material

SmTlCd

ID:

mp-1019255

DOI:

10.17188/1350767


Tags: Cadmium samarium thallium (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.321 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.002 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.64 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SmTl + SmCd2 + SmTl3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
C (mp-48) <0 0 1> <0 0 1> 196.1
C (mp-48) <1 0 0> <0 0 1> 152.5
C (mp-48) <1 0 1> <0 0 1> 239.7
C (mp-48) <1 1 0> <1 1 1> 67.8
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 348.6
AlN (mp-661) <0 0 1> <0 0 1> 261.4
AlN (mp-661) <1 0 0> <1 0 0> 111.2
AlN (mp-661) <1 0 1> <1 1 0> 192.5
CeO2 (mp-20194) <1 1 0> <0 0 1> 326.8
BaF2 (mp-1029) <1 1 0> <1 1 1> 271.1
SiO2 (mp-6930) <1 0 0> <1 0 0> 111.2
SiO2 (mp-6930) <1 0 1> <0 0 1> 239.7
SiO2 (mp-6930) <1 1 0> <1 1 0> 192.5
SiO2 (mp-6930) <1 1 1> <1 1 0> 320.9
KCl (mp-23193) <1 1 1> <0 0 1> 283.2
AlN (mp-661) <1 1 0> <1 0 0> 111.2
CeO2 (mp-20194) <1 1 1> <0 0 1> 152.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 196.1
BaF2 (mp-1029) <1 1 1> <0 0 1> 65.4
InAs (mp-20305) <1 0 0> <1 0 1> 300.9
InAs (mp-20305) <1 1 0> <0 0 1> 261.4
InP (mp-20351) <1 1 0> <1 0 0> 148.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 21.8
InAs (mp-20305) <1 1 1> <0 0 1> 65.4
Te2W (mp-22693) <0 0 1> <1 0 0> 296.4
CdWO4 (mp-19387) <0 0 1> <1 0 0> 148.2
CdWO4 (mp-19387) <0 1 0> <0 0 1> 283.2
CdWO4 (mp-19387) <1 1 0> <1 0 0> 296.4
TePb (mp-19717) <1 0 0> <1 0 0> 222.3
TePb (mp-19717) <1 1 1> <0 0 1> 283.2
KTaO3 (mp-3614) <1 0 0> <1 0 1> 214.9
KTaO3 (mp-3614) <1 1 0> <1 0 1> 343.9
KTaO3 (mp-3614) <1 1 1> <0 0 1> 87.1
Te2W (mp-22693) <0 1 0> <1 0 1> 257.9
Te2W (mp-22693) <1 1 0> <1 0 0> 111.2
Ni (mp-23) <1 0 0> <0 0 1> 108.9
Ni (mp-23) <1 1 0> <1 0 1> 86.0
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 65.4
BN (mp-984) <1 0 0> <0 0 1> 152.5
BN (mp-984) <1 0 1> <0 0 1> 239.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 222.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 283.2
Te2Mo (mp-602) <1 0 0> <0 0 1> 261.4
Te2Mo (mp-602) <1 0 1> <1 1 1> 271.1
Ni (mp-23) <1 1 1> <0 0 1> 21.8
GaSe (mp-1943) <0 0 1> <0 0 1> 87.1
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 185.3
MoS2 (mp-1434) <0 0 1> <1 0 0> 222.3
MoS2 (mp-1434) <1 0 0> <1 0 0> 259.4
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 222.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
101 34 35 0 0 0
34 101 35 0 0 0
35 35 59 0 0 0
0 0 0 27 0 0
0 0 0 0 27 0
0 0 0 0 0 34
Compliance Tensor Sij (10-12Pa-1)
12.8 -2.1 -6.3 0 0 0
-2.1 12.8 -6.3 0 0 0
-6.3 -6.3 24.4 0 0 0
0 0 0 37.6 0 0
0 0 0 0 37.6 0
0 0 0 0 0 29.7
Shear Modulus GV
28 GPa
Bulk Modulus KV
52 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
49 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
51 GPa
Elastic Anisotropy
0.40
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaHgPb (mp-20879) 0.0299 0.076 3
YbHgPb (mp-571493) 0.1729 0.080 3
NdTlCd (mp-1018819) 0.1348 0.010 3
HfGaCu (mp-1018714) 0.1073 0.000 3
CeInCu (mp-1077348) 0.0653 0.133 3
EuHg2 (mp-20719) 0.0871 0.010 2
PrAg2 (mp-568654) 0.1203 0.005 2
In2Cu (mp-1018730) 0.0136 0.188 2
CeSe2 (mp-1011376) 0.0903 0.566 2
PuGa2 (mp-21200) 0.0687 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sm_3 Tl_d Cd
Final Energy/Atom
-2.9826 eV
Corrected Energy
-17.8956 eV
Uncorrected energy = -17.8956 eV Corrected energy = -17.8956 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 620482
Submitted by
User remarks:
  • Cadmium samarium thallium (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)