Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.127 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.489 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3As + Na3As |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImmm [71] |
Hall-I 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 141.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 172.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 203.6 |
C (mp-48) | <1 1 0> | <0 1 1> | 193.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 219.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 203.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 109.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 212.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 297.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 141.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 141.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 344.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 328.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 116.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 248.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 313.3 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 154.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 235.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 249.3 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 70.0 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 154.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 181.0 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 31.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 1> | 215.1 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 0> | 279.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 31.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 177.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 328.9 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 94.0 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 94.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 141.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 141.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 297.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 109.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 219.3 |
BN (mp-984) | <1 1 0> | <0 1 1> | 193.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 172.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 271.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 203.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 313.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 375.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 109.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 193.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 281.9 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 297.6 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 297.6 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 116.2 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 318.8 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 154.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 203.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2YAl (mp-1014462) | 0.7206 | 0.299 | 3 |
AlCo2Si (mp-1015811) | 0.5697 | 1.093 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points63 |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Li_sv As |
Final Energy/Atom-2.5740 eV |
Corrected Energy-10.2960 eV
-10.2960 eV = -10.2960 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)