Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.226 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.450 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 275.8 |
C (mp-48) | <1 0 0> | <0 0 1> | 275.8 |
C (mp-48) | <1 0 1> | <1 0 -1> | 258.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 272.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 110.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 264.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 272.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 198.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 111.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 272.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 258.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 165.5 |
KCl (mp-23193) | <1 1 0> | <1 1 -1> | 111.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 322.9 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 111.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 165.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 206.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 110.3 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 103.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 322.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 181.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 275.8 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 132.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 275.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 220.6 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 -1> | 129.2 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 -1> | 322.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 322.9 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 275.8 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 258.3 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 103.2 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 258.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 165.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 206.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 272.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 272.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 206.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 330.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 322.9 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 275.8 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 103.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 55.2 |
TiO2 (mp-2657) | <1 1 1> | <1 0 -1> | 258.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 275.8 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 206.5 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 224.9 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 275.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 220.6 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 322.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 330.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.02 | 0.00 | 0.08 |
0.00 | 5.75 | 0.00 |
0.08 | 0.00 | 5.65 |
Dielectric Tensor εij (total) |
||
---|---|---|
17.01 | 0.00 | 1.97 |
0.00 | 14.52 | 0.00 |
1.97 | 0.00 | 18.59 |
Polycrystalline dielectric constant
εpoly∞
5.80
|
Polycrystalline dielectric constant
εpoly
16.71
|
Refractive Index n2.41 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K4SnO4 (mp-7258) | 0.4784 | 0.000 | 3 |
Sr3MoN4 (mp-31356) | 0.4643 | 0.004 | 3 |
Sr3MoN4 (mp-570046) | 0.4827 | 0.000 | 3 |
Na4SiO4 (mp-7500) | 0.4640 | 0.000 | 3 |
Ca4GeN4 (mp-29808) | 0.2789 | 0.000 | 3 |
SrCa2WN4 (mp-567568) | 0.5822 | 0.000 | 4 |
SnHg6(P2Cl3)2 (mp-568612) | 0.6215 | 0.000 | 4 |
Na4Mo(NO)2 (mp-18772) | 0.5841 | 0.062 | 4 |
Na4W(NO)2 (mp-19125) | 0.6047 | 0.156 | 4 |
Li6Fe(SiO4)2 (mp-768001) | 0.6488 | 0.063 | 4 |
LiCaMgSiN3 (mp-1020108) | 0.7107 | 0.004 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Si N |
Final Energy/Atom-6.2622 eV |
Corrected Energy-225.4390 eV
-225.4390 eV = -225.4390 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)