Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.158 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.333 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3AsN |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 124.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 146.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 87.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 263.6 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 248.5 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 82.8 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 289.9 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 202.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 289.9 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 124.2 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 87.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 263.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 263.6 |
C (mp-48) | <0 0 1> | <1 0 0> | 263.6 |
C (mp-48) | <1 0 0> | <1 1 0> | 207.1 |
C (mp-48) | <1 0 1> | <1 0 0> | 322.1 |
C (mp-48) | <1 1 0> | <1 1 0> | 165.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 205.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 146.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 124.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 205.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 175.7 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 304.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 82.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 289.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 29.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 41.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 50.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 263.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 124.2 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 87.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 263.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 263.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 165.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 202.9 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 234.3 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 124.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 41.4 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 205.0 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 292.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 152.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 82.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 331.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 234.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 165.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 165.7 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 202.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 58.6 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 205.0 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 146.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Sr2GaSbO6 (mp-6065) | 0.0003 | 0.039 | 4 |
YbBa2SbO6 (mp-14223) | 0.0000 | 1.748 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.084 | 4 |
Cs2LiYCl6 (mp-567652) | 0.0001 | 0.000 | 4 |
Ni4N (mp-20839) | 0.0000 | 2.016 | 2 |
Ca3N2 (mp-1013524) | 0.0000 | 0.511 | 2 |
Sr3As2 (mp-1013559) | 0.0000 | 0.370 | 2 |
Ca3Bi2 (mp-1013735) | 0.0000 | 0.366 | 2 |
Ca3P2 (mp-1013547) | 0.0000 | 0.143 | 2 |
Mn3RhN (mp-582028) | 0.0000 | 0.091 | 3 |
Ba3BiP (mp-1013691) | 0.0000 | 0.104 | 3 |
PrGaO3 (mp-9833) | 0.0000 | 1.455 | 3 |
Li3ClO (mp-985585) | 0.0000 | 0.022 | 3 |
BaTiO3 (mp-2998) | 0.0000 | 0.014 | 3 |
SrLaNbZnO6 (mp-41918) | 0.0385 | 0.126 | 5 |
BaLaMgBiO6 (mp-41414) | 0.0288 | 0.069 | 5 |
BaCaLaBiO6 (mp-39886) | 0.0711 | 0.125 | 5 |
BaLaTaZnO6 (mp-42054) | 0.0630 | 0.112 | 5 |
BaLaMgTaO6 (mp-40251) | 0.0443 | 0.079 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.6831 | 0.059 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv As N |
Final Energy/Atom-3.5636 eV |
Corrected Energy-17.8178 eV
-17.8178 eV = -17.8178 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)