Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.129 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.226 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToReN + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 22.3 |
C (mp-48) | <1 0 0> | <1 1 0> | 39.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 81.7 |
C (mp-48) | <1 1 0> | <1 0 0> | 68.4 |
C (mp-48) | <1 1 1> | <1 0 0> | 227.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 96.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 227.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 96.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 79.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 191.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 157.9 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 80.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 52.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 118.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 208.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 237.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 200.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 273.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 66.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 236.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 321.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 200.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 273.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 66.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 250.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 45.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 95.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 287.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 182.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 304.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 66.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.7 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 185.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 237.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 237.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 118.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 178.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 148.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 263.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 287.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 197.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 230.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 29.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InSnCl3 (mp-998567) | 0.7005 | 0.000 | 3 |
Ca4Ta2O9 (mp-769307) | 0.6891 | 0.005 | 3 |
Sr4Ta2O9 (mp-769268) | 0.6856 | 0.032 | 3 |
YbTiO3 (mp-753164) | 0.7020 | 0.051 | 3 |
HfCuP (mp-569933) | 0.6725 | 0.798 | 3 |
TiFe(BiO3)2 (mp-560185) | 0.7219 | 0.015 | 4 |
OsC2 (mp-1018850) | 0.1161 | 0.578 | 2 |
WN2 (mp-999549) | 0.1000 | 0.027 | 2 |
OsC2 (mp-1008835) | 0.1314 | 0.600 | 2 |
ReN2 (mp-1008798) | 0.0576 | 0.232 | 2 |
WN2 (mp-1077232) | 0.0852 | 0.027 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Re_pv N |
Final Energy/Atom-9.3210 eV |
Corrected Energy-55.9260 eV
-55.9260 eV = -55.9260 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)