Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.682 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbInSe2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 96.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 171.0 |
C (mp-48) | <1 0 1> | <1 0 0> | 211.0 |
C (mp-48) | <1 1 0> | <1 1 0> | 261.1 |
C (mp-48) | <1 1 1> | <1 0 0> | 271.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 150.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 287.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 32.1 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 156.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 128.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 271.3 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 208.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 267.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 287.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 203.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 301.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 351.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 203.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 203.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 331.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 241.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 241.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 211.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 287.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 159.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 351.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 271.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 331.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 319.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 150.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 52.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 203.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 301.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 331.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 208.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 203.0 |
InP (mp-20351) | <1 0 0> | <1 1 1> | 106.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 52.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 90.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 211.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 60.3 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 156.6 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 180.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 309.9 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 156.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 211.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KNbSe2 (mp-7940) | 0.5465 | 0.029 | 3 |
KNbS2 (mp-7938) | 0.5497 | 0.009 | 3 |
LiNb2O (mp-1025455) | 0.5972 | 0.686 | 3 |
InMoS2 (mp-1087488) | 0.5042 | 0.091 | 3 |
NbInS2 (mp-20621) | 0.1564 | 0.016 | 3 |
SrMg (mp-1094286) | 0.5149 | 0.204 | 2 |
Re3N (mp-974435) | 0.2099 | 0.000 | 2 |
Tc3N (mp-1017987) | 0.1649 | 0.000 | 2 |
SrMg2 (mp-1094282) | 0.3631 | 0.275 | 2 |
SrMg2 (mp-1094323) | 0.4540 | 0.272 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv In_d Se |
Final Energy/Atom-5.6429 eV |
Corrected Energy-23.5155 eV
Uncorrected energy = -22.5715 eV
Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV
Corrected energy = -23.5155 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)