Final Magnetic Moment4.972 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.501 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.149 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToEu2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 62.5 |
C (mp-48) | <1 0 0> | <1 1 0> | 155.6 |
C (mp-48) | <1 0 1> | <1 1 0> | 155.6 |
C (mp-48) | <1 1 0> | <1 0 0> | 242.0 |
C (mp-48) | <1 1 1> | <1 0 0> | 308.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 176.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 217.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 66.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 31.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 187.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 134.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 112.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 62.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 286.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 312.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 62.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 312.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 176.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 154.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 110.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 217.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 134.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 174.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 278.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 264.0 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 155.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 110.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 274.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 311.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 268.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 312.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 342.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 62.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 278.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 154.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 110.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 337.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 62.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 312.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 176.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 62.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 234.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 199.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 312.4 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 262.4 |
InP (mp-20351) | <1 1 1> | <1 0 1> | 303.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 22.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 110.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 174.9 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 93.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
UGeS (mp-638018) | 0.2939 | 0.426 | 3 |
USiS (mp-7932) | 0.1610 | 0.543 | 3 |
NiGePd (mp-3274) | 0.2526 | 0.000 | 3 |
LaTeCl (mp-1018752) | 0.3492 | 0.003 | 3 |
NiAsRh (mp-19768) | 0.2177 | 0.000 | 3 |
Ba2Sb (mp-9908) | 0.2569 | 0.016 | 2 |
Ba2As (mp-2768) | 0.1866 | 0.070 | 2 |
Ca2As (mp-10106) | 0.2572 | 0.041 | 2 |
Sr2As (mp-15697) | 0.2117 | 0.075 | 2 |
Mn2As (mp-610522) | 0.2321 | 0.065 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu O |
Final Energy/Atom-8.7622 eV |
Corrected Energy-55.3827 eV
-55.3827 eV = -52.5735 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)