Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.043 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.511 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrN + N2 |
Band Gap0.164 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI212121 [24] |
HallI 2b 2c |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 208.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 229.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 104.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 271.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 334.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 215.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 125.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 237.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 355.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 188.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 237.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 167.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 152.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 355.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 304.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 167.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 334.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 292.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 237.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 334.1 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 237.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 229.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 292.4 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 250.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 271.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 146.2 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 208.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 229.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 107.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 146.2 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 215.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 208.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 125.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 41.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 208.8 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 146.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 229.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 271.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 229.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 188.0 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 355.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 355.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 313.3 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 334.1 |
Al2O3 (mp-1143) | <1 1 0> | <0 1 0> | 219.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 167.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 229.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 355.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 292.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoPO4 (mp-689943) | 0.4799 | 0.223 | 3 |
LiFeF4 (mp-777020) | 0.4326 | 0.095 | 3 |
LiFeF4 (mp-777567) | 0.4493 | 0.090 | 3 |
BAsO4 (mp-3277) | 0.4652 | 0.000 | 3 |
NiPO4 (mp-697731) | 0.4686 | 0.151 | 3 |
Rb2Al2Si3O10 (mp-975622) | 0.6647 | 0.009 | 4 |
RbBe2P3O10 (mp-557673) | 0.6826 | 0.000 | 4 |
K2Ge3(BO5)2 (mp-560019) | 0.6656 | 0.000 | 4 |
KGe2BO6 (mp-556463) | 0.6902 | 0.000 | 4 |
MnS2 (mvc-11047) | 0.3959 | 0.308 | 2 |
BeH2 (mp-768203) | 0.3064 | 0.000 | 2 |
SiO2 (mp-557244) | 0.1808 | 0.177 | 2 |
CO2 (mp-1077316) | 0.3780 | 0.450 | 2 |
CeSe2 (mp-1098703) | 0.0936 | 0.512 | 2 |
RbZnB(PO4)2 (mp-557658) | 0.6166 | 0.000 | 5 |
CsZnB(PO4)2 (mp-560244) | 0.6715 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv N |
Final Energy/Atom-8.4767 eV |
Corrected Energy-101.7202 eV
-101.7202 eV = -101.7202 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)