Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.030 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.067 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToReN + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <1 1 0> | <0 0 1> | 224.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 98.4 |
C (mp-48) | <0 0 1> | <0 0 1> | 42.2 |
C (mp-48) | <1 0 0> | <1 0 -1> | 116.6 |
C (mp-48) | <1 0 1> | <0 0 1> | 154.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 299.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 186.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 140.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 56.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 107.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 212.1 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 116.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 116.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 215.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 161.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 134.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 279.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 186.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 152.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 190.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 209.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 210.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 136.3 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 209.8 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 213.0 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 279.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 53.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 134.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 154.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 134.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 53.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 303.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 -1> | 218.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 210.8 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 334.7 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 186.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 134.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 139.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 161.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 84.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 134.7 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 186.5 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 240.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 242.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 116.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 209.8 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 281.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 300.0 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 183.9 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 253.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuReO4 (mp-755115) | 0.4637 | 0.056 | 3 |
NbFeO4 (mp-34591) | 0.4211 | 0.034 | 3 |
LiFeF4 (mp-777252) | 0.4500 | 0.308 | 3 |
FeOF (mp-768030) | 0.4344 | 0.021 | 3 |
NbFeO4 (mp-691132) | 0.4203 | 0.034 | 3 |
LiV2(OF)3 (mp-782714) | 0.5020 | 0.091 | 4 |
LiVOF3 (mp-764787) | 0.4549 | 0.017 | 4 |
LiV3O5F3 (mp-764776) | 0.3947 | 0.047 | 4 |
LiV3O5F3 (mp-764754) | 0.4909 | 0.053 | 4 |
AlAg(WO4)2 (mvc-641) | 0.5064 | 0.113 | 4 |
NbO2 (mp-821) | 0.5312 | 0.003 | 2 |
NbO2 (mp-557057) | 0.5180 | 0.000 | 2 |
TaO2 (mp-510) | 0.5159 | 0.060 | 2 |
WN2 (mp-776321) | 0.3603 | 0.143 | 2 |
TiO2 (mp-1840) | 0.5159 | 0.020 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Re_pv N |
Final Energy/Atom-9.4803 eV |
Corrected Energy-56.8817 eV
-56.8817 eV = -56.8817 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)