Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.581 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.581 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2 + C |
Band Gap2.720 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 62.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 227.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 120.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 198.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 232.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 77.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 277.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 236.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 33.8 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 174.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 164.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 176.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 176.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 169.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 149.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 96.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 58.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 275.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 217.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 62.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 256.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 174.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 277.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 207.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 285.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 126.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 135.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 324.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 270.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 193.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 217.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 96.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 58.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 188.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 198.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 58.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 151.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 217.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu2WSe4 (mp-1025150) | 0.6914 | 0.188 | 3 |
Zn2GeS4 (mp-675748) | 0.6801 | 0.012 | 3 |
Li2MnF4 (mp-763098) | 0.6711 | 0.093 | 3 |
Co2MoS4 (mp-1023124) | 0.6266 | 0.345 | 3 |
Mn(GaS2)2 (mp-20025) | 0.6658 | 0.000 | 3 |
LiCoGeO4 (mp-763507) | 0.6807 | 0.199 | 4 |
LiZnPS4 (mp-11175) | 0.7021 | 0.000 | 4 |
SiP2 (mp-9996) | 0.7277 | 0.000 | 2 |
C3N4 (mp-571653) | 0.6344 | 0.484 | 2 |
B2O (mp-614006) | 0.5197 | 0.925 | 2 |
CN2 (mp-1019086) | 0.3032 | 0.358 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: C N |
Final Energy/Atom-7.7967 eV |
Corrected Energy-46.7804 eV
-46.7804 eV = -46.7804 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)