Final Magnetic Moment0.271 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.424 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 1 0> | 42.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 156.2 |
C (mp-48) | <1 1 0> | <1 0 0> | 269.0 |
C (mp-48) | <1 1 1> | <1 0 0> | 269.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 149.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 209.2 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 211.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 295.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 288.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 149.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 209.2 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 126.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 156.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 288.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 156.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 295.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 84.5 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 149.4 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 209.2 |
InP (mp-20351) | <1 1 1> | <1 1 0> | 126.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 156.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 300.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 300.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 64.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 108.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 225.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 156.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 168.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 219.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 60.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 298.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 156.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 252.4 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 179.3 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 1> | 289.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 252.4 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 312.5 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 0> | 328.7 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 204.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 156.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 204.3 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 307.6 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 307.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 42.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 192.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 211.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 239.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 209.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 84.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 108.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ScAu2 (mp-1018148) | 0.1204 | 0.000 | 2 |
ZrPd2 (mp-1018102) | 0.1704 | 0.006 | 2 |
ScAg2 (mp-1018128) | 0.1308 | 0.000 | 2 |
Ge2W (mp-542595) | 0.1210 | 0.067 | 2 |
TmAg2 (mp-30359) | 0.1654 | 0.000 | 2 |
LaSb2Au (mp-675224) | 0.6911 | 0.268 | 3 |
Pa (mp-62) | 0.3215 | 0.023 | 1 |
Hg (mp-569289) | 0.6174 | 0.008 | 1 |
Sn (mp-55) | 0.2812 | 0.055 | 1 |
Pr (mp-568938) | 0.5498 | 0.093 | 1 |
Rb (mp-639755) | 0.6535 | 0.005 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points104 |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Au |
Final Energy/Atom-5.2392 eV |
Corrected Energy-15.7177 eV
-15.7177 eV = -15.7177 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)