Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.431 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.511 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3N2 |
Band Gap0.500 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 105.9 |
MoS2 (mp-1434) | <1 0 0> | <1 1 0> | 269.5 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 275.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 84.7 |
Al (mp-134) | <1 1 0> | <1 1 0> | 89.8 |
Al (mp-134) | <1 1 1> | <1 1 1> | 110.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 239.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 169.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 179.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 146.7 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 42.3 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 59.9 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 256.7 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 269.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 317.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 269.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 317.6 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 110.0 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 329.3 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 239.5 |
SiC (mp-7631) | <1 1 1> | <1 1 0> | 239.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 119.8 |
LiTaO3 (mp-3666) | <1 0 1> | <1 1 0> | 239.5 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 127.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 275.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 169.4 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 239.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 21.2 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 119.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 127.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 169.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 148.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 105.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 239.5 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 269.5 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 105.9 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 179.6 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 209.6 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 275.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 317.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 317.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 190.5 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 329.3 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 256.7 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 146.7 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 190.5 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 256.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 105.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 209.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
180 | 21 | 21 | 0 | 0 | 0 |
21 | 180 | 21 | 0 | 0 | 0 |
21 | 21 | 180 | 0 | 0 | 0 |
0 | 0 | 0 | 43 | 0 | 0 |
0 | 0 | 0 | 0 | 43 | 0 |
0 | 0 | 0 | 0 | 0 | 43 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.7 | -0.6 | -0.6 | 0 | 0 | 0 |
-0.6 | 5.7 | -0.6 | 0 | 0 | 0 |
-0.6 | -0.6 | 5.7 | 0 | 0 | 0 |
0 | 0 | 0 | 23.4 | 0 | 0 |
0 | 0 | 0 | 0 | 23.4 | 0 |
0 | 0 | 0 | 0 | 0 | 23.4 |
Shear Modulus GV57 GPa |
Bulk Modulus KV74 GPa |
Shear Modulus GR52 GPa |
Bulk Modulus KR74 GPa |
Shear Modulus GVRH55 GPa |
Bulk Modulus KVRH74 GPa |
Elastic Anisotropy0.47 |
Poisson's Ratio0.20 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3AsN (mp-1013709) | 0.0000 | 1.117 | 3 |
CsEuF3 (mp-8396) | 0.0000 | 0.000 | 3 |
RbCaF3 (mp-3654) | 0.0000 | 0.000 | 3 |
Sr3BiP (mp-1013530) | 0.0000 | 0.809 | 3 |
Ce3InC (mp-1069526) | 0.0000 | 2.105 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.945 | 4 |
Ca3Sb2 (mp-1013546) | 0.0000 | 0.421 | 2 |
Ca3Bi2 (mp-1013735) | 0.0000 | 0.363 | 2 |
Ba3N2 (mp-1013528) | 0.0000 | 0.683 | 2 |
Ba3P2 (mp-1013551) | 0.0000 | 0.446 | 2 |
Sr3Bi2 (mp-1013587) | 0.0000 | 0.371 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.249 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv N |
Final Energy/Atom-4.8158 eV |
Corrected Energy-24.0789 eV
-24.0789 eV = -24.0789 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)