material

Ga3BN4

ID:

mp-1019743

DOI:

10.17188/1350815


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.644 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.223 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BN + GaN
Band Gap
2.393 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P43m [215]
Hall
P 4 2 3
Point Group
43m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.000 278.7
NaCl (mp-22862) <1 1 1> <1 1 1> 0.011 225.3
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.023 148.6
TePb (mp-19717) <1 1 1> <1 1 1> 0.025 225.3
Si (mp-149) <1 0 0> <1 0 0> 0.027 148.6
C (mp-66) <1 0 0> <1 0 0> 0.032 167.2
Ni (mp-23) <1 1 0> <1 1 0> 0.034 52.6
Ge (mp-32) <1 0 0> <1 0 0> 0.036 167.2
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.054 223.0
LiF (mp-1138) <1 0 0> <1 0 0> 0.069 148.6
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.072 225.3
LiF (mp-1138) <1 1 0> <1 1 0> 0.075 210.2
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.076 210.2
C (mp-48) <1 1 1> <1 0 0> 0.077 204.4
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.080 353.0
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.092 225.3
GaN (mp-804) <1 0 0> <1 1 0> 0.094 183.9
GaAs (mp-2534) <1 0 0> <1 0 0> 0.095 167.2
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.098 105.1
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.109 353.0
Al (mp-134) <1 0 0> <1 0 0> 0.111 148.6
Mg (mp-153) <1 0 0> <1 1 0> 0.114 183.9
Al (mp-134) <1 1 0> <1 1 0> 0.121 210.2
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.126 236.5
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.126 96.5
GaN (mp-804) <1 1 0> <1 1 0> 0.127 236.5
BN (mp-984) <1 0 0> <1 1 0> 0.128 289.0
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.138 241.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.139 78.8
C (mp-48) <1 0 0> <1 1 0> 0.140 289.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.146 167.2
CdTe (mp-406) <1 1 1> <1 1 1> 0.155 225.3
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.166 225.3
InSb (mp-20012) <1 1 1> <1 1 1> 0.185 225.3
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.194 148.6
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.196 315.8
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.205 278.7
Cu (mp-30) <1 0 0> <1 0 0> 0.209 167.2
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.209 157.7
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.210 353.0
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.211 210.2
Au (mp-81) <1 1 1> <1 0 0> 0.220 334.4
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.222 278.7
GaAs (mp-2534) <1 1 1> <1 1 1> 0.237 225.3
Mg (mp-153) <1 1 1> <1 0 0> 0.240 148.6
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.242 297.3
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.252 148.6
C (mp-48) <0 0 1> <1 0 0> 0.259 167.2
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.269 210.2
SiC (mp-7631) <1 1 0> <1 1 1> 0.285 160.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
328 147 147 0 0 0
147 328 147 0 0 0
147 147 328 0 0 0
0 0 0 173 0 0
0 0 0 0 173 0
0 0 0 0 0 173
Compliance Tensor Sij (10-12Pa-1)
4.2 -1.3 -1.3 0 0 0
-1.3 4.2 -1.3 0 0 0
-1.3 -1.3 4.2 0 0 0
0 0 0 5.8 0 0
0 0 0 0 5.8 0
0 0 0 0 0 5.8
Shear Modulus GV
140 GPa
Bulk Modulus KV
207 GPa
Shear Modulus GR
127 GPa
Bulk Modulus KR
207 GPa
Shear Modulus GVRH
134 GPa
Bulk Modulus KVRH
207 GPa
Elastic Anisotropy
0.52
Poisson's Ratio
0.23

Similar Structures

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CoSiO4 (mp-764642) 0.1301 0.026 4
Li2CoGeO4 (mp-769776) 0.2256 0.000 4
Li2CoSiO4 (mp-764957) 0.2025 0.015 4
Li2SiCuO4 (mp-752606) 0.1555 0.063 4
Li2FeSiO4 (mp-765904) 0.2122 0.015 4
RhI (mp-975142) 0.3297 0.442 2
BC5 (mp-1018649) 0.2353 0.269 2
ZnP2 (mp-2782) 0.3155 0.000 2
Si3H (mp-1040468) 0.2975 0.043 2
ZnP2 (mp-11025) 0.3148 0.000 2
B2CN (mp-1008526) 0.1562 0.334 3
B2CN (mp-1008525) 0.1905 0.331 3
Al3BN4 (mp-1019380) 0.1599 0.252 3
Li3AsO4 (mp-9197) 0.2133 0.000 3
VCu3O4 (mp-510657) 0.1579 0.085 3
C (mp-611426) 0.4516 0.145 1
Si (mp-971662) 0.2634 0.063 1
Sn (mp-949028) 0.2658 0.027 1
C (mp-569567) 0.4527 0.174 1
C (mp-569517) 0.4526 0.145 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
10
U Values
--
Pseudopotentials
VASP PAW: Ga_d B N
Final Energy/Atom
-6.5918 eV
Corrected Energy
-52.7343 eV
-52.7343 eV = -52.7343 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
User remarks:
  • new ICSD batch
  • MP user submission

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)