Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.173 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.091 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa4Ge9O20 + Na2GeO3 + NaV(GeO3)2 + NaVO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3d [230] |
Hall-I 4bd 2c 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 151.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 151.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 151.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 151.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 151.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 151.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 151.6 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 151.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 151.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 151.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 151.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 151.6 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 151.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb3Al5O12 (mp-3800) | 0.1771 | 0.036 | 3 |
Eu3Al5O12 (mp-21757) | 0.1331 | 0.000 | 3 |
La3Al5O12 (mp-780432) | 0.0467 | 0.033 | 3 |
Gd3Al5O12 (mp-14133) | 0.1834 | 0.000 | 3 |
Sm3Al5O12 (mp-780370) | 0.1696 | 0.000 | 3 |
Na3Fe2(GeO4)3 (mp-1013864) | 0.1049 | 0.089 | 4 |
Na3Ti2(GeO4)3 (mp-1012670) | 0.0606 | 0.043 | 4 |
Na3Ni2(GeO4)3 (mp-1013808) | 0.1171 | 0.308 | 4 |
Na3Ge3(MoO6)2 (mp-1013797) | 0.1435 | 0.038 | 4 |
Na3Co2(GeO4)3 (mp-1013794) | 0.1311 | 0.151 | 4 |
Ca10V5Fe15(BiO24)2 (mp-697835) | 0.2792 | 0.084 | 5 |
Na2CaSn2(GeO4)3 (mp-677095) | 0.2716 | 0.000 | 5 |
Li6Nd6Sb(TeO8)3 (mp-532789) | 0.2537 | 0.009 | 5 |
Na2CaTi2(GeO4)3 (mp-695511) | 0.1430 | 0.007 | 5 |
Ca2VFe4BiO12 (mp-705898) | 0.3014 | 0.090 | 5 |
Ca11YAl15Cr4SiO48 (mp-743917) | 0.3267 | 0.116 | 6 |
Ca3Y9Al18CrSiO48 (mp-744910) | 0.3266 | 0.021 | 6 |
NaYbTiNbO6F (mp-684861) | 0.6916 | 0.065 | 6 |
Ca4Y2Al7Cr2SiO24 (mp-743704) | 0.3686 | 0.104 | 6 |
NaEuTiNbO6F (mp-43048) | 0.6693 | 0.021 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv Ge_d O |
Final Energy/Atom-6.3496 eV |
Corrected Energy-554.5420 eV
Uncorrected energy = -507.9660 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.700 eV/atom x 8.0 atoms) = -13.6000 eV
Corrected energy = -554.5420 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)