Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.103 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 133.9 |
C (mp-48) | <1 0 0> | <1 0 1> | 136.8 |
C (mp-48) | <1 0 1> | <1 1 0> | 174.1 |
C (mp-48) | <1 1 0> | <1 1 0> | 174.1 |
C (mp-48) | <1 1 1> | <1 1 0> | 174.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 74.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 74.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 217.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 252.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 163.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 238.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 170.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 92.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 239.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 123.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 130.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 170.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 246.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 307.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 238.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 193.4 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 170.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 92.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 223.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 61.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 282.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 74.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 273.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 92.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 43.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 217.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 92.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 338.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 130.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 223.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 130.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 92.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 74.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 327.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 267.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 297.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 133.9 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 239.3 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 1> | 322.0 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 217.7 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 307.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
USbTe (mp-7935) | 0.1296 | 0.000 | 3 |
UAsSe (mp-22595) | 0.1432 | 0.081 | 3 |
ThBiTe (mp-1019362) | 0.1507 | 0.000 | 3 |
NpSbTe (mp-1018824) | 0.0982 | 0.000 | 3 |
ThPS (mp-12876) | 0.1506 | 0.000 | 3 |
SmSe2 (mp-1019253) | 0.0156 | 0.000 | 2 |
PrSe2 (mp-1018940) | 0.0251 | 0.022 | 2 |
NdSe2 (mp-1018817) | 0.0162 | 0.020 | 2 |
GdSe2 (mp-1018707) | 0.0252 | 0.000 | 2 |
TmS2 (mp-1071948) | 0.0228 | 0.043 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 S |
Final Energy/Atom-5.9537 eV |
Corrected Energy-38.3758 eV
-38.3758 eV = -35.7220 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)