Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.050 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToReN + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 61.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 98.1 |
C (mp-48) | <1 1 0> | <1 0 1> | 67.8 |
C (mp-48) | <1 0 0> | <1 0 1> | 113.0 |
C (mp-48) | <1 1 1> | <0 0 1> | 134.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 226.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 226.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 274.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 258.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 147.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 199.1 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 120.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 159.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 113.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 159.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 210.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 165.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 306.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 110.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 133.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 98.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 139.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 173.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 192.1 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 304.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 221.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 44.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 73.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 239.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 295.6 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 271.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 171.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 180.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 306.4 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 133.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 98.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 139.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 173.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 118.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 29.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 93.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 165.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 272.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 45.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 139.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 110.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 171.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 134.8 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 221.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 49.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2CrO5 (mvc-5219) | 0.6419 | 0.318 | 3 |
Ca4Ta2O9 (mp-769307) | 0.5987 | 0.005 | 3 |
Sr4Ta2O9 (mp-769268) | 0.5532 | 0.032 | 3 |
Mg(HO)2 (mp-626143) | 0.6168 | 0.009 | 3 |
H2C2S (mp-1096982) | 0.6325 | 1.036 | 3 |
Ca2TeWO6 (mvc-5060) | 0.7100 | 0.263 | 4 |
Na3Mo(OF)3 (mp-18753) | 0.6128 | 0.000 | 4 |
Li3Nb4NiO12 (mp-772009) | 0.7386 | 0.089 | 4 |
TiFe(BiO3)2 (mp-560185) | 0.6286 | 0.015 | 4 |
Ca2NiWO6 (mvc-16546) | 0.7127 | 0.102 | 4 |
RuN2 (mp-607371) | 0.4963 | 0.110 | 2 |
ReN2 (mp-1019078) | 0.3927 | 0.144 | 2 |
IrN2 (mp-13076) | 0.5021 | 0.200 | 2 |
OsN2 (mp-21264) | 0.5017 | 0.272 | 2 |
FeN2 (mp-1080202) | 0.4963 | 0.140 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Re_pv N |
Final Energy/Atom-9.5002 eV |
Corrected Energy-57.0014 eV
-57.0014 eV = -57.0014 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)