Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.000 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaTiPO5 + NaTi2(PO4)3 + TiO2 + P |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 148.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 246.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 296.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 296.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 296.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 317.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 246.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 197.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 229.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 317.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 239.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 200.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 246.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 98.8 |
C (mp-48) | <1 1 1> | <1 0 -1> | 305.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 178.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 220.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 246.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 66.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 238.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 296.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 -1> | 220.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 238.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 98.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 246.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 98.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 345.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 98.8 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 98.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 246.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 178.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 268.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 246.9 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 268.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 345.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 345.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 76.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 -1> | 229.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 229.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 246.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 66.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 317.6 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 207.7 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 133.9 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 133.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 197.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 246.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 66.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 317.6 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 -1> | 220.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni6P7O24 (mp-504372) | 0.6674 | 0.023 | 3 |
CuReO4 (mp-768878) | 0.7448 | 0.023 | 3 |
Fe7(AsO4)6 (mp-542660) | 0.7298 | 0.000 | 3 |
Fe5(PO4)4 (mp-540432) | 0.7470 | 0.010 | 3 |
NaFe3P3O13 (mp-1040459) | 0.2750 | 0.033 | 4 |
SrFe3P3O13 (mp-704109) | 0.3050 | 0.000 | 4 |
MgTi3P3O13 (mvc-10233) | 0.3155 | 0.124 | 4 |
CaTi3P3O13 (mvc-10257) | 0.2858 | 0.078 | 4 |
MgCo3P3O13 (mvc-10586) | 0.3354 | 0.082 | 4 |
LiVP2HO8 (mp-780110) | 0.7155 | 0.047 | 5 |
LiV3Fe2CuO12 (mp-767459) | 0.6768 | 0.017 | 5 |
LiVP2HO8 (mp-777138) | 0.7285 | 0.048 | 5 |
LiVP2HO8 (mp-781014) | 0.7117 | 0.051 | 5 |
Li3V2P4(HO8)2 (mp-781013) | 0.7281 | 0.067 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ti_pv P O |
Final Energy/Atom-7.8224 eV |
Corrected Energy-331.1566 eV
-331.1566 eV = -312.8970 eV (uncorrected energy) - 18.2595 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)