Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.975 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.055 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.36 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
HfO2
Band Gap
4.675 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P42/nmc [137]
Hall
P 4n 2n 1n
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 173966 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
C (mp-48) <0 0 1> <0 0 1> 64.6
C (mp-48) <1 0 0> <1 1 0> 79.7
C (mp-48) <1 0 1> <0 0 1> 167.9
C (mp-48) <1 1 0> <1 1 0> 159.3
C (mp-48) <1 1 1> <0 0 1> 271.2
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 177.1
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 281.6
AlN (mp-661) <1 0 1> <1 0 0> 187.7
AlN (mp-661) <1 1 0> <0 0 1> 219.5
AlN (mp-661) <0 0 1> <1 0 1> 68.4
AlN (mp-661) <1 0 0> <0 0 1> 77.5
AlN (mp-661) <1 1 1> <0 0 1> 116.2
CeO2 (mp-20194) <1 0 0> <0 0 1> 116.2
CeO2 (mp-20194) <1 1 0> <1 0 0> 169.0
BaF2 (mp-1029) <1 0 0> <1 0 1> 159.5
BaF2 (mp-1029) <1 1 0> <1 0 1> 113.9
GaAs (mp-2534) <1 0 0> <0 0 1> 64.6
GaAs (mp-2534) <1 1 0> <1 1 1> 236.2
GaAs (mp-2534) <1 1 1> <1 0 0> 300.4
BaF2 (mp-1029) <1 1 1> <1 0 0> 281.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 64.6
SiO2 (mp-6930) <1 0 0> <1 0 1> 159.5
SiO2 (mp-6930) <1 1 0> <1 0 0> 337.9
KCl (mp-23193) <1 0 0> <1 0 1> 159.5
KCl (mp-23193) <1 1 1> <1 0 0> 281.6
SiO2 (mp-6930) <1 0 1> <1 0 1> 182.3
SiO2 (mp-6930) <1 1 1> <1 0 1> 273.4
KCl (mp-23193) <1 1 0> <1 0 1> 113.9
DyScO3 (mp-31120) <0 0 1> <1 0 1> 250.6
DyScO3 (mp-31120) <0 1 0> <0 0 1> 129.1
DyScO3 (mp-31120) <1 0 0> <0 0 1> 322.8
DyScO3 (mp-31120) <1 1 1> <1 1 1> 206.7
DyScO3 (mp-31120) <0 1 1> <1 0 0> 206.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 319.2
DyScO3 (mp-31120) <1 1 0> <0 0 1> 64.6
InAs (mp-20305) <1 1 0> <1 0 1> 113.9
InAs (mp-20305) <1 0 0> <1 0 1> 159.5
ZnSe (mp-1190) <1 0 0> <0 0 1> 64.6
ZnSe (mp-1190) <1 1 0> <1 1 1> 236.2
ZnSe (mp-1190) <1 1 1> <1 0 0> 300.4
KTaO3 (mp-3614) <1 0 0> <0 0 1> 64.6
KTaO3 (mp-3614) <1 1 0> <1 1 0> 212.4
KTaO3 (mp-3614) <1 1 1> <0 0 1> 206.6
Te2W (mp-22693) <1 0 0> <1 0 1> 296.2
Te2W (mp-22693) <1 0 1> <1 0 1> 205.1
Te2W (mp-22693) <1 1 1> <1 0 1> 113.9
InP (mp-20351) <1 0 0> <0 0 1> 167.9
InP (mp-20351) <1 1 0> <1 0 0> 150.2
InP (mp-20351) <1 1 1> <1 0 1> 182.3
Te2W (mp-22693) <0 0 1> <1 0 1> 22.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
377 248 85 0 0 0
248 377 85 0 0 0
85 85 321 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 175
Compliance Tensor Sij (10-12Pa-1)
4.7 -3 -0.5 0 0 0
-3 4.7 -0.5 0 0 0
-0.5 -0.5 3.4 0 0 0
0 0 0 58.6 0 0
0 0 0 0 58.6 0
0 0 0 0 0 5.7
Shear Modulus GV
86 GPa
Bulk Modulus KV
212 GPa
Shear Modulus GR
34 GPa
Bulk Modulus KR
201 GPa
Shear Modulus GVRH
60 GPa
Bulk Modulus KVRH
207 GPa
Elastic Anisotropy
7.51
Poisson's Ratio
0.37

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Zr9ScO20 (mp-674976) 0.4432 0.097 3
CeZr7O16 (mp-752983) 0.4630 0.047 3
CeZr9O20 (mp-766370) 0.3735 0.046 3
HfZrO4 (mp-754964) 0.3343 0.048 3
CeZr6O14 (mp-757324) 0.4480 0.051 3
HfTaNO3 (mp-1018719) 0.5234 0.167 4
ZrO2 (mp-2574) 0.0357 0.036 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

To confirm the nature of the released species we combined IR, NMR, and X-ray fluorescence (XRF) analysis. Upon addition of Am to HfO2 NCs, the expected carboxylic acid band at 1720cm1 is absent in t [...]
High purity HfO2 (99.9% purity) 5inch sputtering target supplied by M/s Semiconductor technology was used to deposit the thin films in MRC rf sputtering machine. The films were deposited on p- type 1 [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition HfO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv O
Final Energy/Atom
-10.1247 eV
Corrected Energy
-63.5576 eV
-63.5576 eV = -60.7484 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 173966
Submitted by
User remarks:
  • Hafnium dioxide