Final Magnetic Moment-0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.231 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.321 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiAl + LiMg149 + Mg17Al12 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImmm [71] |
Hall-I 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 226.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 347.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 241.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 256.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 166.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 272.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 297.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 182.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 145.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 166.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 145.5 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 297.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 151.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 181.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 226.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 226.7 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 226.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 132.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 62.8 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 151.1 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 277.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 136.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 231.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 256.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 231.5 |
Al (mp-134) | <1 1 1> | <0 1 1> | 145.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 226.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 254.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 218.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 330.8 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 327.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 226.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 211.5 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 211.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 304.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 241.8 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 241.8 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 188.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 75.6 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 241.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 297.7 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 165.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 136.0 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 181.3 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 226.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 226.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 347.5 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 272.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 136.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 218.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LuCd2 (mp-1008910) | 0.6625 | 0.401 | 2 |
TmCd2 (mp-1008673) | 0.6397 | 0.419 | 2 |
HoCd2 (mp-1009080) | 0.6620 | 0.428 | 2 |
CeCd2 (mp-622107) | 0.6487 | 0.435 | 2 |
Ti3Ga (mp-672250) | 0.6429 | 0.529 | 2 |
AlCo2Si (mp-1015811) | 0.6924 | 1.093 | 3 |
LiFeAs (mp-1018785) | 0.6474 | 0.528 | 3 |
Si (mp-34) | 0.7381 | 0.304 | 1 |
Sr (mp-19858) | 0.7391 | 0.222 | 1 |
K (mp-604325) | 0.7146 | 0.064 | 1 |
Rb (mp-639736) | 0.7143 | 0.058 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points63 |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Mg_pv Al |
Final Energy/Atom-1.9796 eV |
Corrected Energy-7.9186 eV
-7.9186 eV = -7.9186 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)