Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.730 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 638931 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
C (mp-48) <0 0 1> <0 0 1> 107.2
C (mp-48) <1 1 1> <1 0 1> 177.0
C (mp-48) <1 0 0> <0 0 1> 174.1
C (mp-48) <1 0 1> <1 0 1> 59.0
C (mp-48) <1 1 0> <0 0 1> 227.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 200.9
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 281.3
AlN (mp-661) <1 1 1> <1 0 0> 236.5
CeO2 (mp-20194) <1 1 0> <1 1 0> 334.5
AlN (mp-661) <0 0 1> <0 0 1> 147.3
AlN (mp-661) <1 0 0> <1 0 1> 206.5
AlN (mp-661) <1 0 1> <0 0 1> 200.9
AlN (mp-661) <1 1 0> <1 0 1> 236.0
CeO2 (mp-20194) <1 0 0> <0 0 1> 120.6
GaAs (mp-2534) <1 0 0> <0 0 1> 67.0
GaAs (mp-2534) <1 1 0> <1 0 1> 236.0
GaAs (mp-2534) <1 1 1> <1 1 1> 276.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 334.9
BaF2 (mp-1029) <1 1 0> <0 0 1> 281.3
SiO2 (mp-6930) <0 0 1> <0 0 1> 241.1
SiO2 (mp-6930) <1 0 0> <0 0 1> 227.7
SiO2 (mp-6930) <1 0 1> <0 0 1> 281.3
KCl (mp-23193) <1 1 0> <1 0 0> 236.5
SiO2 (mp-6930) <1 1 1> <1 0 1> 265.5
KCl (mp-23193) <1 0 0> <1 0 0> 210.2
DyScO3 (mp-31120) <0 0 1> <1 0 0> 289.1
DyScO3 (mp-31120) <0 1 0> <1 0 1> 88.5
DyScO3 (mp-31120) <1 0 1> <1 0 1> 265.5
DyScO3 (mp-31120) <0 1 1> <1 0 1> 324.5
DyScO3 (mp-31120) <1 0 0> <1 0 1> 236.0
DyScO3 (mp-31120) <1 1 0> <0 0 1> 120.6
DyScO3 (mp-31120) <1 1 1> <0 0 1> 281.3
InAs (mp-20305) <1 1 0> <0 0 1> 281.3
InAs (mp-20305) <1 0 0> <1 0 1> 265.5
ZnSe (mp-1190) <1 0 0> <0 0 1> 67.0
ZnSe (mp-1190) <1 1 1> <1 1 1> 276.5
ZnSe (mp-1190) <1 1 0> <1 0 1> 236.0
KTaO3 (mp-3614) <1 1 1> <0 0 1> 334.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 67.0
KTaO3 (mp-3614) <1 1 0> <1 0 0> 210.2
InP (mp-20351) <1 0 0> <0 0 1> 67.0
InP (mp-20351) <1 1 0> <1 1 0> 148.7
InP (mp-20351) <1 1 1> <1 1 0> 297.3
Te2W (mp-22693) <0 0 1> <1 0 0> 184.0
Te2W (mp-22693) <0 1 0> <1 1 0> 111.5
Te2W (mp-22693) <0 1 1> <1 0 0> 236.5
Te2W (mp-22693) <1 1 0> <1 1 0> 111.5
CdWO4 (mp-19387) <0 0 1> <1 1 1> 158.0
CdWO4 (mp-19387) <0 1 0> <1 0 1> 265.5
CdWO4 (mp-19387) <0 1 1> <1 0 1> 324.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
191 175 81 0 0 0
175 191 81 0 0 0
81 81 318 0 0 0
0 0 0 112 0 0
0 0 0 0 112 0
0 0 0 0 0 157
Compliance Tensor Sij (10-12Pa-1)
31.1 -28 -0.8 0 0 0
-28 31.1 -0.8 0 0 0
-0.8 -0.8 3.5 0 0 0
0 0 0 9 0 0
0 0 0 0 9 0
0 0 0 0 0 6.4
Shear Modulus GV
100 GPa
Bulk Modulus KV
153 GPa
Shear Modulus GR
33 GPa
Bulk Modulus KR
152 GPa
Shear Modulus GVRH
67 GPa
Bulk Modulus KVRH
152 GPa
Elastic Anisotropy
10.20
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZrVSi (mp-5541) 0.0478 0.000 3
PrTeCl (mp-1018941) 0.2632 0.000 3
HfVGe (mp-1018726) 0.0449 0.000 3
CeTeCl (mp-1018667) 0.2591 0.023 3
CeScSi (mp-910150) 0.2604 0.068 3
LuTe2 (mp-973750) 0.2387 0.100 2
UTe2 (mp-21335) 0.2497 0.000 2
GdO2 (mp-21149) 0.2469 0.145 2
CeS2 (mp-1018663) 0.2354 0.014 2
TmTe2 (mp-1072729) 0.2492 0.078 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv V_pv Si
Final Energy/Atom
-8.8844 eV
Corrected Energy
-53.1642 eV
Uncorrected energy = -53.3062 eV Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV Corrected energy = -53.1642 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 638931
Submitted by
User remarks:
  • Hafnium vanadium silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)