Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.478 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaCoPO4 + NaPO3 |
Band Gap2.380 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group1 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 1 1> | <1 0 0> | 240.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 336.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 240.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 288.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 192.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 232.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 232.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 261.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 141.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 240.6 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 -1> | 239.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 192.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 336.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 192.5 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 261.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 192.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 222.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 336.8 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 240.6 |
Al (mp-134) | <1 1 1> | <0 1 1> | 141.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 111.0 |
C (mp-48) | <1 0 1> | <1 1 1> | 160.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 48.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 141.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 336.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 144.4 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 240.6 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 318.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 318.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 240.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 336.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 96.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 48.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 116.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 192.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 261.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 48.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 116.1 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 48.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 288.7 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 336.8 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 240.6 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 87.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.7 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 192.5 |
GaSe (mp-1943) | <1 1 0> | <1 0 -1> | 239.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 261.7 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 240.6 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 192.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
P2Pd2O7 (mp-554320) | 0.6814 | 0.013 | 3 |
Na2P2PdO7 (mp-8989) | 0.2110 | 0.000 | 4 |
Na2CuP2O7 (mp-6467) | 0.0925 | 0.000 | 4 |
Na2CuP2O7 (mp-760251) | 0.5307 | 0.033 | 4 |
NaCuP2O7 (mp-755492) | 0.3975 | 0.000 | 4 |
Li2MnP2O7 (mp-761564) | 0.4815 | 0.079 | 4 |
NaCa3Fe4(SiO3)8 (mp-705483) | 0.7313 | 0.198 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Na_pv Co P O |
Final Energy/Atom-6.5122 eV |
Corrected Energy-339.7449 eV