Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.302 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 0 0> | <1 0 0> | 128.4 |
C (mp-48) | <1 0 1> | <0 0 1> | 166.7 |
C (mp-48) | <1 1 0> | <0 0 1> | 269.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 269.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 77.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 115.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 115.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 346.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 320.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 160.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 243.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 192.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 256.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 160.6 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 289.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 69.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 166.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 179.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 64.1 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 90.8 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 1> | 235.9 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 90.8 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 224.8 |
CdWO4 (mp-19387) | <1 1 0> | <1 1 1> | 283.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 166.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 103.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 289.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 89.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 160.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 115.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 12.8 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 34.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 166.7 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 141.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 136.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 136.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 333.5 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 269.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 64.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 224.8 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 136.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 64.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 38.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 166.7 |
BN (mp-984) | <1 1 0> | <1 1 0> | 136.2 |
BN (mp-984) | <1 1 1> | <1 1 0> | 136.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 136.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 224.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
107 | 78 | 64 | 0 | 0 | 0 |
78 | 107 | 64 | 0 | 0 | 0 |
64 | 64 | 153 | 0 | 0 | 0 |
0 | 0 | 0 | 48 | 0 | 0 |
0 | 0 | 0 | 0 | 48 | 0 |
0 | 0 | 0 | 0 | 0 | 73 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
20.8 | -13.2 | -3.2 | 0 | 0 | 0 |
-13.2 | 20.8 | -3.2 | 0 | 0 | 0 |
-3.2 | -3.2 | 9.2 | 0 | 0 | 0 |
0 | 0 | 0 | 21 | 0 | 0 |
0 | 0 | 0 | 0 | 21 | 0 |
0 | 0 | 0 | 0 | 0 | 13.7 |
Shear Modulus GV44 GPa |
Bulk Modulus KV86 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR85 GPa |
Shear Modulus GVRH39 GPa |
Bulk Modulus KVRH86 GPa |
Elastic Anisotropy1.65 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaSb2Au (mp-675224) | 0.2886 | 0.286 | 3 |
PrAs (mp-1009583) | 0.0678 | 0.425 | 2 |
CeBi (mp-635471) | 0.0709 | 0.161 | 2 |
SmAs (mp-1009814) | 0.0693 | 0.448 | 2 |
TaNi2 (mp-1157) | 0.0729 | 0.001 | 2 |
PrSb (mp-1644) | 0.0682 | 0.247 | 2 |
Sc (mp-601273) | 0.2864 | 0.128 | 1 |
Pr (mp-568938) | 0.3533 | 0.086 | 1 |
Pa (mp-62) | 0.2424 | 0.027 | 1 |
Pr (mp-1056311) | 0.2006 | 0.086 | 1 |
Sn (mp-55) | 0.1008 | 0.063 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv Ag |
Final Energy/Atom-4.3013 eV |
Corrected Energy-12.9040 eV
-12.9040 eV = -12.9040 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)