Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.600 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.600 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2 + Ru |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 1 0> | 134.2 |
C (mp-48) | <1 0 1> | <1 1 1> | 103.0 |
C (mp-48) | <1 0 0> | <1 1 1> | 180.3 |
C (mp-48) | <1 1 0> | <1 0 0> | 201.6 |
C (mp-48) | <1 1 1> | <1 0 0> | 201.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 71.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 225.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 94.9 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 114.3 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 114.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 137.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 225.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 249.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 205.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 205.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 215.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 156.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 283.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 166.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 156.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 234.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 154.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 114.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 156.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 283.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 47.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 166.0 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 297.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 177.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 320.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 94.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 260.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 334.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 249.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 166.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 195.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 156.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 283.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 234.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 201.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 218.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 296.4 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 175.9 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 180.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 284.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 285.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbOF (mp-7028) | 0.7444 | 0.000 | 3 |
ReN2 (mp-1019055) | 0.1308 | 0.495 | 2 |
OsN2 (mp-1018852) | 0.0841 | 0.912 | 2 |
ReC2 (mp-1008802) | 0.6172 | 0.910 | 2 |
MoN2 (mp-1080193) | 0.2720 | 0.252 | 2 |
TiN2 (mp-1080172) | 0.5608 | 0.268 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ru_pv N |
Final Energy/Atom-7.7933 eV |
Corrected Energy-46.7597 eV
-46.7597 eV = -46.7597 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)