) | 0.0000 | 0.000 | 3 |
TiFeCoAs (mp-998974) | 0.0000 | 0.134 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnGaFeCo (mp-999552) | 0.0000 | 0.044 | 4 |
CeHg (mp-702) | 0.0000 | 0.000 | 2 |
TmCu (mp-985) | 0.0000 | 0.000 | 2 |
SrCd (mp-30496) | 0.0000 | 0.000 | 2 |
HfIr (mp-1002122) | 0.0000 | 0.042 | 2 |
CeZn (mp-986) | 0.0000 | 0.028 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 As |
Final Energy/Atom-5.6828 eV |
Corrected Energy-11.3656 eV
-11.3656 eV = -11.3656 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)