Final Magnetic Moment0.195 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.269 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.603 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToEuBO3 + GeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <0 0 1> | 260.0 |
C (mp-48) | <1 0 0> | <0 0 1> | 303.3 |
C (mp-48) | <1 0 1> | <0 0 1> | 260.0 |
C (mp-48) | <1 1 1> | <0 1 1> | 301.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 303.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 130.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 185.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 260.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 216.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 308.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 303.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 123.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 173.3 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 123.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 173.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 260.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 216.7 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 185.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 346.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 303.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 246.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 260.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 216.7 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 185.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 226.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 301.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 308.6 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 260.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 303.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 246.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 346.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 303.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 246.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 260.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 216.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 308.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 303.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 130.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 303.3 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 308.6 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 308.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 260.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 145.6 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 123.5 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 185.2 |
TiO2 (mp-2657) | <0 0 1> | <1 1 1> | 151.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 123.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 308.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 173.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 150.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgPO3 (mp-775762) | 0.6460 | 0.045 | 3 |
BaSiO3 (mp-7339) | 0.6716 | 0.022 | 3 |
Na2Cr2O7 (mp-743627) | 0.6896 | 0.005 | 3 |
CrAgO4 (mp-850137) | 0.6831 | 0.030 | 3 |
CrHgO4 (mp-19155) | 0.6219 | 0.004 | 3 |
SrZn2(PO4)2 (mp-8810) | 0.7282 | 0.000 | 4 |
BaZn2(PO4)2 (mp-6089) | 0.7299 | 0.000 | 4 |
Li2Bi2(SO4)3 (mp-777356) | 0.6311 | 0.093 | 4 |
Cs2AgAsS4 (mp-561622) | 0.7458 | 0.000 | 4 |
KZnP2O7 (mp-773901) | 0.6413 | 0.087 | 4 |
SrZnP2WO8 (mvc-3145) | 0.6793 | 0.279 | 5 |
KH6C2S2NO4 (mp-24179) | 0.7408 | 0.217 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Eu Ge_d B O |
Final Energy/Atom-7.8480 eV |
Corrected Energy-430.5674 eV
-430.5674 eV = -408.0941 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)