Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.046 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlPO4 |
Band Gap5.302 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 1 0> | 312.5 |
C (mp-48) | <1 0 0> | <1 0 -1> | 135.1 |
C (mp-48) | <1 0 1> | <1 1 1> | 179.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 269.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 156.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 312.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 207.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 312.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 312.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 156.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 269.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 208.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 312.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 156.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 312.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 156.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 156.3 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 208.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 260.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 156.3 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 126.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 312.5 |
BN (mp-984) | <1 1 0> | <0 1 0> | 260.4 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 269.6 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 269.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 156.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 312.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 260.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 260.4 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 260.4 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 179.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 312.5 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 312.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 89.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 312.5 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 312.5 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 208.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 208.3 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 156.3 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 156.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 269.6 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 126.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 126.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 156.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 208.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 156.3 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 312.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 260.4 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 -1> | 135.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiReO4 (mp-540946) | 0.3764 | 0.000 | 3 |
ZnMoO4 (mp-25085) | 0.4230 | 0.000 | 3 |
Fe7(AsO4)6 (mp-542660) | 0.4107 | 0.000 | 3 |
LiFeF4 (mp-777920) | 0.3778 | 0.087 | 3 |
AlPO4 (mp-1019514) | 0.2206 | 0.083 | 3 |
V4Zn3(PO4)6 (mp-25129) | 0.4628 | 0.074 | 4 |
V4Zn3(PO4)6 (mvc-15017) | 0.4559 | 0.074 | 4 |
Mn3V6(FeO6)4 (mp-567051) | 0.4403 | 0.004 | 4 |
Li2U(MoO5)2 (mp-565208) | 0.4351 | 0.000 | 4 |
Mg3Cr6(FeO6)4 (mvc-7826) | 0.4605 | 0.111 | 4 |
LiVP2HO8 (mp-850369) | 0.7287 | 0.105 | 5 |
LiVP2HO8 (mp-780110) | 0.7026 | 0.100 | 5 |
LiV3Fe2CuO12 (mp-767459) | 0.5458 | 2.323 | 5 |
Al2CuSi2O7F2 (mp-557084) | 0.6035 | 0.034 | 5 |
LiMgIn(MoO4)3 (mp-566467) | 0.4007 | 0.000 | 5 |
LiMnVP2(O4F)2 (mp-778336) | 0.6317 | 0.001 | 6 |
LiVFeP2(O4F)2 (mp-777635) | 0.6601 | 0.026 | 6 |
LiVCrP2(O4F)2 (mp-767464) | 0.7134 | 0.152 | 6 |
LiVCrP2(O4F)2 (mp-765305) | 0.7234 | 0.139 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.7257 | 0.111 | 6 |
Explore more synthesis descriptions for materials of composition AlPO4.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al P O |
Final Energy/Atom-7.4029 eV |
Corrected Energy-566.7183 eV
-566.7183 eV = -533.0084 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)