Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.673 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.739 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 285.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 268.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 276.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 69.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 285.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 268.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 285.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 285.7 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 268.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 171.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.1 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 242.4 |
GaSe (mp-1943) | <1 0 0> | <1 1 1> | 212.6 |
BN (mp-984) | <1 0 0> | <1 1 1> | 212.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 276.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 171.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 285.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 89.6 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 342.8 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 0> | 242.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 171.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 207.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 276.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 285.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 342.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 276.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 57.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 342.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 285.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 179.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 276.2 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 242.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 242.4 |
GaSe (mp-1943) | <1 1 1> | <1 1 0> | 242.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 285.7 |
BN (mp-984) | <1 1 1> | <1 0 1> | 268.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 228.5 |
Al (mp-134) | <1 1 0> | <1 0 0> | 285.7 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 228.5 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.1 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 285.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 276.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 228.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 268.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 171.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 207.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 276.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.1 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 276.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
73 | 9 | 9 | 0 | 0 | 0 |
9 | 24 | 24 | 0 | 0 | 0 |
9 | 24 | 24 | 0 | 0 | 0 |
0 | 0 | 0 | 12 | 0 | 0 |
0 | 0 | 0 | 0 | 10 | 0 |
0 | 0 | 0 | 0 | 0 | 10 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
14.3 | -2.7 | -2.7 | 0 | 0 | 0 |
-2.7 | -775.7 | 797.5 | 0 | 0 | 0 |
-2.7 | 797.5 | -775.7 | 0 | 0 | 0 |
0 | 0 | 0 | 85 | 0 | 0 |
0 | 0 | 0 | 0 | 96.9 | 0 |
0 | 0 | 0 | 0 | 0 | 96.9 |
Shear Modulus GV12 GPa |
Bulk Modulus KV23 GPa |
Shear Modulus GR-2 GPa |
Bulk Modulus KR21 GPa |
Shear Modulus GVRH5 GPa |
Bulk Modulus KVRH22 GPa |
Elastic Anisotropy-37.94 |
Poisson's Ratio0.40 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.72 | 0.00 | -0.00 |
0.00 | 6.91 | 0.00 |
-0.00 | 0.00 | 6.91 |
Dielectric Tensor εij (total) |
||
---|---|---|
20.71 | 0.00 | -0.00 |
0.00 | 16.42 | 0.00 |
-0.00 | 0.00 | 16.42 |
Polycrystalline dielectric constant
εpoly∞
7.51
|
Polycrystalline dielectric constant
εpoly
17.85
|
Refractive Index n2.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl3In7Se10 (mp-675519) | 0.1094 | 0.034 | 3 |
RbInTe2 (mp-22255) | 0.1208 | 0.000 | 3 |
KInTe2 (mp-19851) | 0.0938 | 0.000 | 3 |
NaGaTe2 (mp-10164) | 0.0413 | 0.006 | 3 |
TlInTe2 (mp-22791) | 0.1157 | 0.000 | 3 |
MnTl2SnTe4 (mp-569859) | 0.1239 | 0.000 | 4 |
Tl2CdSnTe4 (mp-570076) | 0.2373 | 0.009 | 4 |
Rb2SnHgTe4 (mp-1080691) | 0.3307 | 0.000 | 4 |
MnTl2GeTe4 (mp-638590) | 0.2701 | 0.000 | 4 |
Tl2SnHgTe4 (mp-570051) | 0.2674 | 0.012 | 4 |
TlSe (mp-1836) | 0.2588 | 0.000 | 2 |
TlS (mp-322) | 0.3527 | 0.052 | 2 |
InTe (mp-20320) | 0.1731 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Al Te |
Final Energy/Atom-3.5091 eV |
Corrected Energy-29.7609 eV
Uncorrected energy = -28.0729 eV
Composition-based energy adjustment (-0.422 eV/atom x 4.0 atoms) = -1.6880 eV
Corrected energy = -29.7609 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)