Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.031 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.438 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrN + N2 |
Band Gap0.157 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 79.7 |
C (mp-48) | <1 0 1> | <1 -1 0> | 161.4 |
C (mp-48) | <1 1 1> | <0 1 1> | 277.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 266.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 -1 -1> | 310.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 207.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 169.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 223.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 295.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 279.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 159.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 -1> | 62.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 212.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 215.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 318.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 223.5 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 -1> | 186.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 295.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 266.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 111.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 279.0 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 304.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 236.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 152.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 236.6 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 -1> | 51.5 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 170.0 |
Ni (mp-23) | <1 1 0> | <0 1 -1> | 158.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 119.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 279.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 159.5 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 238.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 225.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 167.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 266.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 279.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 -1> | 198.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 170.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 -1> | 309.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 111.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 266.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 277.9 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 266.6 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 325.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 -1> | 154.5 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 212.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 223.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 212.5 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 169.3 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 236.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.42075 | -1.27733 | -1.10332 | 0.30091 | 0.15277 | -0.14158 |
-0.14552 | -0.44744 | 0.48437 | 0.57830 | -0.01697 | 0.22806 |
1.48031 | 0.78023 | 0.54407 | -0.23594 | 0.06930 | -0.37806 |
Piezoelectric Modulus ‖eij‖max2.34954 C/m2 |
Crystallographic Direction vmax |
---|
-2.00000 |
2.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
28.03 | 0.43 | 3.71 |
0.44 | 23.48 | -10.32 |
3.68 | -10.30 | 25.33 |
Dielectric Tensor εij (total) |
||
---|---|---|
49.79 | 12.15 | 4.04 |
12.15 | 86.43 | -47.22 |
4.02 | -47.21 | 61.93 |
Polycrystalline dielectric constant
εpoly∞
25.61
|
Polycrystalline dielectric constant
εpoly
66.05
|
Refractive Index n5.06 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H4SO5 (mp-626172) | 0.6338 | 0.017 | 3 |
H4SO5 (mp-626483) | 0.5916 | 0.025 | 3 |
H4SO5 (mp-626229) | 0.6394 | 0.029 | 3 |
Si4H2O9 (mp-627632) | 0.5529 | 0.043 | 3 |
Si2H2O5 (mp-626085) | 0.6043 | 0.138 | 3 |
Al2Si2H4O9 (mp-720262) | 0.7270 | 0.726 | 4 |
Al2H18SO15 (mp-720965) | 0.7295 | 0.314 | 4 |
Li2Cr2H4O9 (mp-744929) | 0.6611 | 0.065 | 4 |
BH3OF4 (mp-696379) | 0.6696 | 0.000 | 4 |
PH5NO4 (mp-720874) | 0.6721 | 0.056 | 4 |
Si3O7 (mp-638900) | 0.7292 | 0.951 | 2 |
NaSi2BH2O7 (mp-867930) | 0.5292 | 0.102 | 5 |
LiAlSiH2O5 (mp-604420) | 0.7034 | 0.105 | 5 |
NaAlSi2H2O7 (mp-676991) | 0.6552 | 0.033 | 5 |
RbPH3O4F (mp-761252) | 0.6410 | 0.000 | 5 |
LiAlSi2H2O7 (mp-24104) | 0.7039 | 0.007 | 5 |
Al2P3H17C4(NO6)2 (mp-709723) | 0.6849 | 0.056 | 6 |
PH9C2NO3F (mp-600215) | 0.7213 | 0.153 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv N |
Final Energy/Atom-8.5503 eV |
Corrected Energy-102.6033 eV
-102.6033 eV = -102.6033 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)