Final Magnetic Moment1.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.642 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO5 + VPO4 |
Band Gap1.482 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <1 0 0> | 215.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 246.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 101.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 118.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 215.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 344.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 147.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 98.5 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 236.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 295.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 344.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 344.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 177.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 246.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 139.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 89.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 98.5 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 98.5 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 246.1 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 139.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 246.1 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 266.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 98.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 98.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 98.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 139.5 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 203.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 246.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 177.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 246.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 246.1 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 266.9 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 266.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 98.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 177.9 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 236.5 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 236.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 215.0 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 236.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 196.9 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 246.1 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 147.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 344.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 147.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 344.6 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 98.5 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 246.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMo2P2O9 (mp-1012668) | 0.2393 | 0.088 | 4 |
Ti2ZnP2O9 (mvc-9747) | 0.3438 | 0.152 | 4 |
LiFe2P2O9 (mp-1013910) | 0.1482 | 0.056 | 4 |
LiTi2P2O9 (mp-1013762) | 0.2838 | 0.056 | 4 |
LiCr2P2O9 (mp-1013922) | 0.1150 | 0.174 | 4 |
MgCrNiP2O9 (mvc-8414) | 0.3072 | 0.075 | 5 |
MgFeNiP2O9 (mvc-8280) | 0.5466 | 0.093 | 5 |
ZnNiMoP2O9 (mvc-8300) | 0.3877 | 0.183 | 5 |
MgNiMoP2O9 (mvc-8284) | 0.5115 | 0.061 | 5 |
ZnFeNiP2O9 (mvc-8277) | 0.4227 | 0.272 | 5 |
KNaZrSi3H4O11 (mp-773906) | 0.6467 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.3384 eV |
Corrected Energy-449.6890 eV
-449.6890 eV = -410.9506 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)